Abstract

Abstract The invention relates to an aqueous coating composition containing an N-alkyl lactam dispersing aid and a water soluble metal salt having an atomic number greater than 50 dispersed in between about 4 and about 50 wt. % of an aqueous binder solution compatible with a binder employed for crystalline polyacetylenic crystals used in an imaging process.

Inventors

  • 👤 David F. Lewis
  • 👤 Robert D. Schenfele

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 16:32
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/02; C08J3/03; C09; C09D; C09D5/00; G; G03; G03F; G03F7/00; G03F7/004; G03F7/025; C08J2349/00

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 89 words
A dispersion composition comprising between about 0.001% and about 1.0% by weight of an N-C 10-22 alkyl lactam dispersing aid, a metal nitrate, acetate or persulfate salt of a metal having an atomic number of at least 50 or a mixture of said lactams or metal salts dispersed in between about 4% and about 50% by weight of an aqueous solution of a binder compatible with the binder of imageable polyacetylene crystals; said composition having a weight ratio of metal salt to binder between about 0.4:1 and about 2.5:1.
Claim 2
Dependent Claim 89 words
A dispersion composition comprising between about 0.001% and about 1.0% by weight of an N-C 10-22 alkyl lactam dispersing aid, a metal nitrate, acetate or persulfate salt of a metal having an atomic number of at least 50 or a mixture of said lactams or metal salts dispersed in between about 4% and about 50% by weight of an aqueous solution of a binder compatible with the binder of imageable polyacetylene crystals; said composition having a weight ratio of metal salt to binder between about 0.4:1 and about 2.5:1.
Claim 3
Dependent Claim 22 words
The composition of claim 1 wherein said salt is a salt of a metal having an atomic number of at least 78.
Claim 4
Dependent Claim 13 words
The composition of claim 2 wherein said metal salt is a lead salt.
Claim 5
Dependent Claim 23 words
The composition of claim 1 wherein said N-alkyl lactam is N-alkyl pyrrolidone and said alkyl group contains from 10 to 14 carbon atoms.
Claim 6
Dependent Claim 11 words
The composition of claim 4 wherein said N-alkyl lactam is N-dodecyl-2-pyrrolidone.
Claim 7
Dependent Claim 12 words
The composition of claim 4 wherein said metal salt contains lead nitrate.
Claim 8
Dependent Claim 23 words
The composition of claim 1 wherein said binder is an aqueous solution containing between about 1% and about 30% by weight of binder.
Claim 9
Dependent Claim 10 words
The composition of claim 7 wherein said binder is gelatin.
Claim 10
Dependent Claim 56 words
The composition of claim 1 containing from about 0.5% to about 1% by weight of said N-alkyl lactam, from about 1% to about 75% by weight metal salt and from about 4% to about 15% by weight of binder and wherein the total solids of said composition is between about 1% and about 60% by weight.
Claim 11
Dependent Claim 52 words
The composition of claim 9 wherein the weight ratio of metal salt to binder is between about 0.8:1 and about 1.5:1, the weight ratio of lactam to metal salt is between about 1:200 and about 1:10 and the total solids of the composition is between about 5% and about 30% by weight.
Claim 12
Dependent Claim 21 words
The composition of claim 10 wherein the weight ratio of lactam to metal salt is between about 1:60 and about 1:10.
Claim 13
Dependent Claim 56 words
The composition of claim 1 containing from about 0.5% to about 1% by weight N-dodecyl pyrrolidone, from about 20% to about 55% by weight of lead nitrate and from about 4% to about 15% by weight gelatin in aqueous solution, said composition having a total solids concentration of between about 5% and about 30% by weight.

References Cited (Backward Citations)

US3966655A Cited
US4439579A Cited
US4567228A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-09-03 1994-03-05 1994-09-04 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-09-03 1998-03-05 1998-09-04 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-09-03 2002-03-05 2002-09-04 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag