US5145929A Expired / Lapsed US ⏱️ 0.0 years remaining

Pressure-activated adhesives

Assignee: 3M Co
•
Filing: 1991-06-24
•
Granted: 1992-09-08
•
Expires: 2011-06-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Pressure-activated adhesive that is a copolymer of butadiene and acrylonitrile or methacrylonitrile. The copolymer has a single glass transition temperature of no higher than about -25° C., a nitrile content of no greater than about 31%, preferably of from about 18% by weight to about 30% by weight, a Mooney viscosity of at least 95 (measured according to ASTM D1646-87 at 100° C. for 4 minutes), preferably from about 120 to about 150. The copolymer is not cross-linked, and the amount of vinyl groups in the copolymer should not exceed 10% by weight. The adhesive can be used to form an adhesive layer of an adhesive tape.

Inventors

  • 👤 David T. Ou-Yang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 19:31
CPC Classifications
C; C09; C09J; C09J109/00; C09J109/02; C08; C08F; C08F236/00; C08F236/02; C08F236/04; C08F236/12

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 97 words
An adhesive composition comprising an amorphous butadiene-nitrile random copolymer having a single glass transition temperature no higher than about -25° C., a nitrile content no higher than about 31% by weight, a Mooney viscosity of at least 95 (measured according to ASTM D1646-87 at 100° C. for 4 minutes), a vinyl content of no greater than 10% by weight, said composition being substantially free of cross-links, provided that said composition is free of any additive that provides more than little or no finger tack or that adversely affects the cohesive and adhesive strength of the adhesive composition.
Claim 2
Dependent Claim 97 words
An adhesive composition comprising an amorphous butadiene-nitrile random copolymer having a single glass transition temperature no higher than about -25° C., a nitrile content no higher than about 31% by weight, a Mooney viscosity of at least 95 (measured according to ASTM D1646-87 at 100° C. for 4 minutes), a vinyl content of no greater than 10% by weight, said composition being substantially free of cross-links, provided that said composition is free of any additive that provides more than little or no finger tack or that adversely affects the cohesive and adhesive strength of the adhesive composition.
Claim 3
Dependent Claim 24 words
The composition of claim 1, wherein the nitrile content of said adhesive composition is from about 18% by weight to about 30% by weight.
Claim 4
Dependent Claim 20 words
The composition of claim 1, wherein the Mooney viscosity of said adhesive composition is from about 120 to about 150.
Claim 5
Dependent Claim 15 words
The composition of claim 1, wherein the nitrile moiety of said adhesive composition is acrylonitrile.
Claim 6
Dependent Claim 15 words
The composition of claim 1, wherein the nitrile moiety of said adhesive composition is methacrylonitrile.
Claim 7
Dependent Claim 19 words
A tape comprising a backing bearing on at least one major surface thereof the adhesive composition of claim 1.
Claim 8
Dependent Claim 19 words
A sheet comprising a backing bearing on at least one major surface thereof the adhesive composition of claim 1.
Claim 9
Dependent Claim 19 words
A label comprising a backing bearing on at least one major surface thereof the adhesive composition of claim 1.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-09-08 1996-03-09 1996-09-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-09-08 2000-03-09 2000-09-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-09-08 2004-03-09 2004-09-08 $7700.00 Window Closed / Lapsed