Claims Analysis
Total Claims: 18
Claim 1
Independent Claim
147 words
An aqueous acid copper plating solution comprising one or more bath soluble copper salts in a concentration sufficient to provide a total copper ion content in an amount of from one to ten grams per liter of solution, an acid in an amount where the acid, expressed as sulfuric acid, to copper weight ratio, has an upper limit in accordance with the equation: R=67-2.7 [X ] and a lower limit in accordance with the equation: R=35-1.3 [X ] where, in each equation, R is the weight ratio of hydrogen ion to copper metal and X is the weight of dissolved copper metal in solution and a surfactant conforming to the formula: R'--O--(CH.sub.2 (CH.sub.2 O).sub.n H where R' is an aryl or alkyl group containing from about 2 to 20 carbon atoms and n is an integer whereby the molecular weight of the surfactant is at least 500,000.
Claim 2
Dependent Claim
147 words
An aqueous acid copper plating solution comprising one or more bath soluble copper salts in a concentration sufficient to provide a total copper ion content in an amount of from one to ten grams per liter of solution, an acid in an amount where the acid, expressed as sulfuric acid, to copper weight ratio, has an upper limit in accordance with the equation: R=67-2.7 [X ] and a lower limit in accordance with the equation: R=35-1.3 [X ] where, in each equation, R is the weight ratio of hydrogen ion to copper metal and X is the weight of dissolved copper metal in solution and a surfactant conforming to the formula: R'--O--(CH.sub.2 (CH.sub.2 O).sub.n H where R' is an aryl or alkyl group containing from about 2 to 20 carbon atoms and n is an integer whereby the molecular weight of the surfactant is at least 500,000.
Claim 3
Dependent Claim
16 words
The solution of claim 1 where R varies between 40 to 1 and 60 to 1.
Claim 4
Dependent Claim
18 words
The solution of claim 1 where the acid is sulfuric acid and the copper salt is copper sulfate.
Claim 5
Dependent Claim
21 words
The solution of claim 1 where the dissolved copper content varies from about 3 to 8 grams per liter of solution.
Claim 6
Dependent Claim
8 words
The solution of claim 1 including chloride ions.
Claim 7
Dependent Claim
9 words
The solution of claim 1 where R' is ethylene.
Claim 8
Dependent Claim
16 words
The solution of claim 1 where the molecular weight of the surfactant is at least 2,500,000.
Claim 9
Dependent Claim
24 words
The solution of claim 1 where the surfactant is present in an amount of from 1 to 2500 parts per million parts of solution.
Claim 10
Dependent Claim
24 words
The solution of claim 1 where the surfactant is present in an amount of from 500 to 1500 parts per million parts of solution.
Claim 11
Dependent Claim
205 words
A process for electrolytically depositing copper on the conductive walls of printed circuit board through holes, said process comprising the steps of providing a printed circuit board substrate having through holes with an aspect ratio of at least 10 to 1 and a length of at least 0.100 inches, electrolytically depositing copper onto the walls of said through holes from a copper plating solution comprising one or more bath soluble copper salts in a concentration sufficient to provide a total copper ion content in an amount of from one to ten grams per liter of solution, an acid in an amount where the acid, expressed as sulfuric acid, to copper weight ratio, has an upper limit in accordance with the equation: R=67-2.7 [X ] and a lower limit in accordance with the equation: R=35-1.3 [X ] where in each equation, R is the weight ratio of hydrogen ion to copper metal and X is the weight of dissolved copper metal in solution and a surfactant conforming to the formula: R'-O-(CH.sub.2 CH.sub.2 O).sub.n H where R' is an aryl or alkyl group containing from about 2 to 20 carbon atoms and n is an integer whereby the molecular weight of the surfactant is at least 500,000.
Claim 12
Dependent Claim
205 words
A process for electrolytically depositing copper on the conductive walls of printed circuit board through holes, said process comprising the steps of providing a printed circuit board substrate having through holes with an aspect ratio of at least 10 to 1 and a length of at least 0.100 inches, electrolytically depositing copper onto the walls of said through holes from a copper plating solution comprising one or more bath soluble copper salts in a concentration sufficient to provide a total copper ion content in an amount of from one to ten grams per liter of solution, an acid in an amount where the acid, expressed as sulfuric acid, to copper weight ratio, has an upper limit in accordance with the equation: R=67-2.7 [X ] and a lower limit in accordance with the equation: R=35-1.3 [X ] where in each equation, R is the weight ratio of hydrogen ion to copper metal and X is the weight of dissolved copper metal in solution and a surfactant conforming to the formula: R'-O-(CH.sub.2 CH.sub.2 O).sub.n H where R' is an aryl or alkyl group containing from about 2 to 20 carbon atoms and n is an integer whereby the molecular weight of the surfactant is at least 500,000.
Claim 13
Dependent Claim
16 words
The solution of claim 10 where R varies between 40 to 1 and 60 to 1.
Claim 14
Dependent Claim
18 words
The process of claim 10 where the acid is sulfuric acid and the copper salt is copper sulfate.
Claim 15
Dependent Claim
21 words
The process of claim 10 where the dissolved copper content varies from about 3 to 8 grams per liter of solution.
Claim 16
Dependent Claim
9 words
The process of claim 10 where R is ethylene.
Claim 17
Dependent Claim
16 words
The process of claim 10 where the molecular weight of the surfactant is at least 2,500,000.
Claim 18
Dependent Claim
24 words
The process of claim 10 where the surfactant is present in an amount of from 500 to 1500 parts per million parts of solution.