Abstract

Abstract Organic pressure-sensitive adhesive and silicone pressure-sensitive adhesive composites have improved shear strength upon the addition of a silicone cross-linking agent.

Inventors

  • 👤 Frank J. Traver
  • 👤 Duane F. Merrill

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 13:34
CPC Classifications
C; C09; C09J; C09J133/00; C09J133/04; C09J133/06; C08; C08F; C08F8/00; C08F8/42; C09J121/00; C09J183/00; C09J183/04; C09J7/00; C09J7/30; C09J7/38; C08L; C08L2205/00; C08L2205/04; C08L2666/00; C08L2666/02; C08L2666/04; C08L2666/14; C08L83/00; C08L83/04; C09J2301/00; C09J2301/30; C09J2301/302

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 139 words
A method for controlling the release properties and increasing the shear strength of an organic pressure-sensitive adhesive which comprises: (a) adding to an organic pressure-sensitive adhesive a release control additive comprising: (i) a silicone pressure-sensitive adhesive, (ii) a silicone cross-linking agent, and (iii) a compatibilizing agent selected from the group consisting of an emulsifying agent compatible with both the silicone pressure-sensitive adhesive and the organic pressure-sensitive adhesive and a solvent capable of dissolving both the silicone pressure-sensitive adhesive and the organic pressure-sensitive adhesive in an amount such that from about 50 to about 99% by weight is the organic pressure-sensitive adhesive and from about 1 to about 50% by weight is the release control additive and (b) mixing the organic pressure-sensitive adhesive together with the release control additive whereby the adhesive and the additive form a compatible uniform mixture.
Claim 2
Independent Claim 139 words
A method for controlling the release properties and increasing the shear strength of an organic pressure-sensitive adhesive which comprises: (a) adding to an organic pressure-sensitive adhesive a release control additive comprising: (i) a silicone pressure-sensitive adhesive, (ii) a silicone cross-linking agent, and (iii) a compatibilizing agent selected from the group consisting of an emulsifying agent compatible with both the silicone pressure-sensitive adhesive and the organic pressure-sensitive adhesive and a solvent capable of dissolving both the silicone pressure-sensitive adhesive and the organic pressure-sensitive adhesive in an amount such that from about 50 to about 99% by weight is the organic pressure-sensitive adhesive and from about 1 to about 50% by weight is the release control additive and (b) mixing the organic pressure-sensitive adhesive together with the release control additive whereby the adhesive and the additive form a compatible uniform mixture.
Claim 3
Dependent Claim 52 words
The method of claim 1 wherein said organic pressure-sensitive adhesive is selected from the group consisting of milled natural rubber, styrene-butadiene rubber, butyl rubber, butadiene-acrylonitrile rubber, polyvinyl ether rubber, polyacrylate ester rubber, styrene-butadiene-styrene rubber, and styrene-isoprene-styrene rubber and said emulsifying agent is a primary or secondary amine salt of an organic acid.
Claim 4
Dependent Claim 15 words
The method of claim 1 wherein said organic pressure-sensitive adhesive is selected from styrene-butadiene rubber.
Claim 5
Dependent Claim 23 words
The method of claim 2 wherein said primary or secondary amine salt of an organic acid is the morpholine salt of undecylenic acid.
Claim 6
Dependent Claim 19 words
The method of claim 1 wherein said silicone pressure-sensitive adhesive is a mixture of silicone resin and silicone fluid.
Claim 7
Dependent Claim 22 words
The method of claim 1 wherein said organic pressure-sensitive adhesive is selected from acrylic rubber and said emulsifying agent is an ethoxylate.
Claim 8
Dependent Claim 12 words
The method of claim 6 wherein said ethoxylate is an aryl ethoxylate.
Claim 9
Dependent Claim 10 words
The method of claim 1 wherein water is also present.
Claim 10
Dependent Claim 31 words
The method of claim 8 wherein said emulsifying agent is present in an amount of from about 1/2 to about 3 parts by weight for each 100 parts by weight water.
Claim 11
Dependent Claim 16 words
The method of claim 1 wherein said silicone cross-linking agent is selected from peroxide cross-linking agents.
Claim 12
Dependent Claim 33 words
The method of claim 10 wherein said silicone cross-linking agent is selected from the group consisting of diaroyl peroxides, dialkyl peroxides, diaralkyl peroxides, alkyl aralkyl peroxides, alkyl arolyl peroxide and alkyl acyl peroxide.
Claim 13
Dependent Claim 30 words
The method of claim 10 wherein said peroxide cross-linking agent is present in an amount ranging from about 0.01 to about 3% by weight based on silicone pressure-sensitive adhesive content.
Claim 14
Dependent Claim 21 words
The method of claim 1 wherein said silicone cross-linking agent is selected from alkoxy silane cross-linking agents with a cross-linking catalyst.
Claim 15
Dependent Claim 26 words
The method of claim 13 wherein said silicone cross-linking agent is selected from the group consisting of methyltrimethoxy silane, ethyl silicate, gamma-aminopropyltrimethoxy silane and triethoxy silane.
Claim 16
Dependent Claim 31 words
The method of claim 13 wherein said alkoxy silane cross-linking agent is present in an amount ranging from about 1 to about 10% by weight based on silicone pressure-sensitive adhesive content.
Claim 17
Dependent Claim 36 words
The method of claim 1 wherein the mixture comprises: (i) from about 3 to about 30% by weight of organic pressure-sensitive adhesive, and (ii) from about 70 to about 97% by weight of silicone pressure-sensitive adhesive.

References Cited (Backward Citations)

US2857356A Cited
US4423095A Cited
US4505976A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-07-07 1996-01-06 1996-07-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-07-07 2000-01-06 2000-07-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-07-07 2004-01-06 2004-07-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag