Abstract

Abstract Resilient surface coverings having improved scratch and stain resistance are disclosed in which a first top layer of a thermally-cured composition of a polyol component, an aminoplast component and an acid catalyst is adhered to a crosslinked or crosslinkable second layer material. A process to prepare such surface coverings is also disclosed.

Inventors

  • 👤 Nicholas C. Bolgiano
  • 👤 Mary B. Grubb
  • 👤 Raymond S. Hudson
  • 👤 William T. Sigman

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 14:19
CPC Classifications
C; C08; C08J; C08J5/00; C08J5/12; D; D06; D06N; D06N3/00; D06N3/04; D06N3/06; D06N3/08; D06N3/12; D06N3/18; D06N3/183; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31551; Y10T428/31573; Y10T428/3158; Y10T428/31594; Y10T428/31786; Y10T428/31797; Y10T428/31942

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 120 words
A resilient surface covering, said covering comprising a resilient support surface; and a resilient wear layer bonded to said support surface, said wear layer comprising a top first layer material and a crosslinked underlying second layer material selected from the group consisting of a moisture cured polyurethane, a moisture and UV-cured polyurethane, a UV-cured polyurethane and a cured unsaturated polyester adhered to said support surface, said first layer material being obtained from the thermal curing of a composition comprising a polyol component, an aminoplast component, and an acid catalyst component wherein said first layer material conforms to physical deformations of said crosslinked second layer material and having improved scratch and stain resistance properties relative to said crosslinked second layer material.
Claim 2
Dependent Claim 120 words
A resilient surface covering, said covering comprising a resilient support surface; and a resilient wear layer bonded to said support surface, said wear layer comprising a top first layer material and a crosslinked underlying second layer material selected from the group consisting of a moisture cured polyurethane, a moisture and UV-cured polyurethane, a UV-cured polyurethane and a cured unsaturated polyester adhered to said support surface, said first layer material being obtained from the thermal curing of a composition comprising a polyol component, an aminoplast component, and an acid catalyst component wherein said first layer material conforms to physical deformations of said crosslinked second layer material and having improved scratch and stain resistance properties relative to said crosslinked second layer material.
Claim 3
Dependent Claim 33 words
The product of claim 1 wherein the polyol component comprises alcohols having two or more alcohol groups and polymeric aqueous dispersion or emulsion resins containing reactive hydroxy or carbonyl functionality, and mixtures thereof.
Claim 4
Dependent Claim 34 words
The product of claim 1 wherein the polyol component comprises, at least in part, an alcohol chosen from the group consisting of 1,6-hexanediol, 1,4-cyclohexane dimethanol, glycerine, neopentyl glycol, tripropylene glycol, 1,4-butanediol, trimethylolpropane and pentaerythritol.
Claim 5
Dependent Claim 23 words
The product of claim 1 wherein said aminoplast component comprises, at least in part, a substantially fully methylolated and substantially fully alkylated melamine.
Claim 6
Dependent Claim 11 words
The product of claim 5 wherein said melamine is hexamethoxymethyl melamine.
Claim 7
Dependent Claim 18 words
The product of claim 1 wherein said acid catalyst component comprises, at least in part, a sulfonic acid.
Claim 8
Dependent Claim 11 words
The product of claim 1 wherein said composition additionally comprises water.
Claim 9
Dependent Claim 14 words
The product of claim 7 wherein said composition additionally comprises at least one surfactant.
Claim 10
Dependent Claim 42 words
The product of claim 7 wherein said composition additionally comprises at least two surfactants, the combination of which provides an improved stain resistance to the cured product relative to a cured product prepared from the same components but without utilizing said surfactants.
Claim 11
Dependent Claim 14 words
The product of claim 9 wherein one of the surfactants is a fluoroaliphatic surfactant.

References Cited (Backward Citations)

US4528344A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-11-01 1992-05-02 1992-11-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-11-01 1996-05-02 1996-11-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-11-01 2000-05-02 2000-11-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag