Abstract
Abstract Disclosed is a method for applying a yellow incandescent bugfoiler pigment coating comprising a fine-ground blend of praseodymium doped zirconium silicate and silica. This cadmium-free blend is preferably applied electrostatically in three coats to the interior of a bulb to diffuse the light and block the emitted UV wavelengths. The color of the blend will intensify with increasing heat and return to it's initial yellow color upon cooling.
Inventors
- 👤 Sarah C. Shobert
- 👤 Ronald G. Blose
- 👤 Costas C. Lagos
- 👤 Charles Wood
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 02:10
CPC Classifications
C; C09; C09K; C09K11/00; C09K11/02; C09K11/08; C09K11/77; C09K11/77062; H; H01; H01J; H01J61/00; H01J61/02; H01J61/38; H01J61/42; H01J61/44; H01J61/46; H01J9/00; H01J9/20; H01J9/22; H01J9/221; H01J9/225
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
59 words
A method of manufacturing yellow incandescent bug lights comprising electrostatically coating the interior surface of incandescent lamps with a cadmiumfree yellow pigment comprising a dry ground homogeneous blend of: a) about 90 percent by weight ZrSiO.sub. 4/Pr yellow pigment, fine-dry ground to an average particle size of about 4 microns; and b) about 10 percent by weight amorphous silica.
Claim 2
Independent Claim
59 words
A method of manufacturing yellow incandescent bug lights comprising electrostatically coating the interior surface of incandescent lamps with a cadmiumfree yellow pigment comprising a dry ground homogeneous blend of: a) about 90 percent by weight ZrSiO.sub. 4/Pr yellow pigment, fine-dry ground to an average particle size of about 4 microns; and b) about 10 percent by weight amorphous silica.
Claim 3
Independent Claim
59 words
A method of manufacturing yellow incandescent bug lights comprising electrostatically coating th interior surface of incandescent lamps with a cadmiumfree yellow pigment comprising a dry ground homogeneous blend of: a) about 90 percent by weight ZrSiO.sub. 4/Pr yellow pigment, fine-dry ground to an average particle size of about 2.8 microns; and b) about 10 percent by weight amorphous silica.
Claim 4
Independent Claim
59 words
A method of manufacturing yellow incandescent bug lights comprising electrostatically coating th interior surface of incandescent lamps with a cadmiumfree yellow pigment comprising a dry ground homogeneous blend of: a) about 90 percent by weight ZrSiO.sub. 4/Pr yellow pigment, fine-dry ground to an average particle size of about 2.8 microns; and b) about 10 percent by weight amorphous silica.
Claim 5
Dependent Claim
27 words
The method fo claim 1 or 2, which further comprises electrostatically applying at least two layers of the pigment coating to the interior surface of the lamps.
Claim 6
Dependent Claim
23 words
The method of claim 1 or 2, which further comprises electrostatically depositing a final coating of amorphous silica over the two pigment layers.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1994-07-15 | 1995-01-14 | 1995-07-16 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1998-07-15 | 1999-01-14 | 1999-07-16 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2002-07-15 | 2003-01-14 | 2003-07-16 | $7700.00 | Window Closed / Lapsed |