Abstract

Abstract A process for treatment of incinerator ash typically including heavy metals and both water soluble and insoluble fractions. The insoluble fraction is first removed from the fly ash. The soluble fraction is treated to precipitate heavy metal compounds. Preferably, the heavy metal precipitates are incorporated in a vitrifiable batch. In a separate vitrifiable batch, the insoluble fly ash portions may also be incorporated. Most preferably, bottom ash from the incinerator is also incorporated in a glass batch. The bottom ash glass batch may also incorporate the insoluble fraction from the fly ash. Precipitation of the heavy metal constituents in the soluble portion of the fly ash is preferably accomplished by raising the pH of the solution, most preferably above 10 by addition of alkali metal or alkaline earth metal hydroxides.

Inventors

  • 👤 Dennis E. Kauser
  • 👤 Robert A. LaMastro

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 11:22
CPC Classifications
C; C03; C03C; C03C1/00; C03C1/002; Y; Y10; Y10S; Y10S106/00; Y10S106/01

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 108 words
A method for treating incinerator fly ash, to separate water insoluble carbonaceous materials, and soluble chlorides, and heavy metals, said method comprising: a) mixing said incinerator fly ash with water to form a solution of the water soluble components of said fly ash, including said chlorides and heavy metals; b) filtering water insoluble fly ash solids from said solution to remove said water insoluble carbonaceous materials; c) precipitating heavy metal compounds from the chloride-containing solution; d) separating said precipitated heavy metal compounds from said chloride-containing solution; e) incorporating said separated heavy metal compounds in a vitrifiable mixture free of chlorides and carbonaceous materials; and f) vitrifying said mixture.
Claim 2
Independent Claim 108 words
A method for treating incinerator fly ash, to separate water insoluble carbonaceous materials, and soluble chlorides, and heavy metals, said method comprising: a) mixing said incinerator fly ash with water to form a solution of the water soluble components of said fly ash, including said chlorides and heavy metals; b) filtering water insoluble fly ash solids from said solution to remove said water insoluble carbonaceous materials; c) precipitating heavy metal compounds from the chloride-containing solution; d) separating said precipitated heavy metal compounds from said chloride-containing solution; e) incorporating said separated heavy metal compounds in a vitrifiable mixture free of chlorides and carbonaceous materials; and f) vitrifying said mixture.
Claim 3
Dependent Claim 22 words
The method of claim 1 including, before step (b), the further step of: decreasing the pH of said solution to below 6.
Claim 4
Dependent Claim 41 words
The method of claim 1 including the further step of: g) incorporating said filtered water insoluble fly ash solids including said carbonaceous materials into a second vitrifiable mixture separate from said mixture produced in step e) and vitrifying said second mixture.
Claim 5
Dependent Claim 15 words
The method of claim 3 wherein said second vitrifiable mixture also includes incinerator bottom ash.
Claim 6
Dependent Claim 35 words
The method of claim 4 wherein said second mixture comprises, by weight: 10-16% Soda Lime Cullet 5-6% Aragonite 2-7% Soda Ash 0-80% Bottom Ash and said filtered insoluble fly ash solids including said carbonaceous material.
Claim 7
Dependent Claim 17 words
The method of claim 1 wherein step (c) comprises adjusting the pH of said solution to 8.5-12.5.
Claim 8
Dependent Claim 15 words
The method of claim 6 wherein the pH of said solution is adjusted to 10-10.5.
Claim 9
Dependent Claim 19 words
The method of claim 6 wherein said pH is adjusted by adding alkaline earth metal or alkali metal hydroxide.
Claim 10
Dependent Claim 25 words
The method of claim 1 wherein step (c) comprises adjusting the pH of said solution to 8-9 by addition of a water soluble phosphate compound.
Claim 11
Dependent Claim 14 words
The method of claim 9 wherein said soluble phosphate compound is diammonium mono-hydrogen phosphate.
Claim 12
Dependent Claim 44 words
The method of claim 6 wherein said mixture comprises, by weight: ______________________________________ Sand 58-62% Nepheline Syenite 0-8% and [/or] Feldspar (combined total) Soda Ash 15-20% Aragonite and 0-11% [/or] Limestone (combined total) Sodium Nitrate 0-1% Said separated heavy metal [up to] 0-25% compounds ______________________________________
Claim 13
Dependent Claim 37 words
The method of claim 1 further comprising the step of: g) treating the separated chloride-containing solution to remove residual heavy metal compounds remaining in said solution, and then evaporating said solution to separate salts from said solution.
Claim 14
Dependent Claim 32 words
The method of claim 12 wherein said residual heavy metal compounds removed from said solution in step g) are returned to the process and subsequently incorporated in a vitrifiable mixture and vitrified.

References Cited (Backward Citations)

US3188201A Cited
US3311447A Cited
US3630673A Cited
US4069315A Cited
US4065281A Cited
US4191546A Cited
US4524049A Cited
US4678493A Cited
JPS60165326A Cited
US4720295A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-08-19 1995-02-18 1995-08-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-08-19 1999-02-18 1999-08-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-08-19 2003-02-18 2003-08-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag