Process for making a thermoplastic resin composition

Assignee: Sumitomo Chemical Co Ltd
•
Filing: 1988-09-13
•
Granted: 1991-05-21
•
Expires: 2008-09-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for making a thermoplastic resin composition which comprises melting and mixing 100 parts by weight of polyphenylene ether (A) and 0.01-5.0 parts by weight of at least one compound (B) which contains in its molecule both (a) carbon-carbon double bond or carbon-carbon triple bond and (b) carboxyl group, acid anhydride group, acid amide group, imide group, carboxylic acid ester group, epoxy group, amino group or hydroxyl group in the presence of 0.01% or more and less than 0.1% by weight of radical initiator based on the polyphenylene ether (A), said polyphenylene ether (A) being obtained by oxidation-polymerization of at least one phenol compound represented by the formula: ##STR1## wherein R 1 , R 2 , R 3 , R 4 and R 5 represent a hydrogen atom, a halogen atom, a hydrocarbon or a substituted hydrocarbon group, with a proviso that at least one of them is a hydrogen atom, and said polyphenylene ether (A) having a reduced viscosity η sp/c of 0.40-0.58 deciliter/gram.

Inventors

  • 👤 Hiroomi Abe
  • 👤 Taichi Nishio
  • 👤 Yasurou Suzuki
  • 👤 Takashi Sanada

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 01:40
CPC Classifications
C; C08; C08G; C08G65/00; C08G65/34; C08G65/48; C08G65/485; C08F; C08F283/00; C08F283/06; C08F283/08; C08L; C08L71/00; C08L71/08; C08L71/10; C08L71/12; C08L71/126; C08L77/00; Y; Y10; Y10S; Y10S525/00; Y10S525/905

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 207 words
A process for making a thermoplastic resin composition which comprises melting and mixing at a temperature of 240°-350° C. 5-95 parts by weight of polyamide and 95-5 parts by weight of a polyphenylene ether composition, said polyphenylene ether composition being obtained by melting and mixing 100 parts by weight of polyphenylene ether (A), 0.01-5.0 parts by weight of at least one compound (B) which contains in its molecule both (a) carbon-carbon double bond or carbon-carbon triple bond and (b) carboxyl group, acid anhydride group, acid made group, imide group, carboxylic acid ester group, epoxy group, amino group or hydroxyl group, and 1-40 parts by weight of rubber-like materials (C) in the presence of 0.01% or more and less than 0.1 % by weight of radical initiator based on the polyphenylene ether (A), said polyphenylene ether (A) being obtained by oxidation-polymerization of at least one phenol compound represented by the formula: ##STR4## wherein R 1 , R 2 , R 3 , R 4 and R 5 represent a hydrogen atom, a halogen atom, a hydrocarbon or a substituted hydrocarbon group, with a proviso that at least one of them is a hydrogen atom, and said polyphenylene ether (a) having a reduced viscosity η sp/c of 0.04-0.58 deciliter/gram.
Claim 2
Dependent Claim 207 words
A process for making a thermoplastic resin composition which comprises melting and mixing at a temperature of 240°-350° C. 5-95 parts by weight of polyamide and 95-5 parts by weight of a polyphenylene ether composition, said polyphenylene ether composition being obtained by melting and mixing 100 parts by weight of polyphenylene ether (A), 0.01-5.0 parts by weight of at least one compound (B) which contains in its molecule both (a) carbon-carbon double bond or carbon-carbon triple bond and (b) carboxyl group, acid anhydride group, acid made group, imide group, carboxylic acid ester group, epoxy group, amino group or hydroxyl group, and 1-40 parts by weight of rubber-like materials (C) in the presence of 0.01% or more and less than 0.1 % by weight of radical initiator based on the polyphenylene ether (A), said polyphenylene ether (A) being obtained by oxidation-polymerization of at least one phenol compound represented by the formula: ##STR4## wherein R 1 , R 2 , R 3 , R 4 and R 5 represent a hydrogen atom, a halogen atom, a hydrocarbon or a substituted hydrocarbon group, with a proviso that at least one of them is a hydrogen atom, and said polyphenylene ether (a) having a reduced viscosity η sp/c of 0.04-0.58 deciliter/gram.
Claim 3
Dependent Claim 36 words
A process according to claim 3 wherein the rubber-like materials are at least one selected from the group consisting of saturated olefin rubber, styrene-grafted copolymer rubber, styrenic block copolymer rubber and hydrogenated styrenic block copolymer rubber.
Claim 4
Dependent Claim 31 words
A process according to claim 1 wherein the saturated olefin rubber is ethylene-propylene copolymer rubber or ethylene-propylene-non-conjugated diene terpolymer rubber with which 0.1-2.0 % by weight of maleic anhydride is graft-polymerized.
Claim 5
Dependent Claim 30 words
A process according to claim 1 wherein compound (B) contains a carbon-carbon double bond and an acid anhydride groups and the rubber-like materials (C) comprise at least one saturated olefin.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-05-20 1994-11-19 1995-05-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-05-20 1998-11-19 1999-05-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-05-20 2002-11-19 2003-05-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag