Pyrolytic boron nitride crucible and method for producing the same
Assignee: Denka Co Ltd
•
Filing: 1986-05-22
•
Granted: 1988-09-27
•
Expires: 2006-05-22
Abstract
Abstract A pyrolytic boron nitride crucible is provided. The crucible contains at least five wall layers consisting of first and second wall layers. The thickness of each of the first wall layers is 5 to 100 microns and the thickness of each of the second wall layers is 1/50 to 1/1 of that of the first wall layer. The total thickness of the entire wall layers is 0.5 to 3 mm. The first wall layer is bonded to and laminated alternately with the second wall layer.
Inventors
- 👤 Hiroaki Tanji
- 👤 Masaharu Suzuki
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 17:22
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/515; C04B35/58; C04B35/583; C23; C23C; C23C16/00; C23C16/22; C23C16/30; C23C16/34; C23C16/342; C30; C30B; C30B15/00; C30B15/10; C30B23/00; C30B23/02; C30B23/06; C30B23/066
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
151 words
A pyrolytic boron nitride crucible having a multi-walled pyrolytic boron nitride structure comprising at least five wall layers of pyrolytic boron nitride, each of first pyrolytic boron nitride wall layers having a thickness of 20 to 100 microns, each of second pyrolytic boron nitride wall layers having a thickness of 1/50 to 1/2 of that of each first wall layer, all pyrolytic boron nitride wall layers combined having a thickness of 0.5 to 3 mm, and said first wall layer being bonded to and laminated alternately with said second wall layer, whereby peeling of one wall layer is prevented from affecting other wall layers so that peeling of one wall layer is not propagated into an adjacent layer, whereupon an exfoliated innermost pyrolytic boron nitride layer is peeled and a pyrolytic boron nitride layer adjacent said exfoliated innermost layer becomes a new innermost wall layer for subsequent use of the crucible.
Claim 2
Dependent Claim
151 words
A pyrolytic boron nitride crucible having a multi-walled pyrolytic boron nitride structure comprising at least five wall layers of pyrolytic boron nitride, each of first pyrolytic boron nitride wall layers having a thickness of 20 to 100 microns, each of second pyrolytic boron nitride wall layers having a thickness of 1/50 to 1/2 of that of each first wall layer, all pyrolytic boron nitride wall layers combined having a thickness of 0.5 to 3 mm, and said first wall layer being bonded to and laminated alternately with said second wall layer, whereby peeling of one wall layer is prevented from affecting other wall layers so that peeling of one wall layer is not propagated into an adjacent layer, whereupon an exfoliated innermost pyrolytic boron nitride layer is peeled and a pyrolytic boron nitride layer adjacent said exfoliated innermost layer becomes a new innermost wall layer for subsequent use of the crucible.
References Cited (Backward Citations)
US2291083A
Cited
US559868A
Cited
US1803135A
Cited
US1996660A
Cited
US2721364A
Cited
US2947114A
Cited
US3181845A
Cited
US3148238A
Cited
US3491992A
Cited
US3345059A
Cited
US3328017A
Cited
US3734480A
Cited
US3779699A
Cited
US4005982A
Cited
US3986822A
Cited
US4055391A
Cited
US4528163A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-09-27 | 1992-03-28 | 1992-09-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-09-27 | 1996-03-28 | 1996-09-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-09-27 | 2000-03-28 | 2000-09-27 | $7700.00 | Window Closed / Lapsed |