Abstract

Abstract An electrical laminate having an ability to absorb or shield ultraviolet rays having wavelength of 300-420 nm which comprises (i) at least one thermosetting resin-impregnated substrate, (ii) said substrate and a metal foil or (iii) said substrate, a metal foil and an adhesive layer for the metal foil comprising a thermosetting resin, characterized in that the thermosetting resin constituting part or all of said substrates or constituting said adhesive layer contains 0.2-6.0% by weight of a light absorber (A) on the basis of weight of the thermosetting resin, said light absorber is (a) an alkylthioxantone or a mixture of (a) said alkylthioxantone and (b) an ultraviolet rays-absorber.

Inventors

  • 👤 Morio Gaku
  • 👤 Kenzi Ishii
  • 👤 Takamasa Nakai

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 08:32
CPC Classifications
B; B32; B32B; B32B15/00; B32B15/04; B32B15/08; B32B7/00; B32B7/04; B32B7/12; B32B15/092; B32B15/18; B32B15/20; B32B27/00; B32B27/38; C; C08; C08K; C08K5/00; C08K5/36; C08K5/45; H; H10; H10W; H10W42/00; H10W42/20; B32B2311/00; B32B2311/12; B32B2311/24; B32B2311/30; H05; H05K; H05K1/00; H05K1/02; H05K1/03; H05K1/0313; H05K1/0353; H05K1/0373; Y; Y10; Y10S; Y10S428/00; Y10S428/901; Y10T; Y10T428/00; Y10T428/26; Y10T428/261; Y10T428/31504; Y10T428/31511; Y10T428/31525; Y10T428/31529; Y10T428/31678; Y10T428/31688; Y10T442/00; Y10T442/20; Y10T442/259; Y10T442/2607; Y10T442/30; Y10T442/3382; Y10T442/3415; Y10T442/60; Y10T442/654; Y10T442/656

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 157 words
An electrical laminate which comprises (i) at least one thermosetting resin-impregnated substrate, (ii) a combination of said substrate and a metal foil, or (iii) a combination of said substrate, a metal foil and an adhesive layer for the metal foil comprising a thermosetting resin, wherein said thermosetting resin of at least one said substrate or said adhesive layer contains 0.2 to 6.0% by weight of a light absorber (A) on the bases of the weight of the thermosetting resin, said light absorber (A) is selected from the group consisting of (a) an alkylthioxantone and said alkylthioxantone (a) and (b) an ultraviolet rays-absorber, said alkylthioxantones represented by the following formula (1): ##STR2## wherein each of R 1 and R 2 represents alkyl group, each of p and q represents 0 or an integer of not more than 4, and p+q≧1, and the electrical laminate having an ability to absorb or shield ultraviolet rays having wavelength of 300-420 nm.
Claim 2
Dependent Claim 157 words
An electrical laminate which comprises (i) at least one thermosetting resin-impregnated substrate, (ii) a combination of said substrate and a metal foil, or (iii) a combination of said substrate, a metal foil and an adhesive layer for the metal foil comprising a thermosetting resin, wherein said thermosetting resin of at least one said substrate or said adhesive layer contains 0.2 to 6.0% by weight of a light absorber (A) on the bases of the weight of the thermosetting resin, said light absorber (A) is selected from the group consisting of (a) an alkylthioxantone and said alkylthioxantone (a) and (b) an ultraviolet rays-absorber, said alkylthioxantones represented by the following formula (1): ##STR2## wherein each of R 1 and R 2 represents alkyl group, each of p and q represents 0 or an integer of not more than 4, and p+q≧1, and the electrical laminate having an ability to absorb or shield ultraviolet rays having wavelength of 300-420 nm.
Claim 3
Dependent Claim 22 words
The electrical laminate of claim 1 wherein said alkylthioxantone (a) is selected from the group consisting of 2,4-dimethylthioxantone; 2,4-diethylthioxantone; 2,4-diisopropylthioxantone and 4-isopropylthioxantone.
Claim 4
Dependent Claim 24 words
The electrical laminate of claim 1, wherein said ultraviolet rays-absorber (b) is selected from the group consisting of 2-(2-hydroxy-5-methylphenyl)benzotriazole, 2-(2-hydroxy-5-butylphenyl)benzotriazole, 2-(2-hydroxy-3,5-di-t-butylphenyl)benzotriazole, 2-(2-hydroxy-3,5-di-t-amylphenyl)benzotriazole and 2-(2-hydroxy-3-t-butyl-5-methylphenyl)-5-chlorobenzotriazole.
Claim 5
Dependent Claim 28 words
The electrical laminate of claim 1 wherein said light absorber in an amount of 2-6% by weight is contained in only the thermosetting resin constituting the adhesive layer.
Claim 6
Dependent Claim 38 words
The electrical laminate of claim 1 wherein two or more thermosetting resin-impregnated substrates are used, and said light absorber in an amount of 2-6% by weight is contained in only the thermosetting resin in part of the substrates.
Claim 7
Dependent Claim 116 words
In an electrical laminate comprising at least one layer formed at least in part of a thermoset resin, the improvement wherein said layer further comprises 0.2 to 6.0% by weight on the basis of the weight of the thermoset resin of a light absorber, said light absorber being selected from the group consisting of (i) an alkylthioxantone of the formula: ##STR3## wherein each of R 1 and R 2 represents alkyl group, each of p and q represents 0 or an integer of not more than 4, and p+q≧1, and (ii) a mixture of said alkylthioxantone and an ultraviolet ray-absorber, said laminate being capable of absorbing or shielding ultraviolet rays having a wavelength of 300-420 nm.
Claim 8
Dependent Claim 116 words
In an electrical laminate comprising at least one layer formed at least in part of a thermoset resin, the improvement wherein said layer further comprises 0.2 to 6.0% by weight on the basis of the weight of the thermoset resin of a light absorber, said light absorber being selected from the group consisting of (i) an alkylthioxantone of the formula: ##STR3## wherein each of R 1 and R 2 represents alkyl group, each of p and q represents 0 or an integer of not more than 4, and p+q≧1, and (ii) a mixture of said alkylthioxantone and an ultraviolet ray-absorber, said laminate being capable of absorbing or shielding ultraviolet rays having a wavelength of 300-420 nm.

References Cited (Backward Citations)

JPH02227442A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-11-03 1996-05-04 1996-11-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-11-03 2000-05-04 2000-11-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-11-03 2004-05-04 2004-11-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag