Abstract

Abstract A polymer laminate produced by crosshead extrusion suitable for wear resistant applications such as a vehicle glass run channel comprises a layer of a weather resistant rubber such as an ethylene-propylenediene (EPDM) rubber and a layer of a wear resistant thermoplastic such as polypropylene. The laminate is passed through an oven at an elevated temperature sufficient to cure the EPDM rubber, for example, at about 375° F., with ambient temperature cooling fluid being blown over the exposed surface of the polypropylene thermoplastic. The interior polypropylene surface or interface is heated by the EPDM rubber which is at a high temperature as a result of the heat of extrusion and heat generated by cure thereof. As a result, the polypropylene interior surface or interface melts and causes it to flow and form a mechanical bond with the EPDM rubber while the exposed surface as well as a substantial portion of the polypropylene is kept from melting by the cooling fluid. The EPDM rubber can be extruded in the form of a channel having a longitudinal web which supports and is bonded to the laminated polypropylene wear strip to form a glass run channel.

Inventors

  • 👤 Mark L. Brooks
  • 👤 Keith E. Wilson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 02:56
CPC Classifications
B; B32; B32B; B32B25/00; B32B25/04; B32B25/08; B60; B60J; B60J10/00; B60J10/15; B60J10/17; B60J10/70; B60J10/74; B60J10/79; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/2419; Y10T428/24198; Y10T428/31504; Y10T428/31855; Y10T428/31931

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 74 words
A glass run strip having a base comprising a cured weather resistant rubber housing, said housing having a base, said base having a longitudinal central web adjoined by two opposing sides to form a channel, each said side having a longitudinal flexible lip, each said lip extending towards each other and forming a channel enclosure, and a thermoplastic wear strip, said thermoplastic wear strip being laminated to said longitudinal central web by melt bonding.
Claim 2
Dependent Claim 74 words
A glass run strip having a base comprising a cured weather resistant rubber housing, said housing having a base, said base having a longitudinal central web adjoined by two opposing sides to form a channel, each said side having a longitudinal flexible lip, each said lip extending towards each other and forming a channel enclosure, and a thermoplastic wear strip, said thermoplastic wear strip being laminated to said longitudinal central web by melt bonding.
Claim 3
Dependent Claim 48 words
A glass run strip according to claim 1, wherein said cured weather resistant rubber housing is a styrene-butadiene rubber, a polychloroprene rubber, a nitrile-polyvinyl chloride rubber blend, an EPDM rubber, or combinations thereof, and wherein said thermoplastic wear strip has a melting point of 350° F. or less.
Claim 4
Dependent Claim 28 words
A glass run strip according to claim 2, wherein said thermoplastic is polyethylene or polypropylene having a density of from about 0.9 to about 1.2 grams per cc.
Claim 5
Dependent Claim 98 words
A glass run strip according to claim 3, wherein said cured weather resistant rubber is said EPDM rubber, wherein said EPDM rubber contains from about 45 percent to about 75 percent by weight of ethylene units therein based upon the total weight of said ethylene and propylene units, wherein said EPDM rubber housing contained from about 4 percent to about 15 percent by weight of non-conjugated diene units based upon the total weight of said EPDM rubber, wherein said non-conjugated diene unit contains from about 5 to about 10 carbon atoms, and wherein said thermoplastic in said polypropylene.
Claim 6
Dependent Claim 69 words
A glass run strip according to claim 4, wherein the amount of said non-conjugated diene unit is from about 6 percent to about 12 percent by weight based upon the total weight of said EPDM rubber, wherein said polypropylene has a melting point of from about 300° F. to about 330° F., and wherein said polypropylene has a density of from about 0.9 to about 1.1 grams per cc.
Claim 7
Dependent Claim 21 words
A glass run strip according to claim 1, wherein said thermoplastic wear strip is mechanically bonded to said cured rubber housing.
Claim 8
Dependent Claim 21 words
A glass run strip according to claim 3, wherein said thermoplastic wear strip is mechanically bonded to said cured rubber housing.
Claim 9
Dependent Claim 20 words
A glass run strip according to claim 5, wherein said thermoplastic strip is mechanically bonded to said cured rubber housing.

References Cited (Backward Citations)

US3659983A Cited
US3624964A Cited
US4296062A Cited
US3918206A Cited
US4104098A Cited
US4538380A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-05-07 1993-11-06 1994-05-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-05-07 1997-11-06 1998-05-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-05-07 2001-11-06 2002-05-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag