Claims Analysis
Total Claims: 18
Claim 1
Independent Claim
90 words
A method of producing a lowered formaldehyde release durable press fabric comprising: oxidizing a solution of a carbamate finishing agent containing free formaldehyde and a durable press catalyst for cellulose with a sufficient amount of magnesium monoperoxyphthalate oxidant to produce a durable press finishing treatment bath having a decreased free formaldehyde content; immersing a cellulose containing fabric in said durable press finishing treatment bath; and then, drying and curing said cellulose containing fabric for sufficient time and temperature to produce durable press and low formaldehyde release properties in the fabric.
Claim 2
Independent Claim
90 words
A method of producing a lowered formaldehyde release durable press fabric comprising: oxidizing a solution of a carbamate finishing agent containing free formaldehyde and a durable press catalyst for cellulose with a sufficient amount of magnesium monoperoxyphthalate oxidant to produce a durable press finishing treatment bath having a decreased free formaldehyde content; immersing a cellulose containing fabric in said durable press finishing treatment bath; and then, drying and curing said cellulose containing fabric for sufficient time and temperature to produce durable press and low formaldehyde release properties in the fabric.
Claim 3
Dependent Claim
50 words
The method of claim 1 wherein the padded fabric is cured for from about 120° C. to 240° C. for from about 0.25 to about 10 minutes, time and temperature being inversely adjusted and the concentration of carbamate finishing agent in the pad bath is from about 4% to 12%.
Claim 4
Independent Claim
59 words
A method of producing a lowered free formaldehyde release carbamate durable press finished fabric comprising immersing a high free formaldehyde release carbamate durable press finished fabric in a solution of magnesium monoperoxyphthalate oxidant of sufficient concentration of sufficient time and temperature to oxidize the free formaldehyde and thereby produce a lowered free formaldehyde release carbamate durable press finished fabric.
Claim 5
Independent Claim
59 words
A method of producing a lowered free formaldehyde release carbamate durable press finished fabric comprising immersing a high free formaldehyde release carbamate durable press finished fabric in a solution of magnesium monoperoxyphthalate oxidant of sufficient concentration of sufficient time and temperature to oxidize the free formaldehyde and thereby produce a lowered free formaldehyde release carbamate durable press finished fabric.
Claim 6
Dependent Claim
42 words
The method of claim 3 wherein the concentration of magnesium monoperoxyphthalate oxident is 0.1 to 10.25% and the temperature is from about 5° to 90° C. for from about 1 to 60 minutes at a pH of from about 6 to 9.
Claim 7
Independent Claim
42 words
A method of producing a concentrated carbamate finishing agent solution of lowered free formaldehyde content comprising oxidizing a carbamate finishing agent solution containing free formaldehyde with a sufficient amount of magnesium monoperoxyphthalate oxidant to decrease the free formaldehyde content of the solution.
Claim 8
Independent Claim
42 words
A method of producing a concentrated carbamate finishing agent solution of lowered free formaldehyde content comprising oxidizing a carbamate finishing agent solution containing free formaldehyde with a sufficient amount of magnesium monoperoxyphthalate oxidant to decrease the free formaldehyde content of the solution.
Claim 9
Dependent Claim
23 words
The method of claim 5 wherein the carbamate finishing agent solution is prepared from the reaction of an alkyl or alkoxyalkylcarbamate and formaldehyde.
Claim 10
Dependent Claim
17 words
The method of claim 6 wherein the alkyl or alkoxyalkyl group contains less than 6 carbon atoms.
Claim 11
Dependent Claim
14 words
The method of claim 7 wherein the amido moiety contains hydroxymethyl, methoxymethyl or hydroxyethoxymethyl.
Claim 12
Dependent Claim
30 words
The method of claim 7 wherein the concentration of magnesium monoperoxyphthalate is from about 0.1% to 10.25% by wt of solution and the pH is from about 6 to 9.
Claim 13
Independent Claim
53 words
A method for producing a lowered free formaldehyde durable press finishing treatment bath for cellulose containing fabric comprising oxidizing a solution of a carbamate finishing agent containing free formaldehyde and a durable press catalyst for cellulose with a sufficient amount of magnesium monoperoxyphthalate oxidant to decrease the free formaldehyde content of said solution.
Claim 14
Independent Claim
53 words
A method for producing a lowered free formaldehyde durable press finishing treatment bath for cellulose containing fabric comprising oxidizing a solution of a carbamate finishing agent containing free formaldehyde and a durable press catalyst for cellulose with a sufficient amount of magnesium monoperoxyphthalate oxidant to decrease the free formaldehyde content of said solution.
Claim 15
Dependent Claim
47 words
The method of claim 10 wherein the durable press catalyst for cellulose is selected from the group consisting of mineral acids. organic acids, salts of strong acids, alkanolamine salts, metallic salts of strong acids and weak bases such as zinc nitrate and magnesium chloride, and combinations thereof.
Claim 16
Dependent Claim
23 words
The method of claim 10 wherein the carbamate finishing agent solution is prepared from the reaction of an alkyl or alkoxyalkylcarbamate and formaldehyde.
Claim 17
Dependent Claim
27 words
The method of claim 12 wherein the alkyl or alkoxyalkyl group contains less than 6 carbon atoms and the amido moiety contains hydroxymethyl, methoxymethyl or hydroxyethoxymethyl groups.
Claim 18
Dependent Claim
29 words
The method of claim 12 wherein the carbamate concentration is from about 4 to 12% and the magnesium monoperoxyphthalate is from about 0.1 to 10.25% by wt of solution.