Method and apparatus for repairing metal in an article
Assignee: General Electric Co
•
Filing: 1984-10-01
•
Granted: 1988-05-10
•
Expires: 2004-10-01
Abstract
Abstract In the repair of a metallic article portion, a metal powder and laser beam are applied concurrently, the laser beam being applied in a power density range of 10 4 to 10 6 watts per square centimeter at an interaction time between the laser and the article and powder of 0.005-2 seconds to generate a repair layer. Apparatus for delivering a consistent, continuous flow of powder comprises the combination of an enclosed powder reservoir including means to introduce a gas under pressure, a mechanical means to feed powder into a conduit, a conduit vibrating means, and a fluid-cooled powder delivery nozzle.
Inventors
- 👤 Paul P. Mehta
- 👤 Robert R. Otten
- 👤 Ernest B. Cooper, Jr.
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-25 11:04
CPC Classifications
B; B05; B05B; B05B7/00; B05B7/14; B05B7/1404; B05B7/144; B05B7/1445; B05B7/1463; B05B7/16; B05B7/166; B05B7/22; B05B7/228; B23; B23K; B23K26/00; B23K26/20; B23K26/32; B23K26/34; B23K35/00; B23K35/02; B23K35/0222; B23K35/0244; B23P; B23P6/00; B23P6/002; B23P6/007; F; F01; F01D; F01D5/00; F01D5/005; B23K2103/00; B23K2103/50
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
167 words
In a method for repairing an article having an article portion of a metallic material, the steps of: concurrently applying to the article portion a laser beam and a powder comprising metal powder; the metal powder being of a composition substantially the same as the metallic material of the article portion; the laser being applied, at a laser beam spot, to the powder and the article portion beneath the powder in a power density range of 10 4 to 10 6 watts per square centimeter to melt both the metal powder and material of the article portion to generate a molten interaction zone from the metal powder and the metallic material of the article portion, while maintaining an interaction time in the range of 0.005-2 seconds between the beam and the powder and article portion beneath the powder thereby reducing the heat affected zone in the article portion and providing a repair layer on the article portion consolidated from the powder and metallic material of the portion.
Claim 2
Dependent Claim
167 words
In a method for repairing an article having an article portion of a metallic material, the steps of: concurrently applying to the article portion a laser beam and a powder comprising metal powder; the metal powder being of a composition substantially the same as the metallic material of the article portion; the laser being applied, at a laser beam spot, to the powder and the article portion beneath the powder in a power density range of 10 4 to 10 6 watts per square centimeter to melt both the metal powder and material of the article portion to generate a molten interaction zone from the metal powder and the metallic material of the article portion, while maintaining an interaction time in the range of 0.005-2 seconds between the beam and the powder and article portion beneath the powder thereby reducing the heat affected zone in the article portion and providing a repair layer on the article portion consolidated from the powder and metallic material of the portion.
Claim 3
Dependent Claim
54 words
The method of claim 1 in which relative lateral movement is provided between the laser beam spot and the article portion between the laser beam spot and the article portion to cooperate with the power density in maintaining the interaction time and to enable progressive movement, cooling and resolidification of the molten interaction zone.
Claim 4
Dependent Claim
16 words
The method of claim 1 in which the laser beam is of a continuous wave type.
Claim 5
Dependent Claim
43 words
The method of claim 1 wherein: the powder is applied at a rate in the range of about 1-30 grams per minute; and the laser is applied with a beam spot size at the article portion in the range of about 0.005-0.2 inches.
Claim 6
Dependent Claim
46 words
The method of claim 1 for repairing an article having an article portion of a metallic material, the portion including an edge of the article, wherein the laser is applied with the central axis of the beam spot being away from the edge of the article.
Claim 7
Dependent Claim
16 words
The method of claim 1 in which the powder is provided in a substantially moisture-free condition.
Claim 8
Dependent Claim
23 words
The method of claim 6 in which the powder is heated to remove moisture prior to applying the powder to the article portion.
Claim 9
Dependent Claim
39 words
The method of claim 1 wherein the sequence of steps is repeated to provide a plurality of superimposed, bonded-together repair layers using the preceding repair layer as the article portion for the concurrent application of powder and laser beam.
References Cited (Backward Citations)
US3819901A
Cited
US4015100A
Cited
US3952180A
Cited
US4122240A
Cited
JPS53112595A
Cited
US4269868A
Cited
US4300474A
Cited
US4323756A
Cited
US4299860A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-05-10 | 1991-11-09 | 1992-05-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-05-10 | 1995-11-09 | 1996-05-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-05-10 | 1999-11-09 | 2000-05-10 | $7700.00 | Window Closed / Lapsed |