Abstract

Abstract A method of correcting a circuit pattern such as an X-ray mask, carried out by first preparing a circuit pattern structure where a circuit pattern on a conductive film is coated with a protective film, then forming a hole or a slit by irradiating a high-intensity focused ion beam to a dropout defective portion in the circuit pattern of the circuit pattern structure, and plating such hole or slit while utilizing the conductive film as a plating electrode, thereby forming a metal frame to correct the dropout defective portion.

Inventors

  • 👤 Hiroshi Yamaguchi
  • 👤 Keiya Saito
  • 👤 Akira Shimase
  • 👤 Satoshi Haraichi
  • 👤 Susumu Aiuchi
  • 👤 Nobuyuki Akiyama
  • 👤 Shinji Kuniyoshi
  • 👤 Takeshi Kimura

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 10:06
CPC Classifications
G; G03; G03F; G03F1/00; G03F1/68; G03F1/72; G03F1/74; G03F1/22

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 185 words
A circuit pattern correcting method comprising the steps of: preparing a circuit pattern structure where a circuit pattern on a conductive film is coated with a protective film; removing a wide area of the protective film of the circuit pattern structure so as to reduce a thickness of the protective film by irradiating with a scan of a high-intensity focused ion beam; visually detecting a dropout portion of said circuit pattern by displaying an image of the circuit pattern for a wide area of the circuit pattern that was scanned in said step of removing a wide area of the protective film and by detecting a current flowing in said conductive film in accordance with the scanning of said ion beam, on a displaying means; forming a hole or a slit in the protective film of reduced thickness by irradiating by scanning with the high-intensity focused ion beam aligned to the dropout defective portion detected by the display means; and plating said hole or slit while utilizing said conductive film as a plating electrode, thereby forming a metal film to correct said dropout defective portion.
Claim 2
Dependent Claim 185 words
A circuit pattern correcting method comprising the steps of: preparing a circuit pattern structure where a circuit pattern on a conductive film is coated with a protective film; removing a wide area of the protective film of the circuit pattern structure so as to reduce a thickness of the protective film by irradiating with a scan of a high-intensity focused ion beam; visually detecting a dropout portion of said circuit pattern by displaying an image of the circuit pattern for a wide area of the circuit pattern that was scanned in said step of removing a wide area of the protective film and by detecting a current flowing in said conductive film in accordance with the scanning of said ion beam, on a displaying means; forming a hole or a slit in the protective film of reduced thickness by irradiating by scanning with the high-intensity focused ion beam aligned to the dropout defective portion detected by the display means; and plating said hole or slit while utilizing said conductive film as a plating electrode, thereby forming a metal film to correct said dropout defective portion.
Claim 3
Dependent Claim 26 words
A method according to claim 1, wherein said hole or slit is formed by detecting a time variation of the current flowing in said conductive film.
Claim 4
Dependent Claim 37 words
A method according to claim 1, wherein said dropout defective portion is detected by displaying the image of the circuit pattern obtained by detecting secondary charged particles emitted from said wire area of the exposed circuit pattern.
Claim 5
Dependent Claim 45 words
A method according to claim 2, wherein said conductive film is composed of a metal film containing nickel or the like which is not processed readily by said high-intensity focused ion beam, whereby said hole or slit can be formed accurately to said conductive film.
Claim 6
Dependent Claim 16 words
A method according to claim 2, wherein said circuit pattern structure is an X-ray exposure mask.
Claim 7
Dependent Claim 39 words
A method according to claim 2, wherein, when said dropout defect is extremely small, said hole or slit is formed in a wider region inclusive of said circuit pattern, and said region is plated to correct the defective portion.

References Cited (Backward Citations)

US4256778A Cited
US4328298A Cited
JPS5852821A Cited
US4503329A Cited
JPS58111317A Cited
JPS60234320A Cited
US4751169A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-05-14 1993-11-13 1994-05-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-05-14 1997-11-13 1998-05-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-05-14 2001-11-13 2002-05-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag