Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
182 words
A continuous method for the detection, recording and repair of defects and/or weak points of a hot semi-finished iron or steel product prior to hot rolling, the method comprising: (a) locating an oxygen supplied blow torch adjacent a surface of the hot semi-finished product so that an oxygen-supplied flame from the torch is at a predetermined angle relative to the plane of the surface of said product; (b) moving the product at a predetermined rate of speed relative to the flame; (c) applying the oxygen-supplied flame to the surface of said product, which causes (1) the iron or steel at said surface to melt, (2) the molten metal to be removed to expose the underlying iron or steel in the semifinished product, and (3) a visual indication of the defects and/or weak points to appear; (d) transmitting a visual image of said surface to a location remote from the torch; (e) reproducing said image at said remote location and recording the position of said defects and/or weak points; and (f) repairing the defects and/or weak points prior to hot rolling said product.
Claim 2
Dependent Claim
182 words
A continuous method for the detection, recording and repair of defects and/or weak points of a hot semi-finished iron or steel product prior to hot rolling, the method comprising: (a) locating an oxygen supplied blow torch adjacent a surface of the hot semi-finished product so that an oxygen-supplied flame from the torch is at a predetermined angle relative to the plane of the surface of said product; (b) moving the product at a predetermined rate of speed relative to the flame; (c) applying the oxygen-supplied flame to the surface of said product, which causes (1) the iron or steel at said surface to melt, (2) the molten metal to be removed to expose the underlying iron or steel in the semifinished product, and (3) a visual indication of the defects and/or weak points to appear; (d) transmitting a visual image of said surface to a location remote from the torch; (e) reproducing said image at said remote location and recording the position of said defects and/or weak points; and (f) repairing the defects and/or weak points prior to hot rolling said product.
Claim 3
Dependent Claim
29 words
Process as in claim 1, wherein the angle between the axis of the torch and the plane of the surface to be examined is between 5 and 15 degrees.
Claim 4
Dependent Claim
23 words
Process as in claim 1, wherein the speed of displacement of the application point of the torch is between 15 and 30 m/minute.
Claim 5
Dependent Claim
23 words
Process as in claim 1, wherein the application of the torch describes a line parallel to the lengthwise axis of the semifinished product.
Claim 6
Dependent Claim
26 words
Process as in claim 1, wherein the application point of the torch describes an oblique line in relation to the lengthwise axis of the semifinished product.
Claim 7
Dependent Claim
37 words
Process as in claim 1, wherein the application point of the torch by successive sequences describes a line which is parallel and a line which is oblique in relation to the lengthwise axis of the semifinished product.