Abstract

Abstract High molecular weight viscoelastic polymers are dissolved by passing the polymer solution through a die which "beads" the polymer allowing the formation of very fine filaments which are drawn into the flow. The beading and flow rate are balanced to maintain constant fine filament formation.

Inventors

  • 👤 Steven L. Baxter
  • 👤 Max H. Lewis

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 16:45
CPC Classifications
C; C08; C08J; C08J3/00; C08J3/02; C08J3/03; C09; C09K; C09K3/00; C10; C10L; C10L1/00; C10L1/10; C10L1/14; C10L1/16; C10L1/1625; C10L1/1633; C10L1/1641; C08J2300/00; C08J2300/10; Y; Y10; Y10T; Y10T137/00; Y10T137/0318; Y10T137/0391

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 106 words
A method for increasing the effectiveness of a drag reducing polymer in reducing the friction loss of flowing liquids through conduits, comprising injecting a drag reducing polymer solution through multiple orifices no larger than 2 millimeters in the largest dimension and allowing the flowing liquid moving past the extruded polymer to dissolve said polymer, wherein the injection rate is such that substantially no reagglomeration occurs on the flowing liquid/conduit side of the orifices prior to dissolution by the flowing liquid and such that the polymer concentrate forms very small filaments of diameter less than 2 millimeters and length less than about 10 meters prior to dissolution.
Claim 2
Independent Claim 106 words
A method for increasing the effectiveness of a drag reducing polymer in reducing the friction loss of flowing liquids through conduits, comprising injecting a drag reducing polymer solution through multiple orifices no larger than 2 millimeters in the largest dimension and allowing the flowing liquid moving past the extruded polymer to dissolve said polymer, wherein the injection rate is such that substantially no reagglomeration occurs on the flowing liquid/conduit side of the orifices prior to dissolution by the flowing liquid and such that the polymer concentrate forms very small filaments of diameter less than 2 millimeters and length less than about 10 meters prior to dissolution.
Claim 3
Dependent Claim 25 words
A method as described in claim 1 wherein the drag reducing polymer is a hydrocarbon soluble polymer and the flowing liquid is a hydrocarbon liquid.
Claim 4
Dependent Claim 28 words
A method as described in claim 2 wherein the drag reducing polymer is substantially an olefin polymer having an inherent viscosity of at least 11 deciliters per gram.
Claim 5
Dependent Claim 25 words
A method as described in claim 3 wherein the olefin-polymer contains at least 60 percent by weight olefinic monomers having at least 6 carbon atoms.
Claim 6
Dependent Claim 26 words
A method as described in claim 3 wherein the orifices are provided by a mesh having openings no larger than 1 millimeter in the largest dimension.
Claim 7
Dependent Claim 24 words
A method as described in claim 1 wherein the drag reducing polymer is a water-soluble polymer and the flowing liquid is an aqueous fluid.
Claim 8
Dependent Claim 28 words
A method as described in claim 1 wherein the high molecular weight polymer is used as a jet fuel anti-mist additive and the flowing liquid is jet fuel.
Claim 9
Dependent Claim 25 words
A method as described in claim 1 wherein the high molecular weight polymer is substantially an alphaolefin polymer and the flowing liquid is petroleum oil.

References Cited (Backward Citations)

US3601079A Cited
US3826279A Cited
US3736288A Cited
US3827447A Cited
US3891593A Cited
US4263926A Cited
US4340076A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-09-20 1992-03-21 1992-09-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-09-20 1996-03-21 1996-09-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-09-20 2000-03-21 2000-09-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag