Polyethylene resin blend

Assignee: Union Camp Corp
•
Filing: 1987-07-23
•
Granted: 1988-09-13
•
Expires: 2007-07-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A polyethylene resin blend is made up from high molecular weight high density polyethylene resin, a linear low density polyethylene resin, and a very low density polyethylene resin. The blend is useful to fabricate films characterized in part by a softness with relatively high strength.

Inventors

  • 👤 William W. Furrer
  • 👤 Ajit K. Bose

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 09:58
CPC Classifications
C; C08; C08L; C08L23/00; C08L23/02; C08L23/04; C08L23/06; C08L2205/00; C08L2205/02; C08L2205/03; C08L23/08; C08L23/0807; C08L23/0815; Y; Y10; Y10T; Y10T428/00; Y10T428/13; Y10T428/1334; Y10T428/1345

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 97 words
A thermoplastic resin blend, which comprises; (A) about 30 to 70 weight percent of a high molecular weight polyethylene resin having a density of at least 0.95 gms/ml and a fractional melt index of from 0.05-0.8. (B) about 20 to 40 weight percent of a linear low density polyethylene resin having a density of 0.91 to 0.93 gms/ml and a melt index of less than 2.0; and (C) about 10 to 30 weight percent of a very low density polyethylene resin having a density of less than 0.91 gms/ml and a melt index of 0.8 to 1.1.
Claim 2
Dependent Claim 97 words
A thermoplastic resin blend, which comprises; (A) about 30 to 70 weight percent of a high molecular weight polyethylene resin having a density of at least 0.95 gms/ml and a fractional melt index of from 0.05-0.8. (B) about 20 to 40 weight percent of a linear low density polyethylene resin having a density of 0.91 to 0.93 gms/ml and a melt index of less than 2.0; and (C) about 10 to 30 weight percent of a very low density polyethylene resin having a density of less than 0.91 gms/ml and a melt index of 0.8 to 1.1.
Claim 3
Dependent Claim 41 words
The blend of claim 1 wherein there is about 50 weight percent of the high molecular weight polyethylene resin, about 30 weight percent of the linear low density polyethylene resin and about 20 weight percent of very low density polyethylene resin.
Claim 4
Dependent Claim 40 words
The blend of claim 1 wherein there is about 50 weight percent of the high molecular weight polyethylene resin, about 40 percent of the linear low density polyethylene resin, and about 10 percent of the very low density polyethylene resin.
Claim 5
Dependent Claim 11 words
A thermoplastically extruded film of the resin blend of claim 1.
Claim 6
Dependent Claim 10 words
A bag-type container fabricated from the blend of claim 1.

References Cited (Backward Citations)

US3998914A Cited
US4303710A Cited
US4330639A Cited
US4335224A Cited
EP0052555A2 Cited
US4346834A Cited
JPS5859242A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-09-13 1992-03-14 1992-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-09-13 1996-03-14 1996-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-09-13 2000-03-14 2000-09-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag