Abstract
Abstract A hydrolyzable resin composition consisting essentially of a resin selected from the group consisting of an acrylic resin, a polyester resin and an epoxy resin and an organic solvent in which the resin is soluble, wherein said resin has at least one side chain bearing at least one terminal group of the formula: -X-[O-M-R]x wherein X represents <IMAGE> M is a metal selected from zinc, copper and tellurium; x is an integer of 1 to 2; R represents an organic acid residue selected from <IMAGE> +TR <IMAGE> and R1 is a monovalent organic residue, and the metal content of said resin is 0.3 to 20% by weight of the resin. The subject composition provides superior antifouling coating compositions.
Inventors
- 👤 Naoki Yamamori
- 👤 Hiroharu Ohsugi
- 👤 Yoshio Eguchi
- 👤 Junji Yokoi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 18:19
CPC Classifications
C; C08; C08G; C08G59/00; C08G59/14; C08G59/1433; C08F; C08F30/00; C08F30/04; C08G63/00; C08G63/68; C09; C09D; C09D5/00; C09D5/16; C09D5/1606; C09D5/1637; C09D5/165
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
119 words
An antifouling coating composition having improved polishing property and consisting essentially of a resin selected from the group consisting of an acrylic resin, a polyester resin and an epoxy resin, an organic solvent in which said resin is soluble, a pigment and other optional additives, wherein said resin has at least one side chain bearing at least one terminal group of the formula: ##STR16## wherein X represents ##STR17## M is a metal selected from zinc, copper and tellurium; x is an integer of 1 to 2, R represents an organic acid residue selected from ##STR18## and R 1 is a monovalent organic residue, and the metal content of said resin is 0.3 to 20% by weight of the resin.
Claim 2
Dependent Claim
119 words
An antifouling coating composition having improved polishing property and consisting essentially of a resin selected from the group consisting of an acrylic resin, a polyester resin and an epoxy resin, an organic solvent in which said resin is soluble, a pigment and other optional additives, wherein said resin has at least one side chain bearing at least one terminal group of the formula: ##STR16## wherein X represents ##STR17## M is a metal selected from zinc, copper and tellurium; x is an integer of 1 to 2, R represents an organic acid residue selected from ##STR18## and R 1 is a monovalent organic residue, and the metal content of said resin is 0.3 to 20% by weight of the resin.
Claim 3
Dependent Claim
17 words
The composition according to claim 1 wherein R is a monovalent organic residue having an antifouling property.
Claim 4
Dependent Claim
69 words
The composition according to claim 1 wherein R 1 represents ##STR19## in which R 2 is hydrogen or a hydrocarbon residue having 1 to 12 carbon atoms, and R 3 and R 4 each represents a hydrocarbon residue having 1 to 12 carbon atoms, R 5 is a hydrocarbon residue having 1 to 4 carbon atoms and R 6 is a cyclic hydrocarbon having 5 to 12 carbon atoms.
Claim 5
Dependent Claim
15 words
The composition according to claim 1 wherein an antifouling agent is employed as the additive.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-09-27 | 1992-03-28 | 1992-09-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-09-27 | 1996-03-28 | 1996-09-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-09-27 | 2000-03-28 | 2000-09-27 | $7700.00 | Window Closed / Lapsed |