Abstract An open-topped casting mold and a matching mold are hingedly connected and are electrostatically coated with a powder screen; casting material is then poured into the molds without disturbing the powder by holding the powder in position with static electricity. The molds are pivoted together to provide a composite body of the hardened casting material formed by the bonding of the material from the two molds.
Inventors
- 👤 Gerard H. Viel
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 12:19
CPC Classifications
B; B29; B29C; B29C69/00; B29C69/004; B29C37/00; B29C37/0067; B29C37/0025; B29C37/0028; B29C39/00; B29C39/02; B29C41/00; B29C41/006; B29K; B29K2105/00; B29K2105/0088; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1002; Y10T156/1051
Claims Analysis
Total Claims: 24
Claim 1
Independent Claim
137 words
A method for packaging a permanent adhesive composition in a mold having an interior surface, said method comprising the steps of: providing an open top casting mold; providing by electrostatic coating a screen of powdery material over the entire surface of the mold; casting the composition in the mold to form a block, the electrostatic coating being such as to maintain the coherence of the screen during casting; cooling the cast block to cause that part of the screen adjacent the block to become part of the block, whereby a packaged article is formed in which all of the surfaces opposite the interior surface of the mold are protected by the screen and the surface corresponding to the open top of the mold is unprotected; protecting the unprotected surface; and removing the packaged article from the mold.
Claim 2
Independent Claim
137 words
A method for packaging a permanent adhesive composition in a mold having an interior surface, said method comprising the steps of: providing an open top casting mold; providing by electrostatic coating a screen of powdery material over the entire surface of the mold; casting the composition in the mold to form a block, the electrostatic coating being such as to maintain the coherence of the screen during casting; cooling the cast block to cause that part of the screen adjacent the block to become part of the block, whereby a packaged article is formed in which all of the surfaces opposite the interior surface of the mold are protected by the screen and the surface corresponding to the open top of the mold is unprotected; protecting the unprotected surface; and removing the packaged article from the mold.
Claim 3
Dependent Claim
164 words
The method of claim 1, wherein the mold comprises two symmetric parts, each having a chamber with an interior surface and joined one to the other around a common axis; wherein in said screen-providing step, the screen is provided electrostatically over the entirety of the interior surface of each part; wherein in said casting step, the adhesive composition is poured into the chamber of each part until it forms an even surface level with the highest part of each chamber to form a half-block, the screen being held coherent with the walls of the chambers throughout the entire casting process by means of static electricity; wherein in said cooling step, the half-blocks are cooled in their respective chambers; and wherein said protecting step comprises bringing together the two parts of the mold until the two unprotected surfaces of the half-blocks meet, whereby the two half-blocks are adhered one to the other, and a packaged article entirely coated in grains is produced from the mold.
Claim 4
Dependent Claim
155 words
The method of claim 1, wherein the mold is formed of several cells each having an interior surface; wherein in said screen-providing step, a screen is provided over the entirety of the interior surface of each cell; wherein in said casting step, the adhesive composition is poured until it reaches a level even with the highest point of each cell to form a half-block, the screen being held coherent with the walls of the cells throughout the entire casting process by means of static electricity; wherein in said cooling step, the half-blocks contained in the cells are cooled; and wherein said protecting step comprises placing opposite the mold another identical mold, in which the cells are filled with identically cast half-blocks, bringing together the unprotected surfaces of the half-blocks, and pressing the two molds to adhere with all the half-blocks facing each other, whereby packaged articles entirely coated with grains are produced from the molds.
Claim 5
Dependent Claim
32 words
The method of claim 2, further comprising the step of superficially reactivating the unprotected surfaces in order to partially change the unprotected surfaces of the cast material, prior to said bringing-together step.
Claim 6
Dependent Claim
32 words
The method of claim 3, further comprising the step of superficially reacting the unprotected surfaces in order to partially change the unprotected surfaces of the cast material, prior to said bringing-together step.
Claim 7
Dependent Claim
48 words
The method of claim 1, wherein said protecting step comprises sprinkling the unprotected surface of the packaged article with grains of a powdery material identical to that provided as a screen between the interior surface of the mold and the surfaces opposite the package article to protect it.
Claim 8
Dependent Claim
48 words
The method of claim 1, wherein said protecting step comprises sprinkling the unprotected surface of the packaged article with grains of a powdery material different from that provided as a screen between the interior surface of the mold and the surface opposite the packaged article to protect it.
Claim 9
Dependent Claim
25 words
The method of claim 1, wherein said protecting step comprises coating the unprotected surface of the block with a fatty liquid material to protect it.
Claim 10
Dependent Claim
23 words
The method of claim 1, wherein in said screen-providing step, the screen is obtained by superimposing several layers of grains of powdery material.
Claim 11
Dependent Claim
40 words
The method of claim 1, wherein in said screen-providing step, the powdery material comprises the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the formulation is complete.
Claim 12
Dependent Claim
40 words
The method of claim 6, wherein in said screen-providing step, the powdery material comprises the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the formulation is complete.
Claim 13
Dependent Claim
40 words
The method of claim 7, wherein in said screen-providing step, the powdery material comprises the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the formulation is complete.
Claim 14
Dependent Claim
40 words
The method of claim 9, wherein in said screen-providing step, the powdery material comprises the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the formulation is complete.
Claim 15
Dependent Claim
63 words
The method of claim 1, wherein in said screen-providing step, the powdery material comprises an insufficient but perfectly defined part of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the quantity of powdery material can be brought up to the ideal percentage when all the other constituents of the formulation are subsequently added.
Claim 16
Dependent Claim
63 words
The method of claim 6, wherein in said screen-providing step, the powdery material comprises an insufficient but perfectly defined part of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the quantity of powdery material can be brought up to the ideal percentage when all the other constituents of the formulation are subsequently added.
Claim 17
Dependent Claim
63 words
The method of claim 7, wherein in said screen-providing step, the powdery material comprises an insufficient but perfectly defined part of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the quantity of powdery material can be brought up to the ideal percentage when all the other constituents of the formulation are subsequently added.
Claim 18
Dependent Claim
63 words
The method of claim 9, wherein in said screen-providing step, the powdery material comprises an insufficient but perfectly defined part of at least one of the constituents of the formulation for which the permanent adhesive composition is intended, whereby the quantity of powdery material can be brought up to the ideal percentage when all the other constituents of the formulation are subsequently added.
Claim 19
Dependent Claim
38 words
The method of claim 1, wherein in said screen-providing step, the powdery material comprises in excess of the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended.
Claim 20
Dependent Claim
38 words
The method of claim 6, wherein in said screen-providing step, the powdery material comprises in excess of the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended.
Claim 21
Dependent Claim
38 words
The method of claim 7, wherein in said screen-providing step, the powdery material comprises in excess of the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended.
Claim 22
Dependent Claim
38 words
The method of claim 9, wherein in said screen-providing step, the powdery material comprises in excess of the full amount of at least one of the constituents of the formulation for which the permanent adhesive composition is intended.
Claim 23
Independent Claim
174 words
A method for packaging a permanent adhesive composition in a mold having two unsymmetrical parts, namely a base forming a chamber having an interior surface and an open top and a lid, said method comprising the steps of: providing a coherent screen of powdery material over the entire interior surface of the chamber and over the entire interior surface of the lid by an electrostatic coating process; casting permanent adhesive composition in the chamber to form a block, while maintaining the coherent nature of the screen during casting; positioning the lid over the chamber to close the chamber while maintaining the coherent screen of powdery material formed over the interior surface of the said lid; cooling the block to cause that part of the screen adjacent the block to become part of the said block, whereby a packaged article is formed in which all of the surfaces opposite the interior surface of the chamber and of the lid are protected by the screen; opening the lid; and removing the packaged article from the mold.
Claim 24
Independent Claim
174 words
A method for packaging a permanent adhesive composition in a mold having two unsymmetrical parts, namely a base forming a chamber having an interior surface and an open top and a lid, said method comprising the steps of: providing a coherent screen of powdery material over the entire interior surface of the chamber and over the entire interior surface of the lid by an electrostatic coating process; casting permanent adhesive composition in the chamber to form a block, while maintaining the coherent nature of the screen during casting; positioning the lid over the chamber to close the chamber while maintaining the coherent screen of powdery material formed over the interior surface of the said lid; cooling the block to cause that part of the screen adjacent the block to become part of the said block, whereby a packaged article is formed in which all of the surfaces opposite the interior surface of the chamber and of the lid are protected by the screen; opening the lid; and removing the packaged article from the mold.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-07-05 | 1992-01-04 | 1992-07-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-07-05 | 1996-01-04 | 1996-07-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-07-05 | 2000-01-04 | 2000-07-05 | $7700.00 | Window Closed / Lapsed |