Articles comprising stabilized piezoelectric vinylidene fluoride polymers

Assignee: Focas Ltd
•
Filing: 1985-08-28
•
Granted: 1987-05-26
•
Expires: 2005-08-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An article comprising vinylidene fluoride polymer which has been rendered piezoelectric by stretching the article to a final draw ratio of less than about 6:1 and polarizing and has an equivalent activity A* of at least 6, where A* is given by A*=d.sub.3h -50(d.sub.o -d) where d 3h is the hydrostatic coefficient of the stretched and polarized vinylidene fluoride polymer after heating at 120° C. for 1 hr, in units of pC/N; d o is the density of the unstretched and unpolarized polymer, in units of g/cc; and d is the density of the stretched and polarized polymer before heating at 120° C. for 1 hr, in units of g/cc, said article having an aggregate dimensional change of less than 15% upon heating at 120° C. for 1 hr, as measured by the sum of the absolute dimensional changes along three orthogonal coordinate axes, one of which is a principal direction of stretching. Vinylidene fluoride polymer with these characteristcs is prepared by stretching, conditioning, and polarizing, or, alternatively, stretching, polarizing, and conditioning.

Inventors

  • 👤 Pravin L. Soni
  • 👤 Alan B. Glendinning

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 18:52
CPC Classifications
H; H10; H10N; H10N30/00; H10N30/01; H10N30/09; H10N30/098; H10N30/04; H10N30/045

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 94 words
A method of making an article comprising highly piezoelectric, low void content vinylidene fluoride polymer, having dimensional and piezoelectric stability upon exposure to elevated temperatures, comprising in sequence the steps of stretching the article from an original configuration to an extended configuration; conditioning the article at a temperature between about 20° C. above the stretching temperature and about 15° C. below the crystalline melting point of the vinylidene fluoride polymer while maintaining the article under an applied electric field, under conditions that permit it to recover towards its original configuration; and polarizing the article.
Claim 2
Independent Claim 94 words
A method of making an article comprising highly piezoelectric, low void content vinylidene fluoride polymer, having dimensional and piezoelectric stability upon exposure to elevated temperatures, comprising in sequence the steps of stretching the article from an original configuration to an extended configuration; conditioning the article at a temperature between about 20° C. above the stretching temperature and about 15° C. below the crystalline melting point of the vinylidene fluoride polymer while maintaining the article under an applied electric field, under conditions that permit it to recover towards its original configuration; and polarizing the article.
Claim 3
Independent Claim 94 words
A method of making an article comprising highly piezoelectric, low void content vinylidene fluoride polymer, having dimensional and piezoelectric stability upon exposure to elevated temperatures, comprising in sequence the steps of stretching the article from an original configuration to an extended configuration; polarizing the article, and conditioning the article at a temperature between about 20° C. above the stretching temperature and about 15° C. below the crystalline melting point of the vinylidene fluoride polymer while maintaining the article under an applied electric field, under conditions that permit it to recover towards its original configuration.
Claim 4
Independent Claim 94 words
A method of making an article comprising highly piezoelectric, low void content vinylidene fluoride polymer, having dimensional and piezoelectric stability upon exposure to elevated temperatures, comprising in sequence the steps of stretching the article from an original configuration to an extended configuration; polarizing the article, and conditioning the article at a temperature between about 20° C. above the stretching temperature and about 15° C. below the crystalline melting point of the vinylidene fluoride polymer while maintaining the article under an applied electric field, under conditions that permit it to recover towards its original configuration.
Claim 5
Dependent Claim 18 words
A method according to claim 1 or claim 2 wherein the vinylidene fluoride polymer is vinylidene fluoride homopolymer.
Claim 6
Dependent Claim 17 words
A method according to claim 1 or claim 2 wherein the conditioning temperature is about 120° C.
Claim 7
Dependent Claim 31 words
A method according to claim 1 or claim 2 wherein the conditioning step is performed while maintaining the article under an applied electric field of between about 50 and 150 MV/m.

References Cited (Backward Citations)

US3878274A Cited
US4308370A Cited
US4427609A Cited
US4560737A Cited
US4592880A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-05-25 1990-11-24 1991-05-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-05-25 1994-11-24 1995-05-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-05-25 1998-11-24 1999-05-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag