← Back to Patent Explorer
US4724357A Expired / Lapsed US ⏱️ 0.0 years remaining

Image intensifier tube with reduced veiling glare and method of making same

Assignee: ITT ELECTRO OPTICAL PRODUCTS A DIVISION OF ITT Corp
•
Filing: 1986-08-22
•
Granted: 1988-02-09
•
Expires: 2006-08-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An image intensifier tube and a method of making same are disclosed wherein veiling glare caused by the amplification of off axis light is reduced. Included is a non-reflective, near infrared light absorbing first layer formed on the face plate of the tube adjacent any surface at which off-axis light could otherwise be reflected to the photoemissive device associated with the face plate and an electronically conductive second layer formed on top of the first layer. Such coatings are preferably formed by sputter deposition.

Inventors

  • 👤 Monte J. Drinkwine

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 11:32
CPC Classifications
H; H01; H01J; H01J29/00; H01J29/86; H01J29/89; H01J2229/00; H01J2229/89; H01J2229/8913

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 183 words
An image intensifier tube comprising: a face plate formed of optical material having light receiving and light transmitting surfaces; photoemissive means on said light transmitting surface of emitting electrons in response to light received at said photoemissive means from said light transmitting surface; a micro-channel plate positioned adjacent said photoemissive means for amplifying the electrons emitted from said photoemissive means; a sputtered metal oxide coating overlying a portion of said light transmitting surface adjoining said photoemissive means, and sputtered metal oxide coating being non-reflective and light absorbing at least in the near infrared region of light; a sputtered metal coating overlying said sputtered metal oxide coating and in contact with said photoemissive means; and a transition layer formed intermediate said sputtered metal oxide coating and said sputtered metal coating, said metal oxide coating taking the form of a reactively sputtered layer of metal, said sputtered metal coating taking the form of a sputtered layer of metal and said transition layer being formed by a gradual withdrawing of reactant upon a formation of said sputtered metal oxide coating to form said sputtered metal coating.
Claim 2
Dependent Claim 183 words
An image intensifier tube comprising: a face plate formed of optical material having light receiving and light transmitting surfaces; photoemissive means on said light transmitting surface of emitting electrons in response to light received at said photoemissive means from said light transmitting surface; a micro-channel plate positioned adjacent said photoemissive means for amplifying the electrons emitted from said photoemissive means; a sputtered metal oxide coating overlying a portion of said light transmitting surface adjoining said photoemissive means, and sputtered metal oxide coating being non-reflective and light absorbing at least in the near infrared region of light; a sputtered metal coating overlying said sputtered metal oxide coating and in contact with said photoemissive means; and a transition layer formed intermediate said sputtered metal oxide coating and said sputtered metal coating, said metal oxide coating taking the form of a reactively sputtered layer of metal, said sputtered metal coating taking the form of a sputtered layer of metal and said transition layer being formed by a gradual withdrawing of reactant upon a formation of said sputtered metal oxide coating to form said sputtered metal coating.
Claim 3
Dependent Claim 23 words
The image intensifier tube according to claim 1 wherein said sputtered metal oxide coating and said sputtered metal coating comprise the same metal.
Claim 4
Dependent Claim 13 words
The image intensifier tube according to claim 2 wherein said metal is chromium.
Claim 5
Dependent Claim 22 words
The image intensifier tube according to claim 1 wherein said sputtered metal oxide coating takes the form of a reactively sputtered layer.

References Cited (Backward Citations)

GB1067186A Cited
GB1582652A Cited
US4295073A Cited
GB2055244A Cited
GB2091482A Cited
GB2122808A Cited
US4475059A Cited
GB2148047A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-02-08 1991-08-10 1992-02-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-02-08 1995-08-10 1996-02-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-02-08 1999-08-10 2000-02-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag