Abstract

Abstract PCT No. PCT/JP83/00260 Sec. 371 Date Apr. 10, 1984 Sec. 102(e) Date Apr. 10, 1984 PCT Filed Aug. 10, 1983.In the manufacture of a magnetic head, a magnetic layer is sputtered or evaporated on a surface of a first substrate of glass or nonmagnetic material and a nonmagnetic material such as glass is sputtered on one end face of the composite body formed by the substrate and the magnetic layer to form a gap filling layer. A second substrate of the same material and thickness as the first is bonded thereto with the magnetic gap filling being interposed therebetween. Magnetic material is sputtered or evaporated on the bonded substrates until a predetermined thickness is reached to form a second magnetic layer. The magnetic layers are then lapped to reveal an edge of the gap filling layer between adjacent edges of the two magnetic layers. Since the gap filling layer is formed by sputtering method, magnetic gap length can be precisely determined and since the thickness of the magnetic layers determines the track width, a magnetic head having a narrow width can be easily manufactured.

Inventors

  • 👤 Hiroshi Sakakima

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 21:19
CPC Classifications
G; G11; G11B; G11B5/00; G11B5/127; G11B5/31; G11B5/3176; G11B5/3179; G11B5/3183; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/4902; Y10T29/49021; Y10T29/49032; Y10T29/49036; Y10T29/49043; Y10T29/49055; Y10T29/49067; Y10T29/49789; Y10T29/49796

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 123 words
A method for forming a magnetic gap, comprising: (a) sputtering a first magnetic layer on a first surface of a substrate; (b) sputtering a nonmagnetic layer on a second surface of the substrate perpendicular to the first surface so that the nonmagnetic layer contacts with an edge of said first magnetic layer; (c) aligning a third surface of another substrate with said first surface; (d) sputtering a second magnetic layer on an area including said third surface and an end face of said nonmagnetic layer; and (e) lapping a portion of said second magnetic layer until said first and second magnetic layers and said nonmagnetic layer present a common surface plane opposite to a plane defined by the aligned first and third surfaces.
Claim 2
Independent Claim 123 words
A method for forming a magnetic gap, comprising: (a) sputtering a first magnetic layer on a first surface of a substrate; (b) sputtering a nonmagnetic layer on a second surface of the substrate perpendicular to the first surface so that the nonmagnetic layer contacts with an edge of said first magnetic layer; (c) aligning a third surface of another substrate with said first surface; (d) sputtering a second magnetic layer on an area including said third surface and an end face of said nonmagnetic layer; and (e) lapping a portion of said second magnetic layer until said first and second magnetic layers and said nonmagnetic layer present a common surface plane opposite to a plane defined by the aligned first and third surfaces.
Claim 3
Independent Claim 162 words
A method of fabricating a magnetic head comprising: (a) sputtering a first magnetic layer on a surface of a first substrate whereby the magnetic layer and the substrate present a common end face perpendicular to said surface; (b) sputtering a nonmagnetic layer on said common end face; (c) bonding a second substrate end-to-end to said first substrate with said nonmagnetic layer in between to define another surface aligned with said surface of the first substrate, whereby an edge portion of the nonmagnetic layer is exposed by an amount equal to the thickness of said first magnetic layer; (d) sputtering a second magnetic layer on an area including said another surface of the second substrate and an end face of said nonmagnetic layer; and (e) lapping said second magnetic layer until the first and second magnetic layers and the nonmagnetic layer present a common surface plane opposite to a common surface plane defined by the aligned surfaces of said first and second substrate.
Claim 4
Independent Claim 162 words
A method of fabricating a magnetic head comprising: (a) sputtering a first magnetic layer on a surface of a first substrate whereby the magnetic layer and the substrate present a common end face perpendicular to said surface; (b) sputtering a nonmagnetic layer on said common end face; (c) bonding a second substrate end-to-end to said first substrate with said nonmagnetic layer in between to define another surface aligned with said surface of the first substrate, whereby an edge portion of the nonmagnetic layer is exposed by an amount equal to the thickness of said first magnetic layer; (d) sputtering a second magnetic layer on an area including said another surface of the second substrate and an end face of said nonmagnetic layer; and (e) lapping said second magnetic layer until the first and second magnetic layers and the nonmagnetic layer present a common surface plane opposite to a common surface plane defined by the aligned surfaces of said first and second substrate.
Claim 5
Dependent Claim 50 words
A method as claimed in claim 2, wherein each of said first and second substrates comprises a first body of ferromagnetic material and a second body of nonmagnetic material, said first and second bodies being bonded together, wherein said nonmagnetic layer is located between said second bodies of said substrates.
Claim 6
Dependent Claim 19 words
A method as claimed in claim 2, wherein said nonmagnetic material is at least one of glass and ceramic.
Claim 7
Dependent Claim 34 words
A method as claimed in claim 2, further comprising the steps of forming a layer of resin on said second magnetic layer prior to step (e) and lapping said resin layer during step (e).
Claim 8
Dependent Claim 36 words
A method as claimed in claim 2, further comprising the step of forming a layer of low-melting point glass on said second magnetic layer prior to step (e) and removing said glass layer during step (e).
Claim 9
Independent Claim 146 words
A method of fabricating a magnetic head comprising: (a) sputtering a first magnetic layer on a surface of a first substrate whereby the magnetic layer and the substrate present a common end face perpendicular to said surface; (b) sputtering a nonmagnetic layer on said common end face; (c) bonding said first substrate to a portion of a second substrate with said first magnetic layer in between, thereby defining a first common surface plane; (d) sputtering a second magnetic layer on an area including the remainder of said second substrate and an end face of said nonmagnetic layer; (e) lapping said second magnetic layer, said first substrate and said nonmagnetic layer until said first and second magnetic layers and said nonmagnetic layer present a second common surface plane opposite to said first common surface plane; and (f) bonding a third substrate to said second common surface plane.
Claim 10
Independent Claim 146 words
A method of fabricating a magnetic head comprising: (a) sputtering a first magnetic layer on a surface of a first substrate whereby the magnetic layer and the substrate present a common end face perpendicular to said surface; (b) sputtering a nonmagnetic layer on said common end face; (c) bonding said first substrate to a portion of a second substrate with said first magnetic layer in between, thereby defining a first common surface plane; (d) sputtering a second magnetic layer on an area including the remainder of said second substrate and an end face of said nonmagnetic layer; (e) lapping said second magnetic layer, said first substrate and said nonmagnetic layer until said first and second magnetic layers and said nonmagnetic layer present a second common surface plane opposite to said first common surface plane; and (f) bonding a third substrate to said second common surface plane.

References Cited (Backward Citations)

US3629519A Cited
JPS53133418A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-06-08 1990-12-08 1991-06-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-06-08 1994-12-08 1995-06-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-06-08 1998-12-08 1999-06-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag