Abstract
Abstract Steel is nitrided first by treating the steel to be nitrided with NF 3 at elevated temperature to form a fluorinated layer on the steel, and then the steel is nitrided by heating in a nitriding atmosphere.
Inventors
- 👤 Masaaki Tahara
- 👤 Takakazu Tomoda
- 👤 Kenzo Kitano
- 👤 Teruo Minato
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 08:00
CPC Classifications
C; C23; C23C; C23C8/00; C23C8/02; C23C8/06; C23C8/08; C23C8/24; C23C8/26; C23C8/34
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
52 words
A method of nitriding steel which comprises treating the steel with NF 3 gas at a temperature of 150°-350° C. to form a fluorinated layer on the surface of the steel, and then heating the fluorinated steel at 480°-700° C. in a nitriding atmosphere to form a nitrided layer on the steel.
Claim 2
Independent Claim
52 words
A method of nitriding steel which comprises treating the steel with NF 3 gas at a temperature of 150°-350° C. to form a fluorinated layer on the surface of the steel, and then heating the fluorinated steel at 480°-700° C. in a nitriding atmosphere to form a nitrided layer on the steel.
References Cited (Backward Citations)
US152947A
Cited
US1529471A
Cited
US1958575A
Cited
US2851387A
Cited
US3140205A
Cited
JPS5114837A
Cited
SU638635A1
Cited
GB2153855A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1994-05-06 | 1994-11-05 | 1995-05-07 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1998-05-06 | 1998-11-05 | 1999-05-07 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2002-05-06 | 2002-11-05 | 2003-05-07 | $7700.00 | Window Closed / Lapsed |