Abstract

Abstract A magnetic recording medium comprising a non-magnetic substrate, a primer coating formed on the substrate and comprising an organic conducting polymer and a magnetic layer formed on the primer coating, which has good surface smoothness and low surface resistance.

Inventors

  • 👤 Akira Miyake
  • 👤 Tsugihiro Doi
  • 👤 Minoru Ezoe
  • 👤 Akira Ohtani

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 17:36
CPC Classifications
G; G11; G11B; G11B5/00; G11B5/62; G11B5/73; Y; Y10; Y10S; Y10S428/00; Y10S428/90; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31855

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 167 words
A magnetic recording medium comprising a non-magnetic substrate, a primer coating on said substrate and a magnetic layer on said primer coating, said primer coating being prepared by doping a polyaniline polymer with a protonic acid having a pKa value of 4.8 or less, which polymer comprises, in a undoped state, repeating units of the formula: ##STR6## wherein m and n are molar fractions of the quinonediimine repeating units and the phenylenediamine repeating units, respectively, and m is larger than 0 and smaller than 1, n is larger than 0 and smaller than 1, and the sum of m and n is 1, and provides a laser Raman spectrum recorded by exciting with a light having a wavelength of 457.9 nm in which a ratio of the Raman line strength (Ia) assigned to the ring stretching vibration appeared at a wave number range larger than 1,600 cm -1 to that (Ib) appeared at a wave number range smaller than 1,600 cm -1 (Ia/Ib) is at least 1.0.
Claim 2
Dependent Claim 167 words
A magnetic recording medium comprising a non-magnetic substrate, a primer coating on said substrate and a magnetic layer on said primer coating, said primer coating being prepared by doping a polyaniline polymer with a protonic acid having a pKa value of 4.8 or less, which polymer comprises, in a undoped state, repeating units of the formula: ##STR6## wherein m and n are molar fractions of the quinonediimine repeating units and the phenylenediamine repeating units, respectively, and m is larger than 0 and smaller than 1, n is larger than 0 and smaller than 1, and the sum of m and n is 1, and provides a laser Raman spectrum recorded by exciting with a light having a wavelength of 457.9 nm in which a ratio of the Raman line strength (Ia) assigned to the ring stretching vibration appeared at a wave number range larger than 1,600 cm -1 to that (Ib) appeared at a wave number range smaller than 1,600 cm -1 (Ia/Ib) is at least 1.0.
Claim 3
Dependent Claim 125 words
A magnetic recording medium comprising a non-magnetic substrate, a primer coating on said substrate consisting essentially of a conductive polyaniline polymer and a magnetic layer on said primer coating, said polyaniline polymer being prepared by doping said polymer with a protonic acid having a pKa value of 4.8 or less, which polymer comprises, in an undoped state, repeating units of the formula: ##STR7## wherein m and n are molar fractions of the quinonediimine repeating units and the phenylenediamine repeating units, respectively, and m is larger than 0 and smaller than 1, n is larger than 0 and smaller than 1, and the sum of m and n is 1, and has an intrinsic viscosity of at least 0.40 dl/g measured in N-methyl-2-pyrrolidone at 30° C.
Claim 4
Dependent Claim 125 words
A magnetic recording medium comprising a non-magnetic substrate, a primer coating on said substrate consisting essentially of a conductive polyaniline polymer and a magnetic layer on said primer coating, said polyaniline polymer being prepared by doping said polymer with a protonic acid having a pKa value of 4.8 or less, which polymer comprises, in an undoped state, repeating units of the formula: ##STR7## wherein m and n are molar fractions of the quinonediimine repeating units and the phenylenediamine repeating units, respectively, and m is larger than 0 and smaller than 1, n is larger than 0 and smaller than 1, and the sum of m and n is 1, and has an intrinsic viscosity of at least 0.40 dl/g measured in N-methyl-2-pyrrolidone at 30° C.

References Cited (Backward Citations)

JPS58150129A Cited
JPS6020316A Cited
US4617226A Cited
US4615829A Cited
US4762644A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-01-06 1995-07-08 1996-01-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-01-06 1999-07-08 2000-01-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-01-06 2003-07-08 2004-01-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag