← Back to Patent Explorer
US4724134A Expired / Lapsed US ⏱️ 0.0 years remaining

Production of tailor-made particle size distributions of substantially spherical metal hydroxide/oxide particles comprising single or multiple hydroxides by hydrolysis of one or more metal alkoxide aerosols

Assignee: Alcoa Corp
•
Filing: 1985-10-21
•
Granted: 1988-02-09
•
Expires: 2005-10-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The invention comprises high purity substantially spherical metal oxide particles having one or more predominant particle sizes formed from one or more metal alkoxides. In one embodiment there is disclosed multimodal particle size distributions of such substantially spherical metal hydroxide particles while a second embodiment describes the formation of such particles using more than one metal alkoxide to form either a mixed metal hydroxide particle or a layered particle comprising a core of a first metal hydroxide and at least one layer of an additional metal hydroxide.

Inventors

  • 👤 Ajay Sood

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 23:36
CPC Classifications
C; C01; C01F; C01F7/00; C01F7/02; C01F7/34; C01F7/36; C01B; C01B13/00; C01B13/14; C01B13/20; C01B13/32; C01B13/34; C01P; C01P2004/00; C01P2004/30; C01P2004/32; C01P2006/00; C01P2006/80

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 145 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two predominant particle sizes which comprises: (a) forming a metal alkoxide vapor from a first metal alkoxide in a first vaporization zone; (b) cooling the metal alkoxide vapor sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; (c) hydrolyzing said metal alkoxide aerosol, while maintaining said aerosol under a turbulent flow condition, in a hydrolysis zone by contact with water vapor to hydrolyze said metal alkoxide to form substantially spherical metal hydroxide particles of a first particle size, and (d) contacting said water vapor in said hydrolysis zone with a second alkoxide metal vapor, to form at least one additional distinct and different particle size of said substantially spherical metal hydroxide particles from the particle size produced in step (c).
Claim 2
Dependent Claim 145 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two predominant particle sizes which comprises: (a) forming a metal alkoxide vapor from a first metal alkoxide in a first vaporization zone; (b) cooling the metal alkoxide vapor sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; (c) hydrolyzing said metal alkoxide aerosol, while maintaining said aerosol under a turbulent flow condition, in a hydrolysis zone by contact with water vapor to hydrolyze said metal alkoxide to form substantially spherical metal hydroxide particles of a first particle size, and (d) contacting said water vapor in said hydrolysis zone with a second alkoxide metal vapor, to form at least one additional distinct and different particle size of said substantially spherical metal hydroxide particles from the particle size produced in step (c).
Claim 3
Dependent Claim 27 words
The process of claim 1 including the further step of forming said second alkoxide vapor by vaporizing liquid alkoxide which accumulates in the bottom of a hydrolyzer.
Claim 4
Dependent Claim 25 words
The process of claim 1 including the further steps of forming said second alkoxide vapor by introducing alkoxide liquid into the bottom of a hydrolyzer.
Claim 5
Dependent Claim 20 words
The process of claim 1 including the further steps of forming said second alkoxide vapor in a separate vaporization zone.
Claim 6
Dependent Claim 24 words
The process of claim 1 wherein said second alkoxide vapor comprises the metal alkoxide vapor which has not been condensed in said condensation zone.
Claim 7
Dependent Claim 133 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two different and distinct metal hydroxide particles which comprises: (a) forming a first metal alkoxide vapor from a first metal alkoxide liquid in a first vaporization zone; (b) forming at least one additional metal alkoxide vapor from a different metal alkoxide liquid in a vaporizaton zone; (c) cooling one of said metal alkoxide vapors sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; and (d) hydrolyzing both said metal alkoxide vapor and said aerosol in a hydrolysis zone by contact with water vapor to form said mixture of substantially spherical metal hydroxide particles of two different and distinct size, said mixture containing a plurality of different metal hydroxides.
Claim 8
Dependent Claim 133 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two different and distinct metal hydroxide particles which comprises: (a) forming a first metal alkoxide vapor from a first metal alkoxide liquid in a first vaporization zone; (b) forming at least one additional metal alkoxide vapor from a different metal alkoxide liquid in a vaporizaton zone; (c) cooling one of said metal alkoxide vapors sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; and (d) hydrolyzing both said metal alkoxide vapor and said aerosol in a hydrolysis zone by contact with water vapor to form said mixture of substantially spherical metal hydroxide particles of two different and distinct size, said mixture containing a plurality of different metal hydroxides.
Claim 9
Dependent Claim 141 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two different and distinct metal hydroxide particles which comprises: (a) forming a first metal alkoxide vapor from a first metal alkoxide liquid in a first vaporization zone; (b) forming at least one additional metal alkoxide vapor from a different metal alkoxide liquid in a vaporization zone; (c) mixing said one additional metal alkoxide vapor with said first metal alkoxide vapor; (d) cooling said mixed metal alkoxide vapors sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; and (e) hydrolyzing said aerosol in a hydrolysis zone by contact with water vapor to form said mixture of substantially spherical metal hydroxide particles of two different and distinct sizes, and said mixture containing a plurality of different metal hydroxides.
Claim 10
Dependent Claim 141 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two different and distinct metal hydroxide particles which comprises: (a) forming a first metal alkoxide vapor from a first metal alkoxide liquid in a first vaporization zone; (b) forming at least one additional metal alkoxide vapor from a different metal alkoxide liquid in a vaporization zone; (c) mixing said one additional metal alkoxide vapor with said first metal alkoxide vapor; (d) cooling said mixed metal alkoxide vapors sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; and (e) hydrolyzing said aerosol in a hydrolysis zone by contact with water vapor to form said mixture of substantially spherical metal hydroxide particles of two different and distinct sizes, and said mixture containing a plurality of different metal hydroxides.
Claim 11
Dependent Claim 110 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two different and distinct metal hydroxide particles which comprises: (a) mixing two different metal alkoxide liquids; (b) forming a metal alkoxide vapor from said mixed metal alkoxide liquids in a vaporization zone; (c) cooling said metal alkoxide vapor sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; and (d) hydrolyzing said aerosol in a hydrolysis zone by contact with water vapor to for said mixture of substantially spherical metal hydroxide particles of two different and distinct sizes, said mixture containing plurality of different metal hydroxides.
Claim 12
Dependent Claim 110 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a mixture of at least two different and distinct metal hydroxide particles which comprises: (a) mixing two different metal alkoxide liquids; (b) forming a metal alkoxide vapor from said mixed metal alkoxide liquids in a vaporization zone; (c) cooling said metal alkoxide vapor sufficiently in a condensation zone to form an aerosol comprising finely divided condensed metal alkoxide; and (d) hydrolyzing said aerosol in a hydrolysis zone by contact with water vapor to for said mixture of substantially spherical metal hydroxide particles of two different and distinct sizes, said mixture containing plurality of different metal hydroxides.
Claim 13
Dependent Claim 212 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a core of a first metal hydroxide and at least one layer of a different metal hydroxide surrounding said core which comprises: (a) forming a first metal alkoxide vapor in a first vaporization zone; (b) cooling said first metal alkoxide vapor sufficiently in a condensation zone to form a first aerosol comprising finely divided condensed metal alkoxide; (c) hydrolyzing said first metal alkoxide aerosol in a hydrolysis zone by contact with water vapor to hydrolyze said metal alkoxide to form a substantially spherical metal hydroxide particles; (d) forming a second metal alkoxide vapor in a second vaporization zone; (e) mixing said second metal alkoxide vapor with said substantially spherical metal hydroxide particles formed from said first aerosol and cooling the formed mixture to form a second aerosol comprising substantially spherical metal hydroxide particles formed from said first aerosol and condensed metal alkoxide from said second metal alkoxide vapor; and (f) hydrolyzing said second metal alkoxide aerosol in a hydrolysis zone by contact with water vapor to hydrolyze said second metal alkoxide; whereby substantially spherical metal hydroxide particles are formed comprising said core containing said first metal hydroxide and a layer of a second metal hydroxide surrounding said core.
Claim 14
Dependent Claim 212 words
A process for the production of high purity substantially spherical metal hydroxide particles comprising a core of a first metal hydroxide and at least one layer of a different metal hydroxide surrounding said core which comprises: (a) forming a first metal alkoxide vapor in a first vaporization zone; (b) cooling said first metal alkoxide vapor sufficiently in a condensation zone to form a first aerosol comprising finely divided condensed metal alkoxide; (c) hydrolyzing said first metal alkoxide aerosol in a hydrolysis zone by contact with water vapor to hydrolyze said metal alkoxide to form a substantially spherical metal hydroxide particles; (d) forming a second metal alkoxide vapor in a second vaporization zone; (e) mixing said second metal alkoxide vapor with said substantially spherical metal hydroxide particles formed from said first aerosol and cooling the formed mixture to form a second aerosol comprising substantially spherical metal hydroxide particles formed from said first aerosol and condensed metal alkoxide from said second metal alkoxide vapor; and (f) hydrolyzing said second metal alkoxide aerosol in a hydrolysis zone by contact with water vapor to hydrolyze said second metal alkoxide; whereby substantially spherical metal hydroxide particles are formed comprising said core containing said first metal hydroxide and a layer of a second metal hydroxide surrounding said core.

References Cited (Backward Citations)

US3403001A Cited
US3406012A Cited
US3647374A Cited
US3663283A Cited
US3914396A Cited
US4117106A Cited
US4241042A Cited
GB2070579A Cited
US4387085A Cited
US4532072A Cited
EP0117755A2 Cited
US4543341A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-02-08 1991-08-10 1992-02-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-02-08 1995-08-10 1996-02-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-02-08 1999-08-10 2000-02-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag