Abstract

Abstract PCT No. PCT/JP87/00673 Sec. 371 Date Apr. 29, 1988 Sec. 102(e) Date Apr. 29, 1988 PCT Filed Sep. 11, 1987 PCT Pub. No. WO88/01849 PCT Pub. Date Mar. 24, 1988.An osteosynthetic pin characterized in that the pin is formed substantially of a poly-L-lactic acid having a molecular weight of at least about 70,000, and is formed by axially drawing about 2 to about 10 times at an elevated temperature of about 70 DEG to about 120 DEG C.

Inventors

  • 👤 Yoshito Ikada
  • 👤 Hyu H. Suong
  • 👤 Yoshihiko Shimizu
  • 👤 Satoshi Watanabe
  • 👤 Tatsuo Nakamura
  • 👤 Masakazu Suzuki
  • 👤 Takeshi Shimamoto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 11:31
CPC Classifications
A; A61; A61B; A61B17/00; A61B17/56; A61B17/58; A61B17/68; A61L; A61L31/00; A61L31/04; A61L31/06; A61B2017/00004; A61F; A61F2/00; A61F2/02; A61F2/30; A61F2002/30001; A61F2002/30108; A61F2002/30199; A61F2002/30205; A61F2002/30207; A61F2230/00; A61F2230/0063; A61F2230/0067; Y; Y10; Y10S; Y10S623/00; Y10S623/909; Y10S623/911

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 41 words
An osteosynthetic pin obtained by shaping a poly-L-lactic acid having a molecular weight of at least about 70,000 and axially drawing the shaped body about 2 to about 10 times at an elevated temperature of about 70° to about 120° C.
Claim 2
Dependent Claim 41 words
An osteosynthetic pin obtained by shaping a poly-L-lactic acid having a molecular weight of at least about 70,000 and axially drawing the shaped body about 2 to about 10 times at an elevated temperature of about 70° to about 120° C.
Claim 3
Dependent Claim 21 words
An osteosynthetic pin as defined in claim 1 wherein the poly-L-lactic acid has a molecular weight of at least about 100,000.
Claim 4
Dependent Claim 27 words
An osteosynthetic pin as defined in claim 1 wherein the poly-L-lactic acid contains about 1 to about 15 wt % of hydroxyapatite admixed with the poly-L-lactic acid.
Claim 5
Dependent Claim 25 words
An osteosynthetic pin as defined in claim 3 wherein the content of hydroxyapatite is in the range of about 5 to about 10 wt %.
Claim 6
Dependent Claim 19 words
An osteosynthetic pin as defined in claim 1 or 3 further comprising a bore extending axially through the pin.
Claim 7
Dependent Claim 44 words
A process for preparing an osteosynthetic pin, omprising: shaping a poly-L-lactic acid having a molecular weight of at least about 70,000 and axially drawing the shaped body about 2 to about 10 times at an elevated temperature of about 70° to about 20° C.
Claim 8
Dependent Claim 44 words
A process for preparing an osteosynthetic pin, omprising: shaping a poly-L-lactic acid having a molecular weight of at least about 70,000 and axially drawing the shaped body about 2 to about 10 times at an elevated temperature of about 70° to about 20° C.

References Cited (Backward Citations)

US4506681A Cited
US4550449A Cited
US4650488A Cited
JPS61135671A Cited
JPS61193666A Cited
US4781183A Cited
JPH06141466A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-02-05 1993-08-07 1994-02-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-02-05 1997-08-07 1998-02-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-02-05 2001-08-07 2002-02-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag