Abstract

Abstract An improved method for extracting copper from copper minerals by heap leaching with dilute sulfuric acid which comprises agglomerating the copper mineral fines prior to their being formed into an heap with an agglomerating agent comprising an anionic acrylamide polymer which contains at least 5 mole percent of carboxylate or sulfonate groups and has a molecular weight of least 100,000.

Inventors

  • 👤 Anthony E. Gross
  • 👤 Jacqueline L. Bonin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 23:44
CPC Classifications
C; C22; C22B; C22B1/00; C22B1/14; C22B1/24; C22B1/242; C22B1/244; C22B15/00; C22B15/0002; C22B15/0004; C22B15/0006; C22B15/0063; C22B15/0065; C22B15/0067; C22B15/0071; Y; Y02; Y02P; Y02P10/00; Y02P10/20

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 84 words
An improved method for extracting copper from copper minerals by heap leaching with dilute sulfuric acid which comprises agglomerating the copper minerals prior to their being formed into a heap with an agglomerating agent comprising an anionic acrylamide polymer which contains at least five mole percent of carboxylate or sulfonate groups and has a molecular weight of at least 100,000 , and then leaching copper from said copper minerals by heap leaching with dilute sulfuric acid, collecting the copper-rich leachate, and recovering copper therefrom.
Claim 2
Dependent Claim 84 words
An improved method for extracting copper from copper minerals by heap leaching with dilute sulfuric acid which comprises agglomerating the copper minerals prior to their being formed into a heap with an agglomerating agent comprising an anionic acrylamide polymer which contains at least five mole percent of carboxylate or sulfonate groups and has a molecular weight of at least 100,000 , and then leaching copper from said copper minerals by heap leaching with dilute sulfuric acid, collecting the copper-rich leachate, and recovering copper therefrom.
Claim 3
Dependent Claim 19 words
An improved method of claim 1 wherein the anionic acrylamide polymer has a molecular weight of at least 3,000,000.
Claim 4
Dependent Claim 19 words
An improved method of claim 1 wherein the anionic acrylamide polymer is an acrylic acid or methacrylic acid polymer.
Claim 5
Dependent Claim 14 words
The improved method of claim 1 wherein the anionic acrylamide polymer contains sulfonate groups.
Claim 6
Dependent Claim 16 words
The improved method of claim 4 where the anionic acrylamide polymer is acrylamide-2-acrylamido,2-methylpropane sulfonic acid copolymer.

References Cited (Backward Citations)

US28474A Cited
US3284393A Cited
US3418237A Cited
US3893847A Cited
USRE28474E Cited
USRE28474F1 Cited
US3692673A Cited
US4802914A Cited
US4703092A Cited
EP0225596A2 Cited
US4704209A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-10-23 1993-04-24 1993-10-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-10-23 1997-04-24 1997-10-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-10-23 2001-04-24 2001-10-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag