Claim 1
Independent Claim
178 words
In a process for the preparation of colloidal particles from rare earth salts by homogeneous precipitation techniques involving the forced hydrolysis of a hydrated cation at elevated temperatures, the improvement comprising: (a) providing an aqueous solution, at an initial pH in the range of from about 4.5 to about 6, containing one or more hydrated rare earth cations; (b) heating the aqueous solution containing one or more hydrated rare earth cations to a temperature in the range of from about 70° to about 90° C., so as to effect deprotonation of the hydrated rare earth cations under conditions conducive to control over the kinetics of formation of a precursor of the colloidal particles, and thereby generate in single burst of nuclei preliminary to formation of colloidal particles; (c) aging the solution, in step (b) the extent of such aging being based upon the growth of said nuclei to the desired particle size for the colloidal particles; and (d) separating the colloidal particles from the solution in step (c) upon attainment of the particles of the desired particle size.
Claim 2
Dependent Claim
178 words
In a process for the preparation of colloidal particles from rare earth salts by homogeneous precipitation techniques involving the forced hydrolysis of a hydrated cation at elevated temperatures, the improvement comprising: (a) providing an aqueous solution, at an initial pH in the range of from about 4.5 to about 6, containing one or more hydrated rare earth cations; (b) heating the aqueous solution containing one or more hydrated rare earth cations to a temperature in the range of from about 70° to about 90° C., so as to effect deprotonation of the hydrated rare earth cations under conditions conducive to control over the kinetics of formation of a precursor of the colloidal particles, and thereby generate in single burst of nuclei preliminary to formation of colloidal particles; (c) aging the solution, in step (b) the extent of such aging being based upon the growth of said nuclei to the desired particle size for the colloidal particles; and (d) separating the colloidal particles from the solution in step (c) upon attainment of the particles of the desired particle size.
Claim 3
Dependent Claim
28 words
The process of claim 1, wherein the source of rare earth cation is a salt which is selected from the group consisting of gadolinium, terbium and europium salts.
Claim 4
Dependent Claim
20 words
The process of claim 1, wherein the solution in step (b) contains a base as a source of hydroxide ions.
Claim 5
Dependent Claim
47 words
The process of claim 3, wherein the source of hydroxide ions is an organic base, said organic base thermally decomposing in said aqueous solution, at temperatures in the range of from about 70° to about 90° C., to produce a deprotonation accelerator effective amount of hydroxide ions.
Claim 6
Dependent Claim
33 words
The process of claim 4, wherein the precursor to colloidal particle formation is generated in solution at supersaturation concentrations and under conditions so that only a single burst of particle forming nuclei occurs.
Claim 7
Dependent Claim
50 words
The process of claim 4, wherein the aqueous solution containing one or more hydrated rare earth cations is acidified so as to increase the size of colloidal particle without extended aging, the acid conscentration of said solution being, at all times, maintained below about 1×10 -2 mol dm -3 .
Claim 8
Dependent Claim
34 words
The process of claim 1, wherein the concentration of rare earth salt in solution is in the range from about 1×10 -3 mol dm -3 to about 2×10 31 2 mol dm -3 .
Claim 9
Dependent Claim
27 words
The process of claim 3, wherein the colloidal particles are heated under conditions conducive to decomposition of organic matter, while preserving the colloidal characteristic of said particles.
Claim 10
Dependent Claim
17 words
The process of claim 1, wherein said rare earth salts used are rare earth nitrates and halides.