← Back to Patent Explorer
US4748070A Expired / Lapsed US ⏱️ 0.0 years remaining

Film/fiber laminates

Assignee: Hercules LLC
•
Filing: 1986-03-24
•
Granted: 1988-05-31
•
Expires: 2006-03-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Tear strength of biaxially oriented polypropylene film is increased by laminating thereto a fibrous web of polypropylene fiber under conditions whereby the orientation of the film is retained.

Inventors

  • 👤 David C. Beehler

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 16:17
CPC Classifications
B; B32; B32B; B32B27/00; B32B27/12; B32B27/32; B32B5/00; B32B5/02; B32B5/022; B32B2262/00; B32B2262/02; B32B2262/0253; B32B2305/00; B32B2305/38; B32B2307/00; B32B2307/50; B32B2307/514; B32B2307/518; B32B2307/582; B32B2307/5825; B32B2307/70; B32B2307/724; B32B2307/7242; B32B2307/7246; B32B2323/00; B32B2323/10; B32B2439/00; B32B2439/70; Y; Y10; Y10S; Y10S428/00; Y10S428/91; Y10T; Y10T428/00; Y10T428/24; Y10T428/24802; Y10T428/24826; Y10T428/27; Y10T428/31504; Y10T428/31855; Y10T428/31909; Y10T428/31913; Y10T442/00; Y10T442/60; Y10T442/674; Y10T442/678

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 70 words
A high tear strength film comprised of a base film of biaxially oriented polypropylene having on one of its surfaces a layer of a lower melting polymer and, thermally bonded to said lower melting polymer layer, and coextensive with the biaxially oriented film, a fibrous polypropylene web, said web being bonded to the lower melting polymer layer in about 10 to 50% of the total surface area of the web.
Claim 2
Dependent Claim 70 words
A high tear strength film comprised of a base film of biaxially oriented polypropylene having on one of its surfaces a layer of a lower melting polymer and, thermally bonded to said lower melting polymer layer, and coextensive with the biaxially oriented film, a fibrous polypropylene web, said web being bonded to the lower melting polymer layer in about 10 to 50% of the total surface area of the web.
Claim 3
Dependent Claim 24 words
The high tear strength film of claim 1 wherein the fibrous web has a weight of about 10 to 40 grams per square yard.
Claim 4
Dependent Claim 17 words
The high tear strength film of claim 2 wherein the fibrous web is a nonwoven polypropylene fabric.
Claim 5
Dependent Claim 19 words
The high tear strength film of claim 2 wherein the fibrous web is a polypropylene bonded staple fiber scrim.

References Cited (Backward Citations)

US4035543A Cited
US4181550A Cited
US4288499A Cited
US4348444A Cited
EP0086057A2 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-05-31 1991-11-30 1992-05-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-05-31 1995-11-30 1996-05-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-05-31 1999-11-30 2000-05-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag