Abstract
Abstract Strain within a substrate is measured by attaching thereto a magnetic circuit comprising a magnetostrictive, soft ferromagnetic element, and sensing a change in the coercive field of the element caused by strain therewith.
Inventors
- 👤 Gordon E. Fish
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-24 08:38
CPC Classifications
G; G01; G01B; G01B7/00; G01B7/16; G01B7/24; Y; Y10; Y10S; Y10S977/00; Y10S977/70; Y10S977/773; Y10S977/775; Y10S977/776; Y10S977/81; Y10S977/832; Y10S977/838; Y10S977/902; Y10S977/932; Y10S977/953; Y10S977/96
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
307 words
A method of measuring strain within a substrate comprising the steps of: i. attaching a magnetic circuit to said substrate, said magnetic circuit comprising a magnetostrictive, soft ferromagnetic element adapted to produce a coercive force in the presence of an applied magnetic field; ii. sensing a change in the coercive field of said ferromagnetic element caused by strain therewithin, said change in said coercive field being measured by a method comprising the steps of: (a) applying a first magnetomotive force to said magnetic circuit, said magnetomotive force having sufficient magnitude to reverse the direction of magnetization of a majority of the volume of said ferromagnetic element; (b) removing said first magnetomotive force; (c) applying a second magnetomotive force to said magnetic circuit in a direction opposite to that of said first magnetomotive force while sensing the magnetization of said ferromagnetic element, said first and second magnetomotive forces being applied by passing an alternating electrical current through a drive coil of at least one turn of winding enclosing an element of said magnetic circuit; (d) increasing the magnitude of said second magnetomotive force to a magnitude at least sufficient to reduce the magnetization of said ferromagnetic element to zero; and (e) determining the change in magnetic field applied to said ferromagnetic element by that magnetomotive force which reduces magnetization of said ferromagnetic element to zero caused by strain therewithin, said magnetization of said ferromagnetic element being sensed using a sense coil of at least one turn of winding enclosing an element of said magnetic circuit and said change in magnetic field of said ferromagnetic element being determined by sending a change in the time for the occurrence of voltage peaks in said sense coil, said time being measured relative to the waveform of said alternating electrical current, said change in time being a measure of said coercive field.
Claim 2
Independent Claim
307 words
A method of measuring strain within a substrate comprising the steps of: i. attaching a magnetic circuit to said substrate, said magnetic circuit comprising a magnetostrictive, soft ferromagnetic element adapted to produce a coercive force in the presence of an applied magnetic field; ii. sensing a change in the coercive field of said ferromagnetic element caused by strain therewithin, said change in said coercive field being measured by a method comprising the steps of: (a) applying a first magnetomotive force to said magnetic circuit, said magnetomotive force having sufficient magnitude to reverse the direction of magnetization of a majority of the volume of said ferromagnetic element; (b) removing said first magnetomotive force; (c) applying a second magnetomotive force to said magnetic circuit in a direction opposite to that of said first magnetomotive force while sensing the magnetization of said ferromagnetic element, said first and second magnetomotive forces being applied by passing an alternating electrical current through a drive coil of at least one turn of winding enclosing an element of said magnetic circuit; (d) increasing the magnitude of said second magnetomotive force to a magnitude at least sufficient to reduce the magnetization of said ferromagnetic element to zero; and (e) determining the change in magnetic field applied to said ferromagnetic element by that magnetomotive force which reduces magnetization of said ferromagnetic element to zero caused by strain therewithin, said magnetization of said ferromagnetic element being sensed using a sense coil of at least one turn of winding enclosing an element of said magnetic circuit and said change in magnetic field of said ferromagnetic element being determined by sending a change in the time for the occurrence of voltage peaks in said sense coil, said time being measured relative to the waveform of said alternating electrical current, said change in time being a measure of said coercive field.
References Cited (Backward Citations)
GB442441A
Cited
JPS4828293A
Cited
SU767574A1
Cited
JPS56101527A
Cited
US4449095A
Cited
US4623841A
Cited
US4931730A
Cited
US4931729A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1995-08-25 | 1996-02-24 | 1996-08-25 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1999-08-25 | 2000-02-24 | 2000-08-25 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2003-08-25 | 2004-02-24 | 2004-08-25 | $7700.00 | Window Closed / Lapsed |