Abstract

Abstract The specification discloses a method for reducing current leakage and enhancing UV stability by using electrochemichromic solutions whose solvents include, either solely or in combination with other solvents, glutaronitrile (GNT).

Inventors

  • 👤 Desaraju V. Varaprasad
  • 👤 Hamid R. Habibi
  • 👤 Niall R. Lynam
  • 👤 Padma Desaraju

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 11:06
CPC Classifications
C; C09; C09K; C09K9/00; C09K9/02; G; G02; G02F; G02F1/00; G02F1/01; G02F1/15; G02F1/1503

Claims Analysis

Total Claims: 46
Claim 1
Independent Claim 81 words
A method for reducing leakage current and enhancing UV stability/in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage said method comprising: using a solvent for said redox chemical pair comprising at least 25% by volume glutaronitrile.
Claim 2
Independent Claim 81 words
A method for reducing leakage current and enhancing UV stability/in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage said method comprising: using a solvent for said redox chemical pair comprising at least 25% by volume glutaronitrile.
Claim 3
Dependent Claim 14 words
The method of claim 1 which additionally includes introducing an electrolyte into said solution.
Claim 4
Independent Claim 91 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising glutaronitrile and 3-methylsulfolane in a ratio by volume of from about 75:25 to about 25:75.
Claim 5
Independent Claim 91 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising glutaronitrile and 3-methylsulfolane in a ratio by volume of from about 75:25 to about 25:75.
Claim 6
Independent Claim 91 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising glutaronitrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 7
Independent Claim 91 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising glutaronitrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 8
Independent Claim 91 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising glutaronitrile and 3-hydroxypropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 9
Independent Claim 91 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising glutaronitrile and 3-hydroxypropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 10
Independent Claim 92 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising propylene carbonate and glutaronitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 11
Independent Claim 92 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said method comprising: using a solvent for said redox chemical pair comprising propylene carbonate and glutaronitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 12
Independent Claim 143 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair comprising a cathodic material selected from the group consisting of one of methyl, ethyl, benzyl and heptylviologen or mixtures thereof, with a counterion selected from the group consisting of one of perchlorate, tetrafluoroborate, trifluoromethanesulfonate, hexafluorophosphate, hexafluoroarsenate and mixtures thereof and an anodic material selected from the group consisting of: DMPA--5,10-dihydro-5,10-dimethylphenazine, DEPA--5,10-dihydro-5,10-diethylphenazine, DOPA--5,10-dihydro-5,10-dioctylphenazine, TMPD--N,N,N',N'-tetramethylphenylenediamine, TMBZ--N,N,N',N'-tetramethylbenzidine, TTF--Tetrathiafulvalene and mixtures thereof, said method comprising: using a solvent for said redox chemical pair comprising at least 25% by volume glutaronitrile.
Claim 13
Independent Claim 143 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair comprising a cathodic material selected from the group consisting of one of methyl, ethyl, benzyl and heptylviologen or mixtures thereof, with a counterion selected from the group consisting of one of perchlorate, tetrafluoroborate, trifluoromethanesulfonate, hexafluorophosphate, hexafluoroarsenate and mixtures thereof and an anodic material selected from the group consisting of: DMPA--5,10-dihydro-5,10-dimethylphenazine, DEPA--5,10-dihydro-5,10-diethylphenazine, DOPA--5,10-dihydro-5,10-dioctylphenazine, TMPD--N,N,N',N'-tetramethylphenylenediamine, TMBZ--N,N,N',N'-tetramethylbenzidine, TTF--Tetrathiafulvalene and mixtures thereof, said method comprising: using a solvent for said redox chemical pair comprising at least 25% by volume glutaronitrile.
Claim 14
Dependent Claim 24 words
The electrochemichromic solution of claim 7 in which said anodic and cathodic materials are employed at from about 0.02 to about 0.05 molar concentrations.
Claim 15
Independent Claim 122 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair comprising a cathodic material and an anodic material, said cathodic material consisting of one of methyl and ethylviologen and mixtures thereof, using one of hexafluorophosphate, hexafluoroarsenate and mixtures thereof as counterion, and said anodic material is 5,10-dihydro-5,10-dimethylphenazine, said method comprising: using a solvent for said redox chemical pair comprising at least 25% by volume glutaronitrile.
Claim 16
Independent Claim 122 words
A method for reducing leakage current and enhancing UV stability in an electrochemichromic cell having spaced plates, each having an inwardly facing conductive surface, and a solution located in said cell between said plates, said solution comprising a redox chemical pair which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair comprising a cathodic material and an anodic material, said cathodic material consisting of one of methyl and ethylviologen and mixtures thereof, using one of hexafluorophosphate, hexafluoroarsenate and mixtures thereof as counterion, and said anodic material is 5,10-dihydro-5,10-dimethylphenazine, said method comprising: using a solvent for said redox chemical pair comprising at least 25% by volume glutaronitrile.
Claim 17
Dependent Claim 19 words
The electrochemichromic solution of claim 9 in which said anodic and cathodic materials are employed at 0.025 molar concentration.
Claim 18
Dependent Claim 69 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including at least 25% by volume of glutaronitrile.
Claim 19
Dependent Claim 69 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including at least 25% by volume of glutaronitrile.
Claim 20
Dependent Claim 20 words
The electrochemichromic cell of claim 11 in which said electrochemichromic solution additionally includes an electrolyte in solution in said solvent.
Claim 21
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including glutaronitrile and 3-methylsulfolane in a ratio by volume of from about 75:25 to about 25:75.
Claim 22
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including glutaronitrile and 3-methylsulfolane in a ratio by volume of from about 75:25 to about 25:75.
Claim 23
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including glutaronitrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 24
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including glutaronitrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 25
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including glutaronitrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 26
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including glutaronitrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 27
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including 3-hydroxypropionitrile and glutaronitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 28
Dependent Claim 78 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage; said solvent including 3-hydroxypropionitrile and glutaronitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 29
Dependent Claim 131 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair comprising a cathodic material selected from the group consisting of one of methyl, ethyl, benzyl and heptylviologen or mixtures thereof, with a counterion selected from the group consisting of one of perchlorate, tetrafluoroborate, trifluoromethanesulfonate, hexafluorophosphate, hexafluoroarsenate and mixtures thereof and an anodic material selected from the group consisting of: DMPA--5,10-dihydro-5,10-dimethylphenazine, DEPA--5,10-dihydro-5,10-diethylphenazine, DOPA--5,10-dihydro-5,10-dioctylphenazine, TMPD--N,N,N',N'-tetramethylphenylenediamine, TMBZ--N,N,N',N'-tetramethylbenzidine, TTF--Tetrathiafulvalene and mixtures thereof, said solvent including at least 25% by volume of glutaronitrile.
Claim 30
Dependent Claim 131 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair comprising a cathodic material selected from the group consisting of one of methyl, ethyl, benzyl and heptylviologen or mixtures thereof, with a counterion selected from the group consisting of one of perchlorate, tetrafluoroborate, trifluoromethanesulfonate, hexafluorophosphate, hexafluoroarsenate and mixtures thereof and an anodic material selected from the group consisting of: DMPA--5,10-dihydro-5,10-dimethylphenazine, DEPA--5,10-dihydro-5,10-diethylphenazine, DOPA--5,10-dihydro-5,10-dioctylphenazine, TMPD--N,N,N',N'-tetramethylphenylenediamine, TMBZ--N,N,N',N'-tetramethylbenzidine, TTF--Tetrathiafulvalene and mixtures thereof, said solvent including at least 25% by volume of glutaronitrile.
Claim 31
Dependent Claim 24 words
The electrochemichromic solution of claim 17 in which said anodic and cathodic materials are employed at from about 0.02 to about 0.05 molar concentrations.
Claim 32
Dependent Claim 110 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair including a cathodic material and an anodic material, said cathodic material consisting of one of methyl and ethylviologen and mixtures thereof, using one of hexafluorophosphate, hexafluoroarsenate and mixtures thereof as counterion, and said anodic material is 5,10-dihydro-5,10-dimethylphenazine, said solvent including at least 25% by volume of glutaronitrile.
Claim 33
Dependent Claim 110 words
An electrochemichromic cell comprising: spaced plates, each having an inwardly facing conductive surface; an electrochemichromic solution in said cell, between said spaced plates, said solution comprising: solvent; and a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said redox pair including a cathodic material and an anodic material, said cathodic material consisting of one of methyl and ethylviologen and mixtures thereof, using one of hexafluorophosphate, hexafluoroarsenate and mixtures thereof as counterion, and said anodic material is 5,10-dihydro-5,10-dimethylphenazine, said solvent including at least 25% by volume of glutaronitrile.
Claim 34
Dependent Claim 19 words
The electrochemichromic solution of claim 19 in which said anodic and cathodic materials are employed at 0.025 molar concentration.
Claim 35
Independent Claim 213 words
A method for filling an electrochemichromic cell having relatively closely spaced plates, each having an inwardly facing conductive surface, said spaced plates being sealed around the periphery by a seal, said filling method comprising: introducing a small gap int said seal of an empty cell; placing said cell in a chamber along with a container of an electrochemichromic solution and evacuating said chamber; lowering said cell into said container of electrochemichromic solution such that said gap is located under the surface of the electrochemichromic solution which solution comprises a solvent, a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said solvent including at least 25% by volume of glutaronitrile; said peripheral seal enclosing an area of each of said plates; said solvent having a vapor pressure such that said vapor pressure, expressed in units of millimeters of mercury, multiplied by said area, expressed in units of square centimeters, is less than 5.969; exposing said electrochemichromic solution to a source of inert gas of pressure greater than that in said cell to thereby cause said solution to flow into said cell; sealing said gap in said peripheral seal of said cell.
Claim 36
Independent Claim 213 words
A method for filling an electrochemichromic cell having relatively closely spaced plates, each having an inwardly facing conductive surface, said spaced plates being sealed around the periphery by a seal, said filling method comprising: introducing a small gap int said seal of an empty cell; placing said cell in a chamber along with a container of an electrochemichromic solution and evacuating said chamber; lowering said cell into said container of electrochemichromic solution such that said gap is located under the surface of the electrochemichromic solution which solution comprises a solvent, a redox chemical pair in solution in said solvent which colors in the presence of an applied voltage and which bleaches to a colorless condition in the absence of an applied voltage, said solvent including at least 25% by volume of glutaronitrile; said peripheral seal enclosing an area of each of said plates; said solvent having a vapor pressure such that said vapor pressure, expressed in units of millimeters of mercury, multiplied by said area, expressed in units of square centimeters, is less than 5.969; exposing said electrochemichromic solution to a source of inert gas of pressure greater than that in said cell to thereby cause said solution to flow into said cell; sealing said gap in said peripheral seal of said cell.
Claim 37
Dependent Claim 33 words
The method of claim 21 in which said exposing step comprises subsequently venting said chamber to atmospheric pressure; said method also including removing said cell from said container prior to said sealing step.
Claim 38
Dependent Claim 24 words
The method of claim 22 in which said vacuum chamber is pressurized to above atmospheric pressure after it has been vented to atmospheric pressure.
Claim 39
Dependent Claim 20 words
The method of claim 23 in which said electrochemichromic solution is cooled prior to backfilling to reduce its vapor pressure.
Claim 40
Dependent Claim 20 words
The method of claim 22 in which said electrochemichromic solution is cooled prior to backfilling to reduce its vapor pressure.
Claim 41
Dependent Claim 25 words
The method of claim 21 in which said solvent comprises: glutaronitrile and 3-methylsulfolane in a ratio by volume of from about 75:25 to about 25:75.
Claim 42
Dependent Claim 25 words
The method of claim 21 in which said solvent comprises: glutarontrile and 3,3'-oxydipropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 43
Dependent Claim 25 words
The method of claim 21 in which said solvent comprises: glutaronitrile and 3-hydroxypropionitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 44
Dependent Claim 26 words
The method of claim 21 in which said solvent comprises: propylene carbonate and glutaronitrile in a ratio by volume of from about 75:25 to about 25:75.
Claim 45
Dependent Claim 12 words
The method of claim 21 in which said inert gas is nitrogen.
Claim 46
Dependent Claim 20 words
The method of claim 21 in which said area of said enclosed plates is at least 110 cm 2 .

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-09-29 1996-03-30 1996-09-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-09-29 2000-03-30 2000-09-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-09-29 2004-03-30 2004-09-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag