Claims Analysis
Total Claims: 32
Claim 1
Independent Claim
141 words
A method for bonding first and second hydrogel lens members to one another including: providing a first hydrogel lens member having a bonding surface; providing a second hydrogel lens member having a bonding surface with an energy director extending from the surface, the energy director having an extended smooth surface configured to engage the bonding surface of the first lens member; mating the smooth extended surface of the energy director of the second lens member with the bonding surface of the first lens member; applying pressure to the lens members to force them together; applying ultrasonic energy to the lens members for a weld time period; discontinuing the application of ultrasonic energy to the lens members for a hold time period following the weld time period; and discontinuing the application of pressure to the lens members following the hold time period.
Claim 2
Independent Claim
141 words
A method for bonding first and second hydrogel lens members to one another including: providing a first hydrogel lens member having a bonding surface; providing a second hydrogel lens member having a bonding surface with an energy director extending from the surface, the energy director having an extended smooth surface configured to engage the bonding surface of the first lens member; mating the smooth extended surface of the energy director of the second lens member with the bonding surface of the first lens member; applying pressure to the lens members to force them together; applying ultrasonic energy to the lens members for a weld time period; discontinuing the application of ultrasonic energy to the lens members for a hold time period following the weld time period; and discontinuing the application of pressure to the lens members following the hold time period.
Claim 3
Dependent Claim
46 words
The method of claim 1 wherein: providing the first hydrogel lens member includes providing a first lens member having an annular bonding surface; and providing a second hydrogel lens member includes providing a second lens member having an annular bonding surface with an annular energy director.
Claim 4
Dependent Claim
34 words
The method of claim 2 wherein providing a second hydrogel lens member includes providing a second lens member with an annular energy director having a height in the range of 0.127 to 0.178 millimeter.
Claim 5
Dependent Claim
34 words
The method of claim 2 wherein providing a second hydrogel lens member includes providing a second lens member with an annular energy director having an extended smooth surface of 0.127 to 0.381 millimeter width.
Claim 6
Dependent Claim
27 words
The method of claim 2 wherein providing a second hydrogel lens member includes providing a second lens member with an energy director having a rectangular cross section.
Claim 7
Dependent Claim
28 words
The method of claim 2 wherein providing a second hydrogel lens member includes providing a second lens member with an energy director having one or more slots therethrough.
Claim 8
Independent Claim
28 words
The method of claim I wherein applying pressure to the lens members includes applying a pressure of 55.1 K to 68.9 K Newtons/square meter to the lens members.
Claim 9
Dependent Claim
23 words
The method of claim 1 wherein applying ultrasonic energy includes applying ultrasonic energy for a weld time period of 0.15 to 0.22 second.
Claim 10
Dependent Claim
33 words
The method of claim 1 wherein discontinuing the application of ultrasonic energy includes discontinuing the application of ultrasonic energy to the lens members for a hold time period of 0.15 to 0.25 second.
Claim 11
Dependent Claim
29 words
The method of claim 1 wherein applying ultrasonic energy includes: monitoring the peak energy applied to the lens members; and applying peak ultrasonic energy of 10 to 25 Joules.
Claim 12
Dependent Claim
19 words
The method of claim 1 wherein applying ultrasonic energy includes applying 40 KHz ultrasonic energy to the lens members.
Claim 13
Dependent Claim
29 words
The method of claim 1 wherein providing first and second hydrogel lens members includes providing first and second hydrogel lens members having an equilibrium moisture content greater than 25.0%.
Claim 14
Dependent Claim
29 words
The method of claim 12 wherein providing first and second hydrogel lens members includes providing first and second hydrogel lens members having an equilibrium moisture content greater than 35.0%.
Claim 15
Dependent Claim
29 words
The method of claim 13 wherein providing first and second hydrogel lens members includes providing first and second hydrogel lens members having an equilibrium moisture content greater than 55.0%.
Claim 16
Independent Claim
190 words
A method for bonding first and second hydrogel lens members to one another, including: providing a first hydrogel lens member having an annular bonding surface and an equilibrium moisture content greater than 25.0%; providing a second hydrogel lens member having an annular bonding surface with an annular energy director extending from the surface and an equilibrium moisture content greater than 25.0%, the energy director having a generally rectangular cross-section, a height of 0.127 to 0.178 millimeter, and an extended smooth surface of 0.127-0.381 millimeter width configured to engage the bonding surface of the first lens member; mating the smooth extended surface of the energy director of the second lens member with the bonding surface of the first lens member; applying a pressure of 55.1 K to 68.9 K Newtons/square meter to the lens members to force them together; applying ultrasonic energy to the lens members for a weld time period of 0.15-0.22 second; discontinuing the application of ultrasonic energy to the lens members for a hold time period of 0.15-0.25 second following the weld period; and discontinuing the application of pressure to the lens members following the hold time period.
Claim 17
Independent Claim
190 words
A method for bonding first and second hydrogel lens members to one another, including: providing a first hydrogel lens member having an annular bonding surface and an equilibrium moisture content greater than 25.0%; providing a second hydrogel lens member having an annular bonding surface with an annular energy director extending from the surface and an equilibrium moisture content greater than 25.0%, the energy director having a generally rectangular cross-section, a height of 0.127 to 0.178 millimeter, and an extended smooth surface of 0.127-0.381 millimeter width configured to engage the bonding surface of the first lens member; mating the smooth extended surface of the energy director of the second lens member with the bonding surface of the first lens member; applying a pressure of 55.1 K to 68.9 K Newtons/square meter to the lens members to force them together; applying ultrasonic energy to the lens members for a weld time period of 0.15-0.22 second; discontinuing the application of ultrasonic energy to the lens members for a hold time period of 0.15-0.25 second following the weld period; and discontinuing the application of pressure to the lens members following the hold time period.
Claim 18
Dependent Claim
15 words
The method of claim 15 wherein applying ultrasonic energy includes applying 40 KHz ultrasonic energy.
Claim 19
Dependent Claim
38 words
The method of claim 15 wherein applying ultrasonic energy includes: monitoring the peak value of the ultrasonic energy applied to the lens members; and applying ultrasonic energy to achieve a peak energy value of 10 to 25 Joules.
Claim 20
Dependent Claim
28 words
The method of claim 15 wherein providing first and second hydrogel lens members includes providing first and second lens members having an equilibrium moisture content greater than 25.0%.
Claim 21
Dependent Claim
28 words
The method of claim 18, wherein providing first and second hydrogel lens members includes providing first and second lens members having an equilibrium moisture content greater than 35.0%.
Claim 22
Dependent Claim
28 words
The method of claim 19, wherein providing first and second hydrogel lens members includes providing first and second lens members having an equilibrium moisture content greater than 55.0%.
Claim 23
Independent Claim
130 words
A method for bonding first and second hydrogel lens members to one another including: providing a first hydrogel lens member having a bonding surface and an equilibrium moisture content greater than 25.0%; providing a second hydrogel lens member having a bonding surface configured to engage the bonding surface of the first lens member and an equilibrium moisture content greater than 25.0%; mating the bonded surface of the second lens member with the bonding surface of the first lens member; applying pressure to the lens members to force them together; applying ultrasonic energy to the lens members for a weld time period; to the lens members for a hold time period following the weld time period; and discontinuing the application of pressure to the lens members following the hold time period.
Claim 24
Independent Claim
130 words
A method for bonding first and second hydrogel lens members to one another including: providing a first hydrogel lens member having a bonding surface and an equilibrium moisture content greater than 25.0%; providing a second hydrogel lens member having a bonding surface configured to engage the bonding surface of the first lens member and an equilibrium moisture content greater than 25.0%; mating the bonded surface of the second lens member with the bonding surface of the first lens member; applying pressure to the lens members to force them together; applying ultrasonic energy to the lens members for a weld time period; to the lens members for a hold time period following the weld time period; and discontinuing the application of pressure to the lens members following the hold time period.
Claim 25
Dependent Claim
62 words
The method of claim 21 wherein: providing the first hydrogel lens member includes providing a first lens member having an annular bonding surface; and providing a second hydrogel lens member includes providing a second lens member having an annular bonding surface with an annular energy director extending from the surface and configured to engage the bonding surface of the first lens member.
Claim 26
Dependent Claim
28 words
The method of claim 21 wherein applying pressure to the lens members includes applying a pressure of 55.1 K to 68.9 K Newtons/square meter to the lens members.
Claim 27
Dependent Claim
23 words
The method of claim 21 wherein applying ultrasonic energy includes applying ultrasonic energy for a weld time period of 0.15 to 0.22 second.
Claim 28
Dependent Claim
33 words
The method of claim 21 wherein discontinuing the application of ultrasonic energy includes discontinuing the application of ultrasonic energy to the lens members for a hold time period of 0.15 to 0.25 second.
Claim 29
Dependent Claim
29 words
The method of claim 21 wherein applying ultrasonic energy includes: monitoring the peak energy applied to the lens members; and applying peak ultrasonic energy of 10 to 25 Joules.
Claim 30
Dependent Claim
19 words
The method of claim 21 wherein applying ultrasonic energy includes applying 40 KHz ultrasonic energy to the lens members.
Claim 31
Dependent Claim
28 words
The method of claim 21 wherein providing first and second hydrogel lens members includes providing first and second lens members having an equilibrium moisture content greater than 35.0%.
Claim 32
Dependent Claim
29 words
The method claim of claim 28 wherein providing first and second hydrogel lens members includes providing first and second lens members having an equilibrium moisture content greater than 55.0%.