Abstract

Abstract Recording and erasing optical information can be done by using an alloy film capable of forming two stable crystalline states differing in crystal texture and optical characteristics by being irradiated with optical energies under different conditions. The memory film includes 35-45 atom % of indium (In) and 55-65 atom % of antimony (Sb). The memory film may include an additional element M selected from the group consisting of Al, Si, P, S, Zn, Ga, Ge, As, Se, Ag, Cd, Sn, Te, Tl, Pb, Bi, and a combination of these elements, the composition of the memory film being expressed by the formula (In x Sb 1-x ) 1-y M y .

Inventors

  • 👤 Nagaaki Koshino
  • 👤 Miyozo Maeda
  • 👤 Yasuyuki Goto
  • 👤 Itaru Shibata
  • 👤 Kenichi Utsumi
  • 👤 Akira Ushioda
  • 👤 Ken-ichi Itoh
  • 👤 Kozo Sueishi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 21:20
CPC Classifications
G; G11; G11B; G11B7/00; G11B7/24; G11B7/241; G11B7/242; G11B7/243; G11B7/2433; G11B7/252; G11B7/257; G11B7/004; G11B2007/24302; G11B2007/2431; G11B2007/24314; G11B7/254; G11B7/2542; G11B7/2572; G11B7/2578; Y; Y10; Y10S; Y10S430/00; Y10S430/146; Y10S430/165

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 205 words
A method for recording information in a memory film of an optical information memory medium including a substrate and a thin memory film formed on the substrate capable of selectively forming two stable crystalline states, the memory film having a first crystalline state when information has been recorded and a second crystalline state when information has been erased said method comprising the steps of: (a) irradiating a first portion of the memory film with an optical energy beam having a first intensity for a first period of time such that the entire thickness of the memory film is fused at the irradiated portion for forming the first crystalline state having a first reflectivity; and (b) irradiating a second portion of the memory film with an optical energy beam having a second intensity less than or equal to the first intensity for a second period of time longer than the first period of time for forming the second crystalline state having a second reflectivity lower than the first reflectivity, whereby information is recorded at one of the first and second portions of the memory film, the memory film comprising a multi-component system including: 35-45 atom % of Indium (In) and 55-65 atom % of antimony (Sb).
Claim 2
Independent Claim 205 words
A method for recording information in a memory film of an optical information memory medium including a substrate and a thin memory film formed on the substrate capable of selectively forming two stable crystalline states, the memory film having a first crystalline state when information has been recorded and a second crystalline state when information has been erased said method comprising the steps of: (a) irradiating a first portion of the memory film with an optical energy beam having a first intensity for a first period of time such that the entire thickness of the memory film is fused at the irradiated portion for forming the first crystalline state having a first reflectivity; and (b) irradiating a second portion of the memory film with an optical energy beam having a second intensity less than or equal to the first intensity for a second period of time longer than the first period of time for forming the second crystalline state having a second reflectivity lower than the first reflectivity, whereby information is recorded at one of the first and second portions of the memory film, the memory film comprising a multi-component system including: 35-45 atom % of Indium (In) and 55-65 atom % of antimony (Sb).
Claim 3
Dependent Claim 39 words
A method according to claim 1, wherein said steps (a) and (b) include irradiating the memory film with a laser selected from the group consisting of a semiconductor laser, an He-Ne laser, an He-Cd laser and an Ar laser.
Claim 4
Dependent Claim 57 words
A method according to claim 1, wherein said steps (a) and (b) include irradiating the memory film with an optical energy for recording having a power between 3 to 20 mW for approximately 50 to 200 ns and an optical energy for erasing having a power between 1 to 8 mW for approximately 0.1 to 10 ρs.
Claim 5
Dependent Claim 31 words
A method according to claim 1, wherein said step (b) includes irradiating the memory film with an optical energy beam having an elongated shape in the circumference direction for erasing information.
Claim 6
Dependent Claim 69 words
A method according to claim 1, wherein the memory film further comprises an additional element M selected from the group consisting of Al, Si, P, S, Zn, Ga, Ge, As, Se, Ag, Cd, Sn Te, Tl, Pb, and Bi, and a combination of these elements, the composition of the memory film being expressed by the formula (In x Sb 1-x ) 1-y M y , wherein 0.35≦x≦0.45 and 0.05≦y≦0.2.

References Cited (Backward Citations)

US3868651A Cited
US4296419A Cited
US4460636A Cited
US4719594A Cited
US4653024A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-10-14 1995-04-15 1995-10-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-10-14 1999-04-15 1999-10-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-10-14 2003-04-15 2003-10-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag