Method for manufacturing lenses

Assignee: EssilorLuxottica SA
•
Filing: 1987-10-30
•
Granted: 1989-10-10
•
Expires: 2007-10-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The disclosure relates to a method and apparatus for manufacturing lenses including the use of a wafer in conjunction with liquid monomer to provide a molded plastic lens. In the molding process, a first mold form is sealingly secured to a gasket to form a part of a mold for receiving liquid monomer. The liquid monomer is poured into the first mold form and the wafer material which can be tinted or have a different index of refraction is then placed in contiguous relationship with the liquid monomer. A second mold form is then secured into the gasket in sealing relationship therewith and spaced from the wafer to form a cavity therebetween. Liquid monomer is then introduced into the cavity to fill all the voids. The mold with the material to be molded is then placed in the oven and cured. After the curing process is completed, the mold is removed and the formed lens extracted. An alternative includes the use of a mold form which is of the same material as the monomer such that it ultimately forms part of the lens. In this instance, the mold form is consumed during the molding process as it becomes bonded by intermolecular action with the liquid monomer.

Inventors

  • 👤 Ronald D. Blum

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 01:07
CPC Classifications
B; B29; B29D; B29D11/00; B29D11/00009; B29D11/0048; B29D11/00528; B29D11/00028; B29D11/00317; B29D11/00413

Claims Analysis

Total Claims: 26
Claim 1
Independent Claim 153 words
A method for tinting plastic lens comprising: (a) arrange a first mold form for receiving molding material; (b) delivering plastic molding material to said first mold form; (c) inserting a tinted wafer of solidified plastic material capable of intermolecular bonding with said plastic molding material into said first mold form in contiguous relationship with said plastic molding material; (d) fixing a second mold form in sealed relationship with said first mold form to form a mold having a cavity between said wafer and said second mold form; (e) inserting additional plastic molding material into said mold cavity; (f) said mold forms configured to form a lens of preselected shape; (g) subjecting said mold to oven curing process to solidify the plastic molding material and to cause intermolecular bonding between the molding material and the wafer; and (h) removing said molded material from said mold with said wafer in the form of a lens.
Claim 2
Independent Claim 153 words
A method for tinting plastic lens comprising: (a) arrange a first mold form for receiving molding material; (b) delivering plastic molding material to said first mold form; (c) inserting a tinted wafer of solidified plastic material capable of intermolecular bonding with said plastic molding material into said first mold form in contiguous relationship with said plastic molding material; (d) fixing a second mold form in sealed relationship with said first mold form to form a mold having a cavity between said wafer and said second mold form; (e) inserting additional plastic molding material into said mold cavity; (f) said mold forms configured to form a lens of preselected shape; (g) subjecting said mold to oven curing process to solidify the plastic molding material and to cause intermolecular bonding between the molding material and the wafer; and (h) removing said molded material from said mold with said wafer in the form of a lens.
Claim 3
Dependent Claim 44 words
The method according to claim 1 wherein said mold includes a flexible gasket with means for releasably securing said first mold in sealable relationship therewith and means for releasably securing said second mold form in sealable relationship therewith spaced from said first mold form.
Claim 4
Dependent Claim 59 words
The method according to claim 2 wherein said first mold form has a generally circular periphery and an internal concave configuration, and said second mold form has a generally circular periphery with an internal surface which is generally convex in configuration; and said wafer being generally circular having an effective diameter substantially identical to that of said mold forms.
Claim 5
Dependent Claim 43 words
The method according to claim 3 wherein said plastic molding material is a liquid monomer and said step of inserting additional molding material includes injecting through the interface between at least one of said mold forms and said flexible gasket said liquid monomer.
Claim 6
Dependent Claim 20 words
The method according to claim 4 wherein said wafer has attached jewelry thereto prior to insertion of said tinted wafer.
Claim 7
Dependent Claim 25 words
The method according to claim 4 wherein said wafer of plastic material and said monomer are formed from the same material of allyl diglycol carbonate.
Claim 8
Dependent Claim 19 words
The method according to claim 6 wherein the molde are configured to produce plastic lens conforming to prescription eyeglasses.
Claim 9
Dependent Claim 20 words
The method according to claim 4 wherein said wafer has attached indicia thereto prior to insertion of said tinted wafer.
Claim 10
Independent Claim 120 words
A method for manufacturing tinted plastic lenses comprising: (a) tinting a plastic preform by dipping the preform into a bath of dye having the desired color; (b) said tinted preform configured to be a first preform of a mold for lenses; (c) fixing a second mold form with respect to said first preform in sealed relationship therewith to form a cavity therebetween; (d) introducing into said cavity plastic molding material capable of intermolecular bonding with said first plastic preform; (e) subjecting said mold to an oven curing process to solidify the moldable plastic material and to cause intermolecular bonding between the plastic material and said first preform; and (f) removing from the mold the preform bonded to the molding material.
Claim 11
Independent Claim 120 words
A method for manufacturing tinted plastic lenses comprising: (a) tinting a plastic preform by dipping the preform into a bath of dye having the desired color; (b) said tinted preform configured to be a first preform of a mold for lenses; (c) fixing a second mold form with respect to said first preform in sealed relationship therewith to form a cavity therebetween; (d) introducing into said cavity plastic molding material capable of intermolecular bonding with said first plastic preform; (e) subjecting said mold to an oven curing process to solidify the moldable plastic material and to cause intermolecular bonding between the plastic material and said first preform; and (f) removing from the mold the preform bonded to the molding material.
Claim 12
Dependent Claim 28 words
The method according to claim 9 wherein said first preform is hard-coated on one exterior surface prior to said preform being fixed relative to said second mold form.
Claim 13
Dependent Claim 21 words
The method for forming a lens according to claim 10 wherein said hard-coat application step occurs independently of any tinting step.
Claim 14
Dependent Claim 85 words
The method according to claim 10 wherein said mold includes a flexible gasket, said first preform has an interior surface which is concave in configuration, and said second mold form includes an interior surface which is convex in configuration, said first preform and said second mold form being configured to form a lens of a preselected prescription for use with eyeglasses; said gasket including means for retaining said first preform and said second mold form in sealed spaced relationship to form the mold cavity therebetween.
Claim 15
Dependent Claim 30 words
The method according to claim 12 wherein at least one of said first preform and said molding material is formed from a plastic material that is softer than the other.
Claim 16
Dependent Claim 61 words
The method according to claim 12 wherein prior to fixing said second mold form, liquid molding material is placed into said mold, photochromatic wafer is placed in contiguous relationship with said liquid plastic molding material, said second form is then fixed with respect to said first preform in sealed relationship to form a cavity between the wafer and said first preform.
Claim 17
Dependent Claim 64 words
The method according to claim 12 wherein prior to fixing said second mold form, liquid molding material is placed into said mold, a wafer of polarized material is placed in contiguous relationship with said liquid plastic molding material, said second preform is then fixed with respect to said first form in sealed relationship to form a cavity between the wafer and said first preform.
Claim 18
Independent Claim 116 words
A method for manufacturing multifocal lens comprising: (a) arranging a first mold form for receiving the plastic molding material; (b) delivering plastic molding material to said first mold form; (c) inserting a wafer having a different index of refraction into said first mold portion in contiguous relationship with said plastic molding material; (d) closing said mold with a second mold form to form a cavity between said second mold form and said wafer; (e) inserting additional plastic molding material into said cavity; (f) subjecting said mold to oven curing process solidifying said plastic molding material and to cause intermolecular bonding between the molding material and said wafer; and (g) removing said molding material from said mold.
Claim 19
Independent Claim 116 words
A method for manufacturing multifocal lens comprising: (a) arranging a first mold form for receiving the plastic molding material; (b) delivering plastic molding material to said first mold form; (c) inserting a wafer having a different index of refraction into said first mold portion in contiguous relationship with said plastic molding material; (d) closing said mold with a second mold form to form a cavity between said second mold form and said wafer; (e) inserting additional plastic molding material into said cavity; (f) subjecting said mold to oven curing process solidifying said plastic molding material and to cause intermolecular bonding between the molding material and said wafer; and (g) removing said molding material from said mold.
Claim 20
Dependent Claim 39 words
The method according to claim 16 wherein said wafer includes a portion of which has a configuration different from the remainder of said wafer to obtain a different power corresponding to that of at least of a bifocal lens.
Claim 21
Independent Claim 95 words
A method for making multifocal lens comprising: (a) forming a first plastic preform having at least a portion with a power different than the remainder of the plastic preform and configured to be part of the lens for use in eyeglasses; (b) fixing a second mold form in sealed relationship with said first preform to form a cavity therebetween; (c) introducing into said cavity plastic molding material; (d) subjecting said mold to an oven curing process to solidify the plastic molding material and to cause intermolecular bonding between the molding material and said first preform.
Claim 22
Independent Claim 95 words
A method for making multifocal lens comprising: (a) forming a first plastic preform having at least a portion with a power different than the remainder of the plastic preform and configured to be part of the lens for use in eyeglasses; (b) fixing a second mold form in sealed relationship with said first preform to form a cavity therebetween; (c) introducing into said cavity plastic molding material; (d) subjecting said mold to an oven curing process to solidify the plastic molding material and to cause intermolecular bonding between the molding material and said first preform.
Claim 23
Dependent Claim 21 words
The method according to claim 18 wherein said first preform is hard-coated prior to being fixed relative to said second form.
Claim 24
Dependent Claim 30 words
The method according to claim 18 wherein said first preform is tinted prior to being fixed relative to said second form by dipping said form into a bath of dye.
Claim 25
Dependent Claim 24 words
The method according to claim 18, 19, or 20 wherein said first preform is made of the same material as said plastic molding material.
Claim 26
Dependent Claim 16 words
The method according to claim 20 wherein said material is a monomer of allyl diglycol carbonate.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-10-09 1993-04-10 1993-10-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-10-09 1997-04-10 1997-10-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-10-09 2001-04-10 2001-10-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag