Abstract

Abstract Disclosed is a novel polymer of this invention which comprises having a recurring unit represented by the formula: <IMAGE> (I) and having a reduced viscosity ( eta sp/c) of 0.2 dl/g or more at 60 DEG C. in a solution of a concentration of 0.2 g/dl in p-chlorophenol as a solvent, a method for preparing the same which comprises reacting a dihalogenobenzonitrile represented by the formula: <IMAGE> (II) wherein X represents a halogen atom, with an alkali metal salt of resorcin represented by the formula: <IMAGE> (III) wherein M represents an alkali metal, in the presence of a solvent; and then treating the reaction product obtained by water or alcohol, and molding materials and molded products employing the polycyanoaryl ether.

Inventors

  • 👤 Shigeru Matsuo
  • 👤 Tomoyoshi Murakami
  • 👤 Thoru Bando
  • 👤 Kikuo Nagatoshi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 09:41
CPC Classifications
C; C08; C08G; C08G65/00; C08G65/34; C08G65/38; C08G65/40; C08G65/4006; C08L; C08L71/00; C08G2650/00; C08G2650/62; C08G2650/64

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 64 words
A resinous composition comprising 10 to 90% by weight of a polycyanoaryl ether containing a recurring unit represented by the formula: ##STR10## and having a reduced viscosity (ηsp/c) of 0.3 d/g or more at 6020 C. in a solution of a concentration of 0.2 g/dl in p-chlorophenol as a solvent, as a main component, and 10 to 90% by weight of a thermoplastic resin.
Claim 2
Dependent Claim 64 words
A resinous composition comprising 10 to 90% by weight of a polycyanoaryl ether containing a recurring unit represented by the formula: ##STR10## and having a reduced viscosity (ηsp/c) of 0.3 d/g or more at 6020 C. in a solution of a concentration of 0.2 g/dl in p-chlorophenol as a solvent, as a main component, and 10 to 90% by weight of a thermoplastic resin.
Claim 3
Dependent Claim 33 words
The resinous composition according to claim 1, wherein the thermoplastic resin is at least one selected from the group consisting of polycarbonate, polyethylene terephthalate, polybutylene terephthalate, polyether ketone, polysulfone, polyetherimide, and polyphenylene sulfide.
Claim 4
Dependent Claim 15 words
The resinous composition according to claim 1 wherein the thermoplastic resin comprises polyether ether ketone.
Claim 5
Dependent Claim 13 words
The resinous composition according to claim 1 wherein the thermoplastic resin comprises polyethersulfone.
Claim 6
Dependent Claim 13 words
The resinous composition according to claim 1 wherein the thermoplastic resin comprises polyamidoimide.

References Cited (Backward Citations)

US4567248A Cited
US4663427A Cited
US4640975A Cited
US4640974A Cited
US4703104A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-07-31 1993-01-30 1993-08-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-07-31 1997-01-30 1997-08-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-07-31 2001-01-30 2001-08-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag