Method for scale and corrosion inhibition in a well penetrating a subterranean formation

Assignee: Mobil Oil AS
•
Filing: 1987-11-18
•
Granted: 1988-11-29
•
Expires: 2007-11-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for inhibiting the formation of scale and corrosion in a well penetrating a subterranean formation for the production of fluids from the formation comprising injecting a predetermined amount of microparticles of a basic anion exchange resin providing a source of polycations into the formation about the well and that are trapped and retained by the interstices of the formation without rendering the interstices or the formation impermeable to the flow of fluids. Thereafter a predetermined amount of an aqueous solution of scale and corrosion inhibitor is injected into the formation about the well that contacts the basic anion exchange resin and becomes fixed in a slightly soluble state either by complexation with the polycations or is precipitated by the polycations in the exchange resin. The scale and corrosion inhibitor is released slowly at effective concentration into fluids produced by the well to inhibit scale formation and corrosion.

Inventors

  • 👤 Earl S. Snavely, Jr.
  • 👤 John Hen

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 17:20
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/52; C09K8/528; C09K8/54; E; E21; E21B; E21B37/00; E21B37/06; E21B41/00; E21B41/02; Y; Y10; Y10S; Y10S166/00; Y10S166/902; Y10S507/00; Y10S507/927

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 128 words
A method for inhibiting scale and corrosion in a well penetrating a subterranean formation for the production of fluids from the formation comprising: (a) injecting a predetermined amount of microparticles of a basic anion exchange resin providing a source of polycations into the formation about the well that are trapped and retained by the interstices of the formation without rendering said interstices or the formation impermeable to the flow of fluids; and (b) injecting a predetermined amount of an aqueous solution of scale and corrosion inhibitor into the formation about the well that contacts the basic anion exchange resin providing a source of polycations and becomes fixed in a slightly soluble state either by complexation with the polycations or is precipitated by the polycations contained in said resin.
Claim 2
Independent Claim 128 words
A method for inhibiting scale and corrosion in a well penetrating a subterranean formation for the production of fluids from the formation comprising: (a) injecting a predetermined amount of microparticles of a basic anion exchange resin providing a source of polycations into the formation about the well that are trapped and retained by the interstices of the formation without rendering said interstices or the formation impermeable to the flow of fluids; and (b) injecting a predetermined amount of an aqueous solution of scale and corrosion inhibitor into the formation about the well that contacts the basic anion exchange resin providing a source of polycations and becomes fixed in a slightly soluble state either by complexation with the polycations or is precipitated by the polycations contained in said resin.
Claim 3
Dependent Claim 56 words
The method of claim 1 wherein the scale and corrosion inhibitor is an organic polycarboxylic acid, modified polyacrylic acid, homopolymers or copolymers where one component is an alpha, beta-ethylenically unsaturated acid monomer and the other component is an alpha, beta-ehthylenically unsaturated monomer with a non-polar, polar or ionic functional group, phosphates, phosphate esters and organic polyphosphonates.
Claim 4
Dependent Claim 21 words
The method of claim 1 wherein the microparticles of a basic anion exchange resin have a diameter less than ten microns.
Claim 5
Dependent Claim 18 words
The method of claim 3 wherein the basic anion exchange resin comprises a strongly basic anion exchange resin.
Claim 6
Dependent Claim 20 words
The method of claim 3 wherein the basic anion exchange resin or substance comprises a weakly basic anion exchange resin.
Claim 7
Dependent Claim 18 words
The method of claim 3 wherein the basic anion exchange resin comprises a moderately basic anion exchange resin.
Claim 8
Dependent Claim 50 words
The method of claim 1 wherein the basic anion exchange resin providing a source of polycations and the scale and corrosion inhibitor fixed in a slightly soluble state either by complexation with the polycations or precipitation by the polycations are preblended prior to injection into the formation about the well.

References Cited (Backward Citations)

US2437475A Cited
US3481400A Cited
US3547817A Cited
US3633672A Cited
US4231869A Cited
US4393938A Cited
US4495996A Cited
US4602683A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-11-29 1992-05-30 1992-11-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-11-29 1996-05-30 1996-11-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-11-29 2000-05-30 2000-11-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag