← Back to Patent Explorer
US5153930A Expired / Lapsed US ⏱️ 0.0 years remaining

Device employing a substrate of a material that exhibits the pyroelectric effect

Assignee: Honeywell Inc
•
Filing: 1990-01-04
•
Granted: 1992-10-06
•
Expires: 2010-01-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An article is manufactured from a substrate of a material that exhibits the pyroelectric effect by depositing a film containing a selected material in a first state over a front surface of the substrate. At least one electrode is formed on the film, portions of the film being exposed around the electrode. The exposed portions of the film are subjected to a treatment such that they are converted from the first state to a second state, in which the material has a resistivity that lies within a desired range of values.

Inventors

  • 👤 Richard E. DuPuy
  • 👤 Harold R. Gilles
  • 👤 Edwin Boyd Osgood

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 00:32
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/01; G02F1/03; G02F1/035; G02F1/21; G02F1/225; G02F1/29; G02F1/31; G02F1/313; G02F1/3132; G02F2201/00; G02F2201/06; G02F2201/066; G02F2201/07; G02F2202/00; G02F2202/20; G02F2203/00; G02F2203/21

Claims Analysis

Total Claims: 30
Claim 1
Independent Claim 211 words
A method of manufacturing an electrooptic device, comprising: (a) providing a substrate of an electrooptic material that exhibits the pyroelectric effect, the substrate having a waveguide formed therein beneath a top surface thereof, (b) forming an insulating buffer layer over the top surface of the substrate, the buffer layer having a bottom surface that confronts the top surface of the substrate and also having a top surface, (c) depositing a film containing a selected material in a low resistivity state over the top surface of the buffer layer, said material being convertible from its low resistivity state to a high resistivity state on being subjected to a predetermined treatment, (d) forming at least one electrode on a first region of said film while leaving a second region of said film exposed, said electrode being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide also passes through the electrode, and (e) exposing said second region of said film to a predetermined agent under conditions such that said second region of the film is subjected to said predetermined treatment, said first region of the film being masked from the predetermined agent by the electrode and therefore not subjected to said predetermined treatment.
Claim 2
Independent Claim 211 words
A method of manufacturing an electrooptic device, comprising: (a) providing a substrate of an electrooptic material that exhibits the pyroelectric effect, the substrate having a waveguide formed therein beneath a top surface thereof, (b) forming an insulating buffer layer over the top surface of the substrate, the buffer layer having a bottom surface that confronts the top surface of the substrate and also having a top surface, (c) depositing a film containing a selected material in a low resistivity state over the top surface of the buffer layer, said material being convertible from its low resistivity state to a high resistivity state on being subjected to a predetermined treatment, (d) forming at least one electrode on a first region of said film while leaving a second region of said film exposed, said electrode being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide also passes through the electrode, and (e) exposing said second region of said film to a predetermined agent under conditions such that said second region of the film is subjected to said predetermined treatment, said first region of the film being masked from the predetermined agent by the electrode and therefore not subjected to said predetermined treatment.
Claim 3
Dependent Claim 85 words
A method according to claim 1, wherein said first region of the film has first and second portions, and step (d) comprises forming first and second electrodes on said first and second portions respectively of said first region of the film, a portion of the second region of said film being exposed between said electrodes, and the electrodes being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide also passes through the first electrode.
Claim 4
Dependent Claim 12 words
An article of manufacture, made by a method according to claim 2.
Claim 5
Dependent Claim 31 words
A method according to claim 1, wherein step (d) comprises depositing a layer of metal over said film and selectively removing said layer to form said electrode and a terminal portion.
Claim 6
Dependent Claim 32 words
A method according to claim 4, further comprising depositing a layer of conductive material over a bottom surface of the substrate and connecting said terminal portion to said layer of conductive material.
Claim 7
Dependent Claim 26 words
A method according to claim 1, wherein the material of the film deposited in step (c) is a refractory metal and the predetermined agent is oxygen.
Claim 8
Dependent Claim 29 words
A method according to claim 6, wherein the substrate provided in step (a) is LiNbO 3 , the waveguide is a titanium-diffused waveguide and the refractory metal is titanium.
Claim 9
Dependent Claim 51 words
A method according to claim 1, wherein step (a) comprises providing a substrate of an electrooptic material that exhibits the pyroelectric effect and forming a waveguide therein by diffusion of titanium into the substrate, the material of the film deposited in step (c) is titanium, and the predetermined agent is oxygen.
Claim 10
Dependent Claim 26 words
A method according to claim 8, wherein the buffer layer is SiO 2 and said predetermined treatment comprises heating in the presence of said predetermined agent.
Claim 11
Dependent Claim 29 words
A method according to claim 1, further comprising depositing a layer of conductive material over a bottom surface of the substrate and connecting said layer electrically to said film.
Claim 12
Dependent Claim 12 words
An article of manufacture, made by a method according to claim 1.
Claim 13
Dependent Claim 143 words
A method according to claim 1, wherein the substrate that is provided in step (a) has first and second waveguides formed therein, the first and second waveguides being spaced in a direction parallel to the top surface of the substrate, said first region of the film has first and second portions, and step (d) comprises forming first and second electrodes on said first and second portions respectively of said first region of the film, the electrodes being positioned so that a line that is normal to the top surface of the substrate and passes through the first waveguide also passes through the first electrode and a line that is normal to the top surface of the substrate and passes through the second waveguide also passes through the second electrode, a portion of the second region of said film being exposed between said electrodes.
Claim 14
Dependent Claim 12 words
An article of manufacture, made by a method according to claim 12.
Claim 15
Independent Claim 140 words
A method of manufacturing an article, comprising: (a) providing a substrate of an electrooptic material that exhibits the pyroelectric effect, the substrate having a waveguide segment formed therein beneath a top surface thereof, (b) forming an insulating buffer layer over the top surface of the substrate, the buffer layer having a bottom surface that confronts the top surface of the substrate and also having a top surface, (c) depositing a film of refractory metal over the top surface of the buffer layer, (d) forming first and second electrodes on said film, portions of said film being exposed between said electrodes and the electrodes being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide segment also passes through the first electrode, and (e) heating said film in an oxidizing atmosphere.
Claim 16
Independent Claim 140 words
A method of manufacturing an article, comprising: (a) providing a substrate of an electrooptic material that exhibits the pyroelectric effect, the substrate having a waveguide segment formed therein beneath a top surface thereof, (b) forming an insulating buffer layer over the top surface of the substrate, the buffer layer having a bottom surface that confronts the top surface of the substrate and also having a top surface, (c) depositing a film of refractory metal over the top surface of the buffer layer, (d) forming first and second electrodes on said film, portions of said film being exposed between said electrodes and the electrodes being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide segment also passes through the first electrode, and (e) heating said film in an oxidizing atmosphere.
Claim 17
Dependent Claim 15 words
A method according to claim 14, further comprising measuring the electrical resistance between the electrodes.
Claim 18
Dependent Claim 42 words
A method according to claim 14, wherein the electrooptic material is LiNbO 3 , the buffer layer is SiO 2 , the waveguide segment in the substrate is a titanium-diffused waveguide segment and the refractory metal deposited in step (c) is titanium.
Claim 19
Dependent Claim 12 words
An article of manufacture, made by a method according to claim 14.
Claim 20
Dependent Claim 100 words
A method according to claim 14, wherein the substrate provided in step (a) has first and second waveguide segments formed therein beneath the top surface thereof and spaced apart in a direction parallel to said top surface, and the electrodes that are formed in step (d) are positioned so that a line that is normal to the top surface of the substrate and passes through the first waveguide segment also passes through the first electrode and a line that is normal to the top surface of the substrate and passes though the second waveguide also pass through the second electrode.
Claim 21
Dependent Claim 12 words
An article of manufacture, made by a method according to claim 18.
Claim 22
Dependent Claim 141 words
An article of manufacture comprising: a substrate of an electrooptic material that exhibits the pyroelectric effect, the substrate having a top surface and there being a waveguide in the substrate beneath said top surface, an insulating buffer layer overlying the top surface of the substrate, the buffer layer having a bottom surface that confronts the top surface of the substrate and also having a top surface, a film over the top surface of the buffer layer, said film including a selected material and having a high resistivity region and a low resistivity region, and at least one electrode overlying the low resistivity region of said film while leaving the high resistivity region exposed, said electrode being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide also passes through the electrode.
Claim 23
Dependent Claim 141 words
An article of manufacture comprising: a substrate of an electrooptic material that exhibits the pyroelectric effect, the substrate having a top surface and there being a waveguide in the substrate beneath said top surface, an insulating buffer layer overlying the top surface of the substrate, the buffer layer having a bottom surface that confronts the top surface of the substrate and also having a top surface, a film over the top surface of the buffer layer, said film including a selected material and having a high resistivity region and a low resistivity region, and at least one electrode overlying the low resistivity region of said film while leaving the high resistivity region exposed, said electrode being positioned so that a line that is normal to the top surface of the substrate and passes through the waveguide also passes through the electrode.
Claim 24
Dependent Claim 123 words
An article according to claim 20, wherein the substrate has first and second waveguides formed therein beneath the top surface thereof, the low resistivity region of the film has first and second portions, and the article comprises first and second discrete electrodes overlying said first and second portions respectively of said low resistivity region of the film while leaving a portion of the high resistivity region exposed therebetween, said electrodes being positioned so that a line that is normal to the top surface of the substrate and passes through the first waveguide also passes through the first electrode and a line that is normal to the top surface of the substrate and passes through the second waveguide also passes through the second electrode.
Claim 25
Dependent Claim 40 words
An article according to claim 20, wherein the substrate has a bottom surface and the article comprises a layer of conductive material over the bottom surface of the substrate, the layer of conductive material being electrically connected to the film.
Claim 26
Dependent Claim 46 words
An article according to claim 22, wherein the low resistivity region of the film has a terminal portion, and the article comprises a terminal portion of metal overlying the terminal portion of said film, and conductive material connecting said terminal portion to the layer of metal.
Claim 27
Dependent Claim 28 words
An article according to claim 20, wherein the material of the substrate is LiNbO 3 , the waveguide is a titanium-diffused waveguide and said selected material is titanium.
Claim 28
Dependent Claim 14 words
An article according to claim 24, wherein the buffer layer is SiO 2 .
Claim 29
Dependent Claim 14 words
An article according to claim 20, wherein said selected material is a refractory metal.
Claim 30
Dependent Claim 12 words
An article according to claim 26, wherein the refractory metal is titanium.

References Cited (Backward Citations)

US4445751A Cited
US4799750A Cited
US4778236A Cited
US4818063A Cited
US4766954A Cited
US4880288A Cited
US4925263A Cited
US4976517A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-10-06 1996-04-06 1996-10-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-10-06 2000-04-06 2000-10-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-10-06 2004-04-06 2004-10-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag