Abstract

Abstract The method includes the steps of coating the peripheral surface of a roll with a film of plasticizer. An offset roll disposed adjacent to the roll is rotated such that the roll and the offset roll define therebetween a transfer nip so that a film of the plasticizer is transferred to the offset roll. The web is moved past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web. The web is then passed with the offset coating of plasticizer through a calendering nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.

Inventors

  • 👤 Samuel F. Keller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 05:53
CPC Classifications
D; D21; D21H; D21H25/00; D21H25/08; D21H25/12; D21H25/14; D21H23/00; D21H23/02; D21H23/22; D21H23/52; D21H23/56

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 164 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of: coating the peripheral surface of a roll with a film of plasticizer; rotating an offset roll disposed adjacent to the roll such that the roll and the offset roll define therebetween a transfer nip so that the film of the plasticizer is transferred to the offset roll; moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 2
Independent Claim 164 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of: coating the peripheral surface of a roll with a film of plasticizer; rotating an offset roll disposed adjacent to the roll such that the roll and the offset roll define therebetween a transfer nip so that the film of the plasticizer is transferred to the offset roll; moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 3
Dependent Claim 67 words
A method as set forth in claim 1 wherein the step of rotating the roll within the receptacle further includes the steps of: partially immersing the roll within a receptacle containing the plasticizer; doctoring the film of plasticizer upstream relative to the transfer nip such that a uniform film of the plasticizer remains on the peripheral surface of the roll between the doctor and the transfer nip.
Claim 4
Dependent Claim 25 words
A method as set forth in claim 1 wherein the step of rotating the roll includes rotating the roll within the plasticizer, which is water.
Claim 5
Dependent Claim 34 words
A method as set forth in claim 1 wherein the step of rotating an offset roll further includes: rotating the offset roll in a direction opposite to the direction of rotation of the roll.
Claim 6
Dependent Claim 64 words
A method as set forth in claim 1 wherein the step of moving the web further includes the step of: rotating a further roll disposed adjacent to the offset roll such that the web is disposed between the offset roll and the further roll, the offset roll and the further roll defining therebetween a guide nip for guiding the web towards the calendering nip.
Claim 7
Dependent Claim 49 words
A method as set forth in claim 5 wherein the further roll is a calender roll such that the web is guided between the offset roll and the calender roll, the web being subsequently supported and guided by the calender roll until the web passe through the calendering nip.
Claim 8
Dependent Claim 58 words
A method as set forth in claim 6 wherein the step of moving the web past the offset roll further includes the step of: rotating the offset roll in an opposite direction to the direction of rotation of the calender roll such that the guide nip becomes filled with a coating meniscus upstream relative to the guide nip.
Claim 9
Dependent Claim 74 words
A method as set forth in claim 5 wherein the further roll is a further offset roll, the further step of rotating the further roll including the sub-step of: rotating a plasticizer roll disposed adjacent to the further roll and rotating within a further receptacle filled with plasticizer such that the plasticizer is transferred from the plasticizer roll to the further offset roll so that plasticizer is applied to opposite surfaces of the web.
Claim 10
Dependent Claim 95 words
A method as set forth in claim 1 wherein the step of passing the web with the offset coating includes the further step of: permitting the plasticizer to coat the surface of the web, which is rough, so that fibers within the web close to the surface of the web being coated are plasticized such that during the passage through the calendering nip, such plasticized fibers are easily compressed to impart smoothness to the web while most of the fibers further away from the surface are not plasticized and consequently remain relatively dry and uncompressible.
Claim 11
Independent Claim 140 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of: coating a roll with a plasticizer from a fountain; doctoring the coated roll; transferring the doctored coating of plasticizer to an offset roll; moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 12
Independent Claim 140 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of: coating a roll with a plasticizer from a fountain; doctoring the coated roll; transferring the doctored coating of plasticizer to an offset roll; moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 13
Independent Claim 180 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of coating the peripheral surface of a roll with a film of plasticizer; the coating step further including: spraying the peripheral surface with a fountain of the plasticizer; rotating an offset roll disposed adjacent to the roll such that the roll and the offset roll define therebetween a transfer nip so that the film of the plasticizer is transferred to the offset roll moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional of compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 14
Independent Claim 180 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of coating the peripheral surface of a roll with a film of plasticizer; the coating step further including: spraying the peripheral surface with a fountain of the plasticizer; rotating an offset roll disposed adjacent to the roll such that the roll and the offset roll define therebetween a transfer nip so that the film of the plasticizer is transferred to the offset roll moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that the film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional of compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 15
Independent Claim 185 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of: coating the peripheral surface of a roll with a film of plasticizer; the coating step further including: coating the peripheral surface by means of a short dwell coater and then doctoring the applied coating; rotating an offset roll disposed adjacent to the roll such that the roll and the offset roll define therebetween a transfer nip so that the roll of the plasticizer is transferred to the offset roll; moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.
Claim 16
Independent Claim 185 words
A method of manufacturing a Z-directional compressibility gradient in a web of paper, said method comprising the steps of: coating the peripheral surface of a roll with a film of plasticizer; the coating step further including: coating the peripheral surface by means of a short dwell coater and then doctoring the applied coating; rotating an offset roll disposed adjacent to the roll such that the roll and the offset roll define therebetween a transfer nip so that the roll of the plasticizer is transferred to the offset roll; moving the web past the offset roll such that the web contacts the offset roll downstream relative to the transfer nip so that film of the plasticizer is offset onto the web; and passing the web with the offset coating of plasticizer through a calender nip such that between the offset coating of the web and the subsequent calendering of the web with the offset coating, the plasticizer is permitted to uniformly and controllably penetrate into the web such that the Z-directional compressibility of the web is controlled prior to the web extending through the calendering nip.

References Cited (Backward Citations)

FR737060A Cited
US3120449A Cited
US3261899A Cited
DE2343930A1 Cited
JPS5427033A Cited
US4378639A Cited
US4596632A Cited
US4534829A Cited
US4836894A Cited
EP0174661A2 Cited
US4670102A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-11-26 1994-05-28 1994-11-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-11-26 1998-05-28 1998-11-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-11-26 2002-05-28 2002-11-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag