Abstract

Abstract The present invention relates to a method of processing a silver halide color photosensitive material. In particular, to a rapid processing method capable of reducing the development time. In the processing method, an exposed silver halide color photosensitive material having at least one emulsion layer containing a silver halide having a chlorine content of at least 80 molar % based on the total halogens is processed with a color developer containing an aromatic primary amine color developing agent and a dialkylhydroxylamine of the following general formula (I) but substantially free of benzyl alcohol: ##STR1## wherein R 1 and R 2 each represent an unsubstituted or substituted alkyl group or an unsubstituted or substituted alkenyl group or R 1 and R 2 may form a hetero ring together with nitrogen atom.

Inventors

  • 👤 Takatoshi Ishikawa
  • 👤 Morio Yagihara

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 09:07
CPC Classifications
G; G03; G03C; G03C7/00; G03C7/30; G03C7/407; G03C7/413

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 139 words
A method of processing a silver halide color photosensitive material comprising, processing an exposed silver halide color photosensitive material having at least one emulsion layer containing a silver halide having a chlorine content of at least 80 molar % based on the total halogens with a color developer which is substantially free of benzyl alcohol, said color developer (i) having a pH of about 9 to about 11, (ii) containing sulfites in an amount ranging from about 0 to about 5 g/l, (iii) containing an aromatic primary amine color developing agent, and (iv) containing a dialkylhydroxylamine of the following general formula (I): ##STR28## wherein R 1 and R 2 each represent an unsubstituted or substituted alkyl group or an unsubstituted or substituted alkenyl group or R 1 and R 2 may form a hetero ring together with nitrogen atom.
Claim 2
Independent Claim 139 words
A method of processing a silver halide color photosensitive material comprising, processing an exposed silver halide color photosensitive material having at least one emulsion layer containing a silver halide having a chlorine content of at least 80 molar % based on the total halogens with a color developer which is substantially free of benzyl alcohol, said color developer (i) having a pH of about 9 to about 11, (ii) containing sulfites in an amount ranging from about 0 to about 5 g/l, (iii) containing an aromatic primary amine color developing agent, and (iv) containing a dialkylhydroxylamine of the following general formula (I): ##STR28## wherein R 1 and R 2 each represent an unsubstituted or substituted alkyl group or an unsubstituted or substituted alkenyl group or R 1 and R 2 may form a hetero ring together with nitrogen atom.
Claim 3
Dependent Claim 21 words
The method as set forth in claim 1, wherein the aromatic primary amine color developing agent is selected from p-phenylenediamine derivatives.
Claim 4
Dependent Claim 34 words
The method as set forth in claim 1, wherein the color developer contains the aromatic primary amine color developing agent in an amount of about 0.1 g to 20 per liter of the developer.
Claim 5
Dependent Claim 25 words
The method as set forth in claim 1, wherein R 1 and R 2 in the formula (I) each has 1 to 5 carbon atoms.
Claim 6
Dependent Claim 18 words
The method as set forth in claim 1, wherein the dialkylhydroxylamine is selected from the group of ##STR29##
Claim 7
Dependent Claim 26 words
The method as set forth in claim 1, wherein the dialkylhydroxylamine is contained in an amount of about 0.05 to about 20 g/l in the developer.
Claim 8
Dependent Claim 17 words
The method as set forth in claim 1, wherein no benzyl alcohol is contained in the developer.
Claim 9
Dependent Claim 32 words
The method as set forth in claim 1, wherein the photosensitive material is developed at a temperature of about 20° to about 50° C. for about 20 seconds to about 5 minutes.
Claim 10
Dependent Claim 31 words
The method as set forth in claim 1, wherein the emulsion layer contains a silver halide having a chlorine content of at least 90 molar % based on the total halogens.
Claim 11
Dependent Claim 110 words
The method as set forth in claim 1, wherein the developer further contains (v) an alkanolamine having the following formula (II): ##STR30## wherein R 3 represents a hydroxyalkyl group having 2 to 6 carbon atoms and R 4 and R 5 each represent a hydrogen atom, an alkyl group having 1 to 6 carbon atoms, hydroxyalkyl group having 2 to 6 carbon atoms, benzyl group or a group of the formula: ##STR31## in which n is an integer of 1 to 6 and X and Z each represent a hydrogen atom, an alkyl group having 1 to 6 carbon atoms or a hydroxyalkyl group having 2 to 6 carbon atoms.
Claim 12
Dependent Claim 28 words
The method as set forth in claim 10, wherein the alkanolamine is contained in an amount of about 0.01 to about 20 g per liter of the developer.
Claim 13
Dependent Claim 14 words
The method as set forth in claim 1, wherein the developer contains sulfite ion.
Claim 14
Dependent Claim 26 words
The method as set forth in claim 1, wherein the developer contains 1×10 -4 to 5×10 -2 mol of sulfite ion per liter of the developer.
Claim 15
Dependent Claim 26 words
The method as set forth in claim 1, wherein the developer contains 2.5×10 -3 to 2.5×10 -2 mol of sulfite ion per liter of the developer.
Claim 16
Dependent Claim 19 words
The method as set forth in claim 1, wherein the color photographic material contains a nitrogen atom-split-off yellow coupler.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-10-23 1993-04-24 1993-10-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-10-23 1997-04-24 1997-10-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-10-23 2001-04-24 2001-10-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag