Abstract

Abstract A method of developing a silver halide photographic material is disclosed. The method comprises a step of supplying a developer to a surface of an exposed silver halide photographic material, which is transferred by at least one pair of rollers, intermittently at least twice wherein an interval time of each supplying is not more than 10 seconds and the amount of developer retained in the light-sensitive material ranges from 50 to 250 ml/m 2 . The method provides a compact developing system, which is free from uneven development with good grainess of the image.

Inventors

  • 👤 Kiyoshi Sato
  • 👤 Masaaki Taguchi
  • 👤 Yasunori Wada
  • 👤 Mikio Kawasaki
  • 👤 Shinichi Ohtani
  • 👤 Masatosi Iwada
  • 👤 Noboru Hatakeyama

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 09:50
CPC Classifications
G; G03; G03D; G03D5/00; G03D5/04; G03C; G03C5/00; G03C5/26; G03C5/29; G03C5/30; G03C5/305; G03C5/3053; Y; Y10; Y10S; Y10S430/00; Y10S430/164

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 76 words
A method of developing a silver halide photographic material, comprising a step of supplying a developer at least twice and intermittently, with an interval time of each supplying being not more than 10 seconds, to a surface of an exposed silver halide photographic material, wherein the photographic material is transferred between at least a pair of rollers and wherein the amount of developer retained in the light-sensitive material ranges from 50 to 250 ml/m 2 .
Claim 2
Independent Claim 76 words
A method of developing a silver halide photographic material, comprising a step of supplying a developer at least twice and intermittently, with an interval time of each supplying being not more than 10 seconds, to a surface of an exposed silver halide photographic material, wherein the photographic material is transferred between at least a pair of rollers and wherein the amount of developer retained in the light-sensitive material ranges from 50 to 250 ml/m 2 .
Claim 3
Dependent Claim 21 words
A method as claimed in claim 1, wherein the developer is supplied to more than one surface of the photographic material.
Claim 4
Dependent Claim 27 words
A method as claimed in claim 1, wherein an amount of the supplied developer is 50 to 180 ml per 1 m 2 of the photographic material.
Claim 5
Dependent Claim 18 words
A method as claimed in claim 1, wherein the at least one of the rollers is kept warm.
Claim 6
Dependent Claim 20 words
A method as claimed in claim 1, wherein the viscosity of the developer is 3 to 100CP at 20° C.
Claim 7
Dependent Claim 23 words
A method as claimed in claim 1, wherein the developer comprises carboxymethylcellulose in an amount of 0.5 to 2.5 g per liter developer.
Claim 8
Dependent Claim 19 words
A method as claimed in claim 1, wherein the developer is supplied to the photographic material by the rollers.
Claim 9
Dependent Claim 19 words
A method as claimed in claim 1, wherein the developer is supplied between the rollers and the photographic material.

References Cited (Backward Citations)

DE1447043A1 Cited
US3334566A Cited
US3826228A Cited
US3960567A Cited
US4562140A Cited
US4868098A Cited
JPS63235940A Cited
US4954425A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-05-19 1995-11-18 1996-05-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-05-19 1999-11-18 2000-05-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-05-19 2003-11-18 2004-05-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag