← Back to Patent Explorer
US4994341A Expired / Lapsed US ⏱️ 0.0 years remaining

Organometallic compounds as mottle prevention additives in liquid electrostatic developers

Assignee: Dx Imaging Inc
•
Filing: 1989-12-20
•
Granted: 1991-02-19
•
Expires: 2009-12-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Electrostatic liquid developer consisting essentially of (A) nonpolar liquid, Kauri-butanol value less than 30, (B) particles of thermoplastic resin having free carboxyl groups (<30μm ave particle size), (C) nonpolar liquid soluble oil-soluble petroleum sulfonate or anionic glyceride charge director, and (D) at least one organometallic compound as defined present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer. The process of preparation of the liquid developer is also disclosed. The developers demonstrate reduced mottle in a fused image. The developers are used in copying, color proofing, preparation of lithographic printing plates and resists.

Inventors

  • 👤 Paul C. Adair
  • 👤 Lalit M. Bhalla
  • 👤 Ronald L. Mueller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 19:10
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/12; G03G9/135; G03G9/1355; Y; Y10; Y10S; Y10S430/00; Y10S430/001; Y10S430/105

Claims Analysis

Total Claims: 51
Claim 1
Independent Claim 205 words
An electrostatic liquid developer consisting essentially of (A) a nonpolar liquid having a Kauri butanol value of less than 30, present in 85 to 99.9% by weight, based on the total weight of liquid developer, (B) particles having an average by area particle size of less than 30 μm of a thermoplastic resin having free carboxyl groups, (C) a nonpolar liquid soluble charge director compound selected from the group consisting of oil-soluble petroleum sulfonate and anionic glycerides present in an amount of 0.25 to 1500 mg/g developer solids, and (D) at least one organometallic compound selected from the group consisting of M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R', and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer, the total weight of developer solids being 0.1 to 15% by weight.
Claim 2
Dependent Claim 205 words
An electrostatic liquid developer consisting essentially of (A) a nonpolar liquid having a Kauri butanol value of less than 30, present in 85 to 99.9% by weight, based on the total weight of liquid developer, (B) particles having an average by area particle size of less than 30 μm of a thermoplastic resin having free carboxyl groups, (C) a nonpolar liquid soluble charge director compound selected from the group consisting of oil-soluble petroleum sulfonate and anionic glycerides present in an amount of 0.25 to 1500 mg/g developer solids, and (D) at least one organometallic compound selected from the group consisting of M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R', and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer, the total weight of developer solids being 0.1 to 15% by weight.
Claim 3
Dependent Claim 65 words
An electrostatic liquid developer according to claim 1 wherein the substituents attached to M +n in the formula for the organometallic compound is selected from the group consisting of propionate, butyrate, hexoate, octoate, nonoate, 2-ethylhexoate, neodecanoate, naphthenate, ethoxide, butyl, and isopropyl, and M is selected from the group consisting of Bi, Ca, Ce, Co, Fe, Mg, Mn, Mo, Ni, Pb, Ti, V, Zn and Zr.
Claim 4
Dependent Claim 85 words
An electrostatic liquid developer according to claim 2 wherein the organometallic compound is selected from the group consisting of zinc naphthenate, zinc 2-ethylhexoate, zinc octoate, zirconium octoate, zirconium 2-ethylhexoate, manganese octoate, manganese naphthenate, manganese 2-ethylhexoate, barium 2-ethylhexoate, cobalt naphthenate, calcium octoate, calcium naphthenate, calcium 2-ethylhexoate, calcium nonoate, nickel octoate, bismuth octoate, bismuth neodecanoate, bismuth 2-ethylhexoate, lead octoate, cobalt octoate, lead naphthenate, cerium naphthenate, cerium 2-ethylhexoate, tetrabutyl titanate, tetra-2-ethylhexyl titanate, titanium tetraethoxide, tetraisopropyl titanate, calcium, cerium, cobalt, lead, manganese, zinc and zirconium neodecanoate, and mixtures thereof.
Claim 5
Dependent Claim 26 words
An electrostatic liquid developer according to claim 1 containing up to about 60% by weight of a colorant based on the total weight of developer solids.
Claim 6
Dependent Claim 14 words
An electrostatic liquid developer according to claim 4 wherein the colorant is a pigment.
Claim 7
Dependent Claim 14 words
An electrostatic liquid developer according to claim 4 wherein the colorant is a dye.
Claim 8
Dependent Claim 17 words
An electrostatic liquid developer according to claim 1 wherein a fine particle size inorganic oxide is present.
Claim 9
Dependent Claim 34 words
An electrostatic liquid developer according to claim 1 wherein an additional compound is present which is an adjuvant selected from the group consisting of polyhydroxy compound, aminoalcohol, polybutylene succinimide, metallic soap, and aromatic hydrocarbon.
Claim 10
Dependent Claim 34 words
An electrostatic liquid developer according to claim 4 wherein an additional compound is present which is an adjuvant selected from the group consisting of polyhydroxy compound, aminoalcohol, polybutylene succinimide, metallic soap, and aromatic hydrocarbon.
Claim 11
Dependent Claim 15 words
An electrostatic liquid developer according to claim 8 wherein a polyhydroxy adjuvant compound is present.
Claim 12
Dependent Claim 15 words
An electrostatic liquid developer according to claim 8 wherein an aminoalcohol adjuvant compound is present.
Claim 13
Dependent Claim 15 words
An electrostatic liquid developer according to claim 11 wherein the aminoalcohol adjuvant compound is triisopropanolamine.
Claim 14
Dependent Claim 16 words
An electrostatic liquid developer according to claim 8 wherein a polybutylene succinimide adjuvant compound is present.
Claim 15
Dependent Claim 16 words
An electrostatic liquid developer according to claim 8 wherein a metallic soap adjuvant compound is present.
Claim 16
Dependent Claim 16 words
An electrostatic liquid developer according to claim 8 wherein an aromatic hydrocarbon adjuvant compound is present.
Claim 17
Dependent Claim 32 words
An electrostatic liquid developer according to claim 1 wherein the thermoplastic resin is a copolymer of ethylene and an unsaturated acid selected from the group consisting of acrylic acid and methacrylic acid.
Claim 18
Dependent Claim 43 words
An electrostatic liquid developer according to claim 1 wherein the thermoplastic resin is a copolymer of ethylene (80 to 99.9%)/acrylic or methacrylic acid (20 to 0.1%)/alkyl ester of acrylic or methacrylic acid wherein alkyl is 1 to 5 carbon atoms (0 to 20%).
Claim 19
Dependent Claim 43 words
An electrostatic liquid developer according to claim 4 wherein the thermoplastic resin is a copolymer of ethylene (80 to 99.9%)/acrylic or methacrylic acid (20 to 0.1%)/alkyl ester of acrylic or methacrylic acid wherein alkyl is 1 to 5 carbon atoms (0 to 20%).
Claim 20
Dependent Claim 29 words
An electrostatic liquid developer according to claim 17 wherein the thermoplastic resin is a copolymer of ethylene (90%)/methacrylic acid (10%) having a melt index at 190° C. of 500.
Claim 21
Dependent Claim 21 words
An electrostatic liquid developer according to claim 1 wherein the particles have an average particle size of less than 10 μm.
Claim 22
Dependent Claim 16 words
An electrostatic liquid developer according to claim 1 wherein component (C) is an oil-soluble petroleum sulfonate.
Claim 23
Dependent Claim 15 words
An electrostatic liquid developer according to claim 1 wherein component (C) is an anionic glyceride.
Claim 24
Dependent Claim 383 words
A process for preparing electrostatic liquid developer for electrostatic imaging comprising (A) dispersing at an elevated temperature in a vessel a thermoplastic resin having free carboxyl groups, a dispersant nonpolar liquid having a Kauri-butanol value of less than 30, and, optionally a colorant, while maintaining the temperature in the vessel at a temperature sufficient to plasticize and liquify the resin and below that at which the dispersant nonpolar liquid degrades and the resin and/or colorant decomposes, (B) cooling the dispersion, either (1) without stirring to form a gel or solid mass, followed by shredding the gel or solid mass and grinding by means of particulate media with or without the presence of additional liquid; (2) with stirring to form a viscous mixture and grinding by means of particulate media with or without the presence of additional liquid; or (3) while grinding by means of particulate media to prevent the formation of a gel or solid mass with or without the presence of additional liquid; (C) separating the dispersion of toner particles having an average particle size of less than 30 μm from the particulate media, (D) adding to the dispersion a nonpolar liquid soluble ionic or zwitterionic charge director compound selected from the group consisting of oil-soluble petroleum sulfonate and anionic glycerides, and (E) adding subsequent to step (C) at least one organometallic compound, selected from the group consisting of formula: M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R' and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal wherein the nonpolar liquid is present in 85 to 99.9% by weight, based on the total weight of liquid developer, the total weight of developer solids is 0.1 to 15.0% by weight, and the ionic or zwitterionic charge director compound is present in an amount of 0.25 to 1500 mg/g developer solids, and the at least one organometallic compound is present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer.
Claim 25
Dependent Claim 383 words
A process for preparing electrostatic liquid developer for electrostatic imaging comprising (A) dispersing at an elevated temperature in a vessel a thermoplastic resin having free carboxyl groups, a dispersant nonpolar liquid having a Kauri-butanol value of less than 30, and, optionally a colorant, while maintaining the temperature in the vessel at a temperature sufficient to plasticize and liquify the resin and below that at which the dispersant nonpolar liquid degrades and the resin and/or colorant decomposes, (B) cooling the dispersion, either (1) without stirring to form a gel or solid mass, followed by shredding the gel or solid mass and grinding by means of particulate media with or without the presence of additional liquid; (2) with stirring to form a viscous mixture and grinding by means of particulate media with or without the presence of additional liquid; or (3) while grinding by means of particulate media to prevent the formation of a gel or solid mass with or without the presence of additional liquid; (C) separating the dispersion of toner particles having an average particle size of less than 30 μm from the particulate media, (D) adding to the dispersion a nonpolar liquid soluble ionic or zwitterionic charge director compound selected from the group consisting of oil-soluble petroleum sulfonate and anionic glycerides, and (E) adding subsequent to step (C) at least one organometallic compound, selected from the group consisting of formula: M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R' and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal wherein the nonpolar liquid is present in 85 to 99.9% by weight, based on the total weight of liquid developer, the total weight of developer solids is 0.1 to 15.0% by weight, and the ionic or zwitterionic charge director compound is present in an amount of 0.25 to 1500 mg/g developer solids, and the at least one organometallic compound is present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer.
Claim 26
Dependent Claim 64 words
A process according to to claim 23 wherein the substituents attached to M +n in the formula for the organometallic compound is selected from the group consisting of propionate, butyrate, hexoate, octoate, nonoate, 2-ethylhexoate, neodecanoate, naphthenate, ethoxide, butyl, and isopropyl, and M is selected from the group consisting of Bi, Ca, Ce, Co, Fe, Mg, Mn, Mo, Ni, Pb, Ti, V, Zn and Zr.
Claim 27
Dependent Claim 83 words
A process according to claim 24 wherein the organometallic compound is selected from the group consisting of zinc naphthenate, zinc 2-ethylhexoate, zinc octoate, zirconium octoate, zirconium 2-ethylhexoate, manganese octoate, manganese naphthenate, manganese 2-ethylhexoate, barium 2-ethylhexoate, cobalt naphthenate, calcium octoate, calcium naphthenate, calcium 2-ethylhexoate, calcium nonoate, nickel octoate, bismuth octoate, bismuth neodecanoate, bismuth 2-ethylhexoate, lead octoate, cobalt octoate, lead naphthenate, cerium naphthenate, cerium 2-ethylhexoate, tetrabutyl titanate, tetra-2-ethylhexyl titanate, titanium tetraethoxide, tetraisopropyl titanate, calcium, cerium, cobalt, lead, manganese, zinc and zirconium neodecanoate, and mixtures thereof.
Claim 28
Dependent Claim 40 words
A process according to claim 23 wherein there is present in the vessel up to 100% by weight of a polar additive having a Kauri-butanol value of at least 30, the percentage based on the total weight of the liquid.
Claim 29
Dependent Claim 27 words
A process according to claim 23 wherein the particulate media are selected from the group consisting of stainless steel, carbon steel, ceramic, alumina, zirconia, silica and sillimanite.
Claim 30
Dependent Claim 30 words
A process according to claim 23 wherein the thermoplastic resin is a copolymer of ethylene and an unsaturated acid selected from the group consisting of acrylic acid and methacrylic acid.
Claim 31
Dependent Claim 41 words
A process according to claim 23 wherein the thermoplastic resin is a copolymer of ethylene (80 to 99.9%)/acrylic or methacrylic acid (20 to 0.1%)/alkyl ester of acrylic or methacrylic acid wherein alkyl is 1 to 5 carbon atoms (0 to 20%).
Claim 32
Dependent Claim 28 words
A process according to claim 29 wherein the thermoplastic resin is a copolymer of ethylene (90%) methacrylic acid (10%) having a melt index at 190° C. of 500.
Claim 33
Dependent Claim 16 words
A process according to claim 23 wherein the charge director compound is an oil-soluble petroleum sulfonate.
Claim 34
Dependent Claim 14 words
A process according to claim 23 wherein the charge director is an anionic glyceride.
Claim 35
Dependent Claim 38 words
A process according to claim 23 wherein the additional nonpolar liquid, polar liquid, or combinations thereof is present to reduce the concentration of toner particles to between 0.1 to 15 percent by weight with respect to the liquid.
Claim 36
Dependent Claim 18 words
A process according to claim 33 wherein the concentration of toner particles is reduced by additional nonpolar liquid.
Claim 37
Dependent Claim 37 words
A process according to claim 23 wherein cooling the dispersion is accomplished while grinding by means of particulate media to prevent the formation of a gel or solid mass with or without the presence of additional liquid.
Claim 38
Dependent Claim 44 words
A process according to claim 23 wherein cooling the dispersion is accomplished without stirring to form a gel or solid mass, followed by shredding the gel or solid mass and grinding by means of particulate media with or without the presence of additional liquid.
Claim 39
Dependent Claim 34 words
A process according to claim 23 wherein cooling the dispersion is accomplished with stirring to form a viscous mixture and grinding by means of particulate media with or without the presence of additional liquid.
Claim 40
Dependent Claim 33 words
A process according to claim 23 wherein an adjuvant compound selected from the group consisting of polyhydroxy compound, aminoalcohol, polybutylene succinimide, metallic soap, and aromatic hydrocarbon is added during the dispersing step (A).
Claim 41
Dependent Claim 13 words
A process according to claim 38 wherein the adjuvant compound is an aminoalcohol.
Claim 42
Dependent Claim 11 words
A process according to claim 39 wherein the aminoalcohol is triisopropanolamine.
Claim 43
Dependent Claim 33 words
A process according to claim 33 wherein an adjuvant compound selected from the group consisting of polyhydroxy compound, aminoalcohol, polybutylene succinimide, metallic soap, and an aromatic hydrocarbon is added to the liquid developer.
Claim 44
Dependent Claim 14 words
A process according to claim 41 wherein the adjuvant compound is a polyhydroxy compound.
Claim 45
Dependent Claim 13 words
A process according to claim 42 wherein the polyhydroxy compound is ethylene glycol.
Claim 46
Dependent Claim 19 words
A process according to claim 41 wherein the adjuvant compound is a metallic soap dispersed in the thermoplastic resin.
Claim 47
Dependent Claim 14 words
A process according to claim 44 wherein the adjuvant compound is an aluminium stearate.
Claim 48
Dependent Claim 339 words
A process for preparing electrostatic liquid developer comprising (A) dispersing a colorant in a thermoplastic resin in the absence of a dispersant nonpolar liquid having a Kauri-butanol value of less than 30 to form a solid mass, (B) shredding the solid mass, (C) grinding the shredded solid mass by means of particulate media in the presence of a liquid selected from the group consisting of a polar liquid having a Kauri-butanol value of at least 30, a nonpolar liquid having a Kauri-butanol value of less than 30, and combinations thereof, (D) separating the dispersion of toner particles having an average particle size of less than 30 μm from the particulate media, and (E) adding additional nonpolar liquid, polar liquid or combinations thereof to reduce the concentration of toner particles to between 0.1 to 15.0 percent by weight with respect to the liquid, (F) adding to the dispersion a liquid soluble ionic or zwitterionic charge director compound selected from the group consisting of oil-soluble petroleum sulfonate and anionic glycerides, and (G) adding subsequent to step (D) at least one organometallic compound selected from the group consisting of formula: M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R' and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal wherein the nonpolar liquid is present in 85 to 99.9% by weight, based on the total weight of liquid developer, the total weight of developer solids is 0.1 to 15.0% by weight, and the ionic or zwitterionic charge director compound is present in an amount of 0.25 to 1500 mg/g developer solids, and the at least one organometallic compound is present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer.
Claim 49
Dependent Claim 339 words
A process for preparing electrostatic liquid developer comprising (A) dispersing a colorant in a thermoplastic resin in the absence of a dispersant nonpolar liquid having a Kauri-butanol value of less than 30 to form a solid mass, (B) shredding the solid mass, (C) grinding the shredded solid mass by means of particulate media in the presence of a liquid selected from the group consisting of a polar liquid having a Kauri-butanol value of at least 30, a nonpolar liquid having a Kauri-butanol value of less than 30, and combinations thereof, (D) separating the dispersion of toner particles having an average particle size of less than 30 μm from the particulate media, and (E) adding additional nonpolar liquid, polar liquid or combinations thereof to reduce the concentration of toner particles to between 0.1 to 15.0 percent by weight with respect to the liquid, (F) adding to the dispersion a liquid soluble ionic or zwitterionic charge director compound selected from the group consisting of oil-soluble petroleum sulfonate and anionic glycerides, and (G) adding subsequent to step (D) at least one organometallic compound selected from the group consisting of formula: M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R' and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal wherein the nonpolar liquid is present in 85 to 99.9% by weight, based on the total weight of liquid developer, the total weight of developer solids is 0.1 to 15.0% by weight, and the ionic or zwitterionic charge director compound is present in an amount of 0.25 to 1500 mg/g developer solids, and the at least one organometallic compound is present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer.
Claim 50
Dependent Claim 433 words
A process for preparing electrostatic liquid developer comprising (A) dispersing a colorant in a thermoplastic resin in the absence of a dispersant nonpolar liquid having a Kauri-butanol value of less than 30 to form a solid mass (B) shredding the solid mass, (C) redispersing the shredded solid mass at an elevated temperature in a vessel in the presence of a dispersant nonpolar liquid having a Kauri-butanol value of less than 30, and optionally a colorant, while maintaining the temperature in the vessel at a temperature sufficient to plasticize and liquify the resin and below that at which the dispersant nonpolar liquid degrades and the resin and/or colorant decomposes, (D) cooling the dispersion, either (1) without stirring to form a gel or solid mass, followed by shredding the gel or solid mass and grinding by means of particulate media with or without the presence of additional liquid; (2) with stirring to form a viscous mixture and grinding by means of particulate media with or without the presence of additional liquid; or (3) while grinding by means of particulate media to prevent the formation of a gel or solid mass with or without the presence of additional liquid; (E) separating the dispersion of toner particles having an average particle size of less than 30 μm from the particulate media, and (F) adding additional nonpolar liquid, polar liquid or combinations thereof to reduce the concentration of toner particles to between 0.1 to 15.0 percent by weight with respect to the liquid, (G) adding to the dispersion a liquid soluble ionic or zwitterionic charge director compound, and (H) adding subsequent to step (E) at least one organometallic compound selected from the group consisting of formula: M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R' and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal wherein the nonpolar liquid is present in 85 to 99.9% by weight, based on the total weight of liquid developer, the total weight of developer solids is 0.1 to 15.0% by weight, and the ionic or zwitterionic charge director compound is present in an amount of 0.25 to 1500 mg/g developer solids, and the at least one organometallic compound is present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer.
Claim 51
Dependent Claim 433 words
A process for preparing electrostatic liquid developer comprising (A) dispersing a colorant in a thermoplastic resin in the absence of a dispersant nonpolar liquid having a Kauri-butanol value of less than 30 to form a solid mass (B) shredding the solid mass, (C) redispersing the shredded solid mass at an elevated temperature in a vessel in the presence of a dispersant nonpolar liquid having a Kauri-butanol value of less than 30, and optionally a colorant, while maintaining the temperature in the vessel at a temperature sufficient to plasticize and liquify the resin and below that at which the dispersant nonpolar liquid degrades and the resin and/or colorant decomposes, (D) cooling the dispersion, either (1) without stirring to form a gel or solid mass, followed by shredding the gel or solid mass and grinding by means of particulate media with or without the presence of additional liquid; (2) with stirring to form a viscous mixture and grinding by means of particulate media with or without the presence of additional liquid; or (3) while grinding by means of particulate media to prevent the formation of a gel or solid mass with or without the presence of additional liquid; (E) separating the dispersion of toner particles having an average particle size of less than 30 μm from the particulate media, and (F) adding additional nonpolar liquid, polar liquid or combinations thereof to reduce the concentration of toner particles to between 0.1 to 15.0 percent by weight with respect to the liquid, (G) adding to the dispersion a liquid soluble ionic or zwitterionic charge director compound, and (H) adding subsequent to step (E) at least one organometallic compound selected from the group consisting of formula: M.sup.+n (R.sup.-).sub.n, M.sup.+n (CO.sub.2 R'.sup.-).sub.n and M.sup.+n (OR".sup.-).sub.n where R, R' and R", which can be the same or different, are moieties of a linear hydrocarbon of 1 to 30 carbon atoms, a branched chain hydrocarbon of 1 to 30 carbon atoms, or a linear or branched chain, substituted hydrocarbon of 1 to 30 carbon atoms, M is a metal, and n is at least 2 and is equal to the valency of the metal wherein the nonpolar liquid is present in 85 to 99.9% by weight, based on the total weight of liquid developer, the total weight of developer solids is 0.1 to 15.0% by weight, and the ionic or zwitterionic charge director compound is present in an amount of 0.25 to 1500 mg/g developer solids, and the at least one organometallic compound is present in 0.01 to 0.15 part by weight metal based on the total weight of liquid developer.

References Cited (Backward Citations)

JPS51107833A Cited
JPS5357039A Cited
JPS6013171A Cited
US4663264A Cited
US4707429A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-02-18 1994-08-20 1995-02-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-02-18 1998-08-20 1999-02-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-02-18 2002-08-20 2003-02-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag