Abstract

Abstract A method of manufacturing thermal barrier structures comprising at least three dimpled cores separated by flat plate material with the outer surface of the flat plate material joined together by diffusion bonding.

Inventors

  • 👤 Winford Blair

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 08:12
CPC Classifications
B; B23; B23K; B23K20/00; B23K20/16; B32; B32B; B32B3/00; B32B3/26; B32B3/30; B32B15/00; B32B15/04; B32B15/043; B32B3/28; B32B2255/00; B32B2255/06; B32B2255/20; B32B2255/205; B32B2307/00; B32B2307/30; B32B2307/304; B32B2605/00; B32B2605/18; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/1234; Y10T428/12347

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 315 words
A method of manufacturing a lightweight metallic structure having stacked dimpled core structures with nodes each having a flat surface projecting in opposite directions from a midplane and flat material sandwiched between each of the stacked dimpled core structures and on the outer surface of the outer most stacked dimpled core structure for forming an end surface thereto, said dimpled core structure and flat plate material comprising thin metallic foil material, with the foil thickness of some of the dimpled core structures and flat plate material being thinner than the others comprising the steps of: selecting component material of a selected size; providing plating material between at least the node and flat plate connecting surface; securing together the stacked components; positioning the nodes of the dimpled core material in substantially vertical alignment during the securing together of the components; placing the secured together components on a reference surface; arranging the secured together components to a predetermined height and subjecting said components to a predetermined pressure against the reference surface, said predetermined pressure and height are provided by rigid tools and dead weight means, wherein said rigid tools surround the components of said lightweight metallic structure and extend to a height less than the height of the stacked components and said dead weight means forces said components downward to a vertical height equal to the height of said rigid tools; placing the secured together components and reference surface in a vacuum furnace; and elevating the temperature within the furnace and maintaining that elevated temperature sufficiently long to cause a eutectic melt of the plating materials and diffuse the plating materials into the base material of the adjacent components creating a diffusion bond between the node flat surface and adjacent flat plate material while maintaining the predetermined height and predetermined pressure to prevent crushing of the dimpled core material during the eutectic melting and diffusion bonding sequence.
Claim 2
Independent Claim 315 words
A method of manufacturing a lightweight metallic structure having stacked dimpled core structures with nodes each having a flat surface projecting in opposite directions from a midplane and flat material sandwiched between each of the stacked dimpled core structures and on the outer surface of the outer most stacked dimpled core structure for forming an end surface thereto, said dimpled core structure and flat plate material comprising thin metallic foil material, with the foil thickness of some of the dimpled core structures and flat plate material being thinner than the others comprising the steps of: selecting component material of a selected size; providing plating material between at least the node and flat plate connecting surface; securing together the stacked components; positioning the nodes of the dimpled core material in substantially vertical alignment during the securing together of the components; placing the secured together components on a reference surface; arranging the secured together components to a predetermined height and subjecting said components to a predetermined pressure against the reference surface, said predetermined pressure and height are provided by rigid tools and dead weight means, wherein said rigid tools surround the components of said lightweight metallic structure and extend to a height less than the height of the stacked components and said dead weight means forces said components downward to a vertical height equal to the height of said rigid tools; placing the secured together components and reference surface in a vacuum furnace; and elevating the temperature within the furnace and maintaining that elevated temperature sufficiently long to cause a eutectic melt of the plating materials and diffuse the plating materials into the base material of the adjacent components creating a diffusion bond between the node flat surface and adjacent flat plate material while maintaining the predetermined height and predetermined pressure to prevent crushing of the dimpled core material during the eutectic melting and diffusion bonding sequence.
Claim 3
Dependent Claim 19 words
The method as defined in claim 1, wherein said plating material is first applied to the flat node surface.
Claim 4
Dependent Claim 18 words
The method of claim 1, wherein the plating material comprises sequentially applying layers of nickel, copper and silver.
Claim 5
Dependent Claim 16 words
The method of claim 2, wherein the layers of plating materials are substantially equal by weight.
Claim 6
Dependent Claim 19 words
The method of claim 3, wherein each layer of plating is from 22/3 to 31/2 grams per square foot.
Claim 7
Dependent Claim 17 words
The method of claim 3, wherein each layer of plating is substantially 3 grams per square foot.
Claim 8
Dependent Claim 21 words
The method of claim 1, wherein the components are secured together by resistance welding together each adjacent component at select locations.
Claim 9
Dependent Claim 26 words
The method of claim 1, wherein the temperature within the furnace is elevated to approximately 940° C. and maintained at that temperature for approximately 90 minutes.
Claim 10
Dependent Claim 66 words
The method of claim 1, wherein said predetermined pressure and height are provided by rigid tools and dead weight means, wherein said rigid tools surround the components of said lightweight metallic structure and extend approximately 0.045 inches less than the height of the stacked components and said dead weight means forces said components downward to a vertical height equal to the height of said rigid tools.
Claim 11
Dependent Claim 70 words
The method of claim 1, wherein the dimpled core material is sized by: coating the entire surface of an unsized sheet of dimpled core material; scribing said sheet of dimpled core material to the desired dimension by burning away the resistant material with a laser beam; and emerging said scribed sheet of dimpled core material into a chem-mill solution, whereby the exposed material outside of the scribed area is removed.
Claim 12
Dependent Claim 11 words
Thermo-barrier material manufactured by the method of claims 1 or 9.

References Cited (Backward Citations)

US1228763A Cited
US1914207A Cited
US2481046A Cited
US3073268A Cited
US3151712A Cited
GB1438842A Cited
JPS5418232A Cited
US4205118A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-10-26 1991-04-27 1991-10-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-10-26 1995-04-27 1995-10-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-10-26 1999-04-27 1999-10-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag