Abstract

Abstract A method of producing a light sensitive element wherein a substrate is coated with a photosensitive layer having a particular class of diazonium salts, a colorant and a polyvinyl acetal resin. Upon imagewise exposure it is developed with an aqueous composition of salts and surfactants in the absence of organic solvents.

Inventors

  • 👤 Shuchen Liu

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 01:02
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/26; G03F7/30; G03F7/32

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 478 words
A method for producing and using a photographic element which comprises coating a substrate with a light sensitive composition, which composition comprises in admixture: (i) from about 1% by weight to about 21% by weight, based on the total weight of the non-solvent parts of said light sensitive composition, of a polyvinyl acetal resin; and (ii) from about 1.1% by weight to about 22% by weight, based on the total weight of the non-solvent parts of said light sensitive composition, of a colorant; and (iii) from about 63% by weight to about 92% by weight, based on the total weight of the non-solvent parts of said light sensitive composition, of a light-sensitive, water insoluble diazonium group-containing polycondensation product, which product is obtained first by condensation of (a) a diazonium salt corresponding to formula I ##STR2## wherein R 1 , R 2 and R 3 each denote separately a hydrogen atom, a halogen atom, an alkyl group having from 1 to 3 carbon atoms, or an alkoxy group having from 1 to 6 carbon atoms, and X denotes the anion of the diazonium salt; (b) with a compound corresponding to formula II R.sup.4 --O--CH.sub.2 --R.sup.5 (II) wherein R 4 denotes a hydrogen atom, an alkyl group or an aliphatic acyl radical and R 5 denotes a mononuclear or polynuclear aromatic radical, which is unsubstituted or substituted by a halogen atom, an alkyl group, a halogenated alkyl group, an alkoxy group having from 1 to 3 carbon atoms, a carboxy group, an aryl group, an arylmercapto group, or an aryloxy group, in a strongly acidic medium, and thereafter condensing with (c) a compound corresponding to formula III R.sup.6 --O--CH.sub.2 --R.sup.8 --CH.sub.2 --O--R.sup.7 (III) wherein R 6 and R 7 each denote separately a hydrogen atom, an alkyl group, or an aliphatic acyl radical, and R 8 denotes an aromatic hydrocarbon radical selected from the group consisting of a phenol, a phenolether, an aromatic thioether, an aromatic heterocyclic compound, and an organic acid amide, with the radicals resulting from compound II being directly linked to the units of the diazonium salt I; and thereafter imagewise exposing said coated substrate to actinic radiation and removing all or substantially all of the non-radiation-exposed areas with a non-organic solvent containing aqueous alkaline developer composition which consists essentially of in admixture: A. from about 80% by weight to about 95% by weight, based on the weight of said developer composition, water; and B. from about 7.7% by weight to about 17% by weight, based on the weight of said developer composition, of one or more salts selected from the group consisting of sodium, potassium, and ammonium hydroxides, silicates, phosphates, bicarbonates, oxalates, carbonates, sulfates, chlorides, acetates, benzoates, borates, citrates, salicylates, and pyrophosphates; and C. from about .3% by weight to about 3.0% by weight, based on the weight of said developer composition, of a anionic surfactant.
Claim 2
Independent Claim 478 words
A method for producing and using a photographic element which comprises coating a substrate with a light sensitive composition, which composition comprises in admixture: (i) from about 1% by weight to about 21% by weight, based on the total weight of the non-solvent parts of said light sensitive composition, of a polyvinyl acetal resin; and (ii) from about 1.1% by weight to about 22% by weight, based on the total weight of the non-solvent parts of said light sensitive composition, of a colorant; and (iii) from about 63% by weight to about 92% by weight, based on the total weight of the non-solvent parts of said light sensitive composition, of a light-sensitive, water insoluble diazonium group-containing polycondensation product, which product is obtained first by condensation of (a) a diazonium salt corresponding to formula I ##STR2## wherein R 1 , R 2 and R 3 each denote separately a hydrogen atom, a halogen atom, an alkyl group having from 1 to 3 carbon atoms, or an alkoxy group having from 1 to 6 carbon atoms, and X denotes the anion of the diazonium salt; (b) with a compound corresponding to formula II R.sup.4 --O--CH.sub.2 --R.sup.5 (II) wherein R 4 denotes a hydrogen atom, an alkyl group or an aliphatic acyl radical and R 5 denotes a mononuclear or polynuclear aromatic radical, which is unsubstituted or substituted by a halogen atom, an alkyl group, a halogenated alkyl group, an alkoxy group having from 1 to 3 carbon atoms, a carboxy group, an aryl group, an arylmercapto group, or an aryloxy group, in a strongly acidic medium, and thereafter condensing with (c) a compound corresponding to formula III R.sup.6 --O--CH.sub.2 --R.sup.8 --CH.sub.2 --O--R.sup.7 (III) wherein R 6 and R 7 each denote separately a hydrogen atom, an alkyl group, or an aliphatic acyl radical, and R 8 denotes an aromatic hydrocarbon radical selected from the group consisting of a phenol, a phenolether, an aromatic thioether, an aromatic heterocyclic compound, and an organic acid amide, with the radicals resulting from compound II being directly linked to the units of the diazonium salt I; and thereafter imagewise exposing said coated substrate to actinic radiation and removing all or substantially all of the non-radiation-exposed areas with a non-organic solvent containing aqueous alkaline developer composition which consists essentially of in admixture: A. from about 80% by weight to about 95% by weight, based on the weight of said developer composition, water; and B. from about 7.7% by weight to about 17% by weight, based on the weight of said developer composition, of one or more salts selected from the group consisting of sodium, potassium, and ammonium hydroxides, silicates, phosphates, bicarbonates, oxalates, carbonates, sulfates, chlorides, acetates, benzoates, borates, citrates, salicylates, and pyrophosphates; and C. from about .3% by weight to about 3.0% by weight, based on the weight of said developer composition, of a anionic surfactant.
Claim 3
Dependent Claim 14 words
The method of claim 1 wherein said substrate comprises aluminum or an aluminum alloy.
Claim 4
Dependent Claim 11 words
The method of claim 1 wherein said colorant is a pigment.
Claim 5
Dependent Claim 35 words
The method of claim 1 wherein said surfactant comprises one or more compounds selected from the group consisting of sodium octyl sulfate, sodium decyl sulfate, ammonium lauryl sulfate, sodium tetradecyl sulfate, and sodium lauryl sulfate.
Claim 6
Dependent Claim 13 words
The method of claim 1 wherein said surfactant component comprises sodium octyl sulfate.
Claim 7
Dependent Claim 28 words
The method of claim 1 wherein said light sensitive composition further comprises one or more components selected from the group consisting of acids, exposure indicators, plasticizers and surfactants.
Claim 8
Dependent Claim 24 words
The method of claim 1 wherein said polyvinyl acetal component is present in an amount of from about 2% to about 15% by weight.
Claim 9
Dependent Claim 23 words
The method of claim 1 wherein said diazo component is present in an amount of from about 68% to about 57% by weight.
Claim 10
Dependent Claim 22 words
The method of claim 1 wherein said colorant is present in an amount of from about 2.2% to about 16.5% by weight.
Claim 11
Dependent Claim 22 words
The method of claim 1 wherein said salt is present in an amount of from about 11.5% to about 13% by weight.
Claim 12
Dependent Claim 22 words
The method of claim 1 wherein said surfactant is present in an amount of from about 0.5% to about 2.0% by weight.
Claim 13
Dependent Claim 30 words
The method of claim 1 wherein R 4 , R 6 and R 7 each denote a hydrogen atom or an alkyl group having from 1 to 3 carbon atoms.
Claim 14
Dependent Claim 37 words
The method of claim 1 wherein R 8 comprises a radical having (a) one aromatic ring or (b) two aromatic rings which are linked by a single bond or by --O--, --NH--, --CH 2 --, or --S--.
Claim 15
Dependent Claim 34 words
The method of claim 1 produced by condensing 1 mole of diazonium salt (I) with from about 0.1 to 1.5 moles of compound II and from about 0.5 to 1.5 moles of compound III.
Claim 16
Dependent Claim 33 words
The method of claim 1, wherein said diazonium salt comprises a diphenylamine-4-diazonium salt which is unsubstituted or is substituted by an alkyl or an alkoxy group having from 1 to 3 carbon atoms.
Claim 17
Dependent Claim 19 words
The method of claim 15, wherein said diazonium salt comprises a diazonium compound derived from 4-amino-diphenylamine, 3-methyl-4-aminodiphenylamine, or 3-methoxy-4-amino-diphenylamine.

References Cited (Backward Citations)

US3396019A Cited
US3679419A Cited
GB1313777A Cited
US3669660A Cited
US4186006A Cited
US4391897A Cited
EP0051081A1 Cited
CA1172492A Cited
US4492748A Cited
EP0104537A2 Cited
EP0126875A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-09-07 1991-03-09 1991-09-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-09-07 1995-03-09 1995-09-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-09-07 1999-03-09 1999-09-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag