Abstract
Abstract A method of coating the cured product of an oxyalkylene polymer having reactive silicon groups with an alkyd paint. The oxyalkylene polymer is combined with a high-molecular weight plasticizer and the composition is cured and the cured product coated with an alkyd paint.
Inventors
- 👤 Sadao Yukimoto
- 👤 Toshifumi Hirose
- 👤 Katsuhiko Isayama
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 12:21
CPC Classifications
C; C08; C08G; C08G65/00; C08G65/02; C08G65/32; C08G65/329; C08G65/336; C08J; C08J7/00; C08J7/04; C08J7/0427; C08J7/043; C08J7/046; C08L; C08L71/00; C08L71/02; C08J2371/00; C08J2371/02; C08J2467/00; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31652; Y10T428/31663; Y10T428/31786
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
92 words
A method of coating the cured product of an oxyalkylene polymer with an alkyd paint comprising (a) combining an oxyalkylene polymer having at least one silicon-containing group that has a hydroxyl group or a hydrolyzable group bonded to a silicon atom and is capable of crosslinking by forming a siloxane bond with a high-molecular weight plasticizer, the amount of the plasticizer being 1-150 parts per 100 parts by weight of the polymer; (b) curing the composition comprising the oxyalkylene polymer and plasticizer; and (c) coating the cured product with an alkyd paint.
Claim 2
Independent Claim
92 words
A method of coating the cured product of an oxyalkylene polymer with an alkyd paint comprising (a) combining an oxyalkylene polymer having at least one silicon-containing group that has a hydroxyl group or a hydrolyzable group bonded to a silicon atom and is capable of crosslinking by forming a siloxane bond with a high-molecular weight plasticizer, the amount of the plasticizer being 1-150 parts per 100 parts by weight of the polymer; (b) curing the composition comprising the oxyalkylene polymer and plasticizer; and (c) coating the cured product with an alkyd paint.
Claim 3
Dependent Claim
19 words
The method of claim 1, wherein the high-molecular weight plasticizer has a molecular weight of from 500 to 15,000.
Claim 4
Dependent Claim
22 words
The method of claim 1, wherein the oxyalkylene polymer contains an average of at least one of said silicon-containing groups per molecule.
Claim 5
Dependent Claim
10 words
The coated product obtained by the method of claim 1.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-02-19 | 1993-08-21 | 1994-02-20 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-02-19 | 1997-08-21 | 1998-02-20 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-02-19 | 2001-08-21 | 2002-02-20 | $7700.00 | Window Closed / Lapsed |