Abstract

Abstract The present invention provides a manufacturing method of a conductive or superconductive thin film of mixed oxide as an easier way to apply the mixed oxide type superconductive materials to electronic devices, etc. The manufacturing method of the present invention comprises using a mixed oxide composition showing conductivity or superconductivity as a target material and sputtering it onto a substrate to form a thin film. Examples of the mixed oxide compositions showing conductivity or superconductivity and to be used as the target material in the present invention are mixed oxides consisting of lanthanoid, alkali earth metal and copper as main components, particularly, a mixed oxide consisting essentially of La-Sr-Cu-O, La-Ba-Cu-O, La-Ca-Cu-O etc. or mixtures thereof, materials containing a small quantity of other metal oxide(s), or mixed oxides mainly consisting of Yb-Ba-Cu-O, Er-Ba-Cu-O, Ho-Ba-Cu-O, Tm-Ba-Cu-O or mixtures thereof.

Inventors

  • 👤 Hideomi Koinuma
  • 👤 Kazuo Fueki
  • 👤 Masashi Kawasaki
  • 👤 Shunroh Nagata

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 17:45
CPC Classifications
H; H10; H10N; H10N60/00; H10N60/01; H10N60/0268; H10N60/0296; H10N60/0408; H10N60/0884; Y; Y10; Y10S; Y10S505/00; Y10S505/725; Y10S505/73; Y10S505/731; Y10S505/80; Y10S505/815; Y10S505/816

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 52 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity as a target material and sputtering it on a substrate to form a thin film, then irradiating the thin film with ultraviolet light or vacuum ultraviolet light in an oxygen atmosphere.
Claim 2
Dependent Claim 52 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity as a target material and sputtering it on a substrate to form a thin film, then irradiating the thin film with ultraviolet light or vacuum ultraviolet light in an oxygen atmosphere.
Claim 3
Dependent Claim 23 words
A manufacturing method of the conductive or superconductive thin film as claimed in claim 4, wherein the thin film is heat-treated after forming.
Claim 4
Dependent Claim 56 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity as a target material and sputtering it on a substrate to form a thin film, wherein the sputtering of the target material is carried out under the radiation of ultraviolet light or vacuum ultraviolet light.
Claim 5
Dependent Claim 56 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity as a target material and sputtering it on a substrate to form a thin film, wherein the sputtering of the target material is carried out under the radiation of ultraviolet light or vacuum ultraviolet light.
Claim 6
Dependent Claim 61 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity comprising lanthanoid, alkali-earth metal, and copper as main components, as a target material and sputtering it onto a substrate to form a thin film, then irradiating the thin film with ultraviolet light or vacuum ultraviolet light in an oxygen atmosphere.
Claim 7
Dependent Claim 61 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity comprising lanthanoid, alkali-earth metal, and copper as main components, as a target material and sputtering it onto a substrate to form a thin film, then irradiating the thin film with ultraviolet light or vacuum ultraviolet light in an oxygen atmosphere.
Claim 8
Dependent Claim 65 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity comprising lanthanoid, alkali-earth metal, and copper as main components, as a target material and sputtering it onto a substrate to form a thin film, wherein the sputtering of the target material is carried out under the radiation of ultraviolet light or vacuum ultraviolet light.
Claim 9
Dependent Claim 65 words
A manufacturing method of a conductive or superconductive thin film which comprises using a mixed oxide composition showing conductivity or superconductivity comprising lanthanoid, alkali-earth metal, and copper as main components, as a target material and sputtering it onto a substrate to form a thin film, wherein the sputtering of the target material is carried out under the radiation of ultraviolet light or vacuum ultraviolet light.

References Cited (Backward Citations)

US4316785A Cited
JPH0696599A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-02-19 1993-08-21 1994-02-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-02-19 1997-08-21 1998-02-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-02-19 2001-08-21 2002-02-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag