US4702989A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for producing pressure-fixable electrophotographic toners
Assignee: Fujikura Kasei Co Ltd
•
Filing: 1986-04-07
•
Granted: 1987-10-27
•
Expires: 2006-04-07
Abstract
Abstract A pressure-fixable toner is produced by: dispersing or dissolving a mixture containing (a) a colorant and/or magnetic particles, (b) a pressure fixable binding material, and (c) a capsule wall-forming resin, in an organic solvent; dispersing the resulting dispersion or solution in a dispersion-stabilizing solution; heating the dispersion to evaporate off the solvent; dispersing the resulting encapsulated toner in a lower alcohol to remove the solvent remaining within the encapsulated toner; and thereafter drying the toner. The toner can be used to develop images in electrophotographic systems.
Inventors
- 👤 Norihide Sugiyama
- 👤 Katsuro Funato
- 👤 Hiroshi Nagase
- 👤 Seiichi Yamamoto
- 👤 Shigeo Miyamori
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 15:30
CPC Classifications
G; G03; G03G; G03G9/00; G03G9/08; G03G9/093; G03G9/09392; Y; Y10; Y10T; Y10T428/00; Y10T428/29; Y10T428/2982; Y10T428/2989
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
216 words
A process for producing a pressure-fixable toner which comprises the steps of: dispersing or dissolving a starting material mixture containing (a) a colorant and/or magnetic particles, (b) a pressure-fixable binding material selected from the group consisting of higher fatty acids, metallic salts of higher fatty acids, derivatives of higher fatty acids, amides of higher fatty acids, natural waxes, synthetic waves, rosin derivatives, polyolefins, olefin copolymers, silicone resins, alkyd resins, natural resin-modified phenol resins, maleic acid-modified phenol resins, phenol resins, rubber and styrene resins; and (c) a capsule wall-forming resin selected from the group consisting of homopolyumers of styrene or vinyl monomers, copolymers of styrene and vinyl monomers, and epoxy resins in an organic solvent; dispersing the resulting dispersion or solution in an aqueous dispersion-stabilizing solution; then gradually heating the thus-obtained dispersion up to the azeotropic temperature of the water-organic solvent to drive off the major portion of the organic solvent from the dispersed droplets and phase-separating the capsule wall-forming resin dissolved in the organic solvent on the surface of the dispersed toner droplets containing components (a) and (b) to form a capsule wall around the surface of the droplets; dispersing the resulting encapsulated toner in a lower alcohol to extract and remove the organic solvent remaining within the encapsulated toner; and thereafter drying the encapsulated toner.
Claim 2
Dependent Claim
216 words
A process for producing a pressure-fixable toner which comprises the steps of: dispersing or dissolving a starting material mixture containing (a) a colorant and/or magnetic particles, (b) a pressure-fixable binding material selected from the group consisting of higher fatty acids, metallic salts of higher fatty acids, derivatives of higher fatty acids, amides of higher fatty acids, natural waxes, synthetic waves, rosin derivatives, polyolefins, olefin copolymers, silicone resins, alkyd resins, natural resin-modified phenol resins, maleic acid-modified phenol resins, phenol resins, rubber and styrene resins; and (c) a capsule wall-forming resin selected from the group consisting of homopolyumers of styrene or vinyl monomers, copolymers of styrene and vinyl monomers, and epoxy resins in an organic solvent; dispersing the resulting dispersion or solution in an aqueous dispersion-stabilizing solution; then gradually heating the thus-obtained dispersion up to the azeotropic temperature of the water-organic solvent to drive off the major portion of the organic solvent from the dispersed droplets and phase-separating the capsule wall-forming resin dissolved in the organic solvent on the surface of the dispersed toner droplets containing components (a) and (b) to form a capsule wall around the surface of the droplets; dispersing the resulting encapsulated toner in a lower alcohol to extract and remove the organic solvent remaining within the encapsulated toner; and thereafter drying the encapsulated toner.
Claim 3
Dependent Claim
106 words
The process according to claim 1 wherein said pressure-fixable binding material comprises (a) from 100 to 40% by weight of a material selected from the group consisting of higher fatty acids, metallic salts of higher fatty acids, derivatives of higher fatty acids, amides of higher fatty acids, natural waxes, synthetic waxes, rosin derivatives polyolefins, olefin copolymers, silicone resins, alkyd resins, natural resin-modified phenol resins, maleic acid-modified phenol resins, phenol resins, rubbers and styrene resins, and (b) from 0 to 60% by weight of petroleum resins obtained by polymerizing unsaturated hydrocarbons comprising aliphatic olefin and/or diolefin which have been obtained in a pyrolysis process of petroleum naphtha.
Claim 4
Dependent Claim
30 words
The process according to claim 2 wherein said petroleum resins are obtained by polymerization of unsaturated C 5 hydrocarbons and have a softening point of from 65° to 110° C.
Claim 5
Dependent Claim
33 words
The process according to claim 1 wherein said capsule wall-forming resin is a resin obtained by polymerizing from 50 to 100 parts of styrene and from 0 to 50 parts of vinyl monomers.
Claim 6
Dependent Claim
18 words
The process according to claim 1 wherein said capsule wall-forming resin is a epoxy resin cured by amine.
Claim 7
Dependent Claim
12 words
The process according to claim 1 wherein said organic solvent is toluene.
Claim 8
Dependent Claim
24 words
The process according to claim 1 wherein said lower alcohol is a member selected from the group consisting of methanol, ethanol, and isopropyl alcohol.
Claim 9
Dependent Claim
22 words
The process according to claim 1 wherein a charge control agent is previously dissolved or dispersed in the lower alcohol as needed.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1990-10-26 | 1991-04-27 | 1991-10-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1994-10-26 | 1995-04-27 | 1995-10-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1998-10-26 | 1999-04-27 | 1999-10-27 | $7700.00 | Window Closed / Lapsed |