Abstract

Abstract A method of manufacturing a rock bit cone having a substantially conical body on a surface of which a number of teeth are formed is manufactured by pressure-casting with using a casting mold having a molding surface including a cone body defining surface portion and tooth defining surface portions, pouring a molten metal of very hard and low melting point alloy having a melting point of 1040°-1120° C. and Rockwell hardness of 55-65 to the casting mold to centrifugal-cast at least a predetermined area including a tip of each tooth with the hard metal, and pouring a molten tough metal to the casting mold to centrifugal-cast the cone body.

Inventors

  • 👤 Shoichiro Tsugaki
  • 👤 Tomoo Miyasaka
  • 👤 Yukio Nishiyama
  • 👤 Toshio Atsuta

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 23:32
CPC Classifications
B; B22; B22D; B22D13/00; B22D13/06; B22D13/066; B22D13/04; B22D19/00; B22D19/06

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 159 words
A method of manufacturing a rock bit cone of the type which comprises a substantially conical body and a number of teeth formed on a surface of the conical body and each covered by a hard metal layer and which is rotatably supported by each of a plurality of bearing pins extending centripetally obliquely from a drill bit body, an axis of the conical body being registered with an axis of the bearing pin, comprising the steps of preparing a casting mold having a molding surface including a cone body defining surface portion and tooth defining surface portions, pouring a molten metal of very hard and low melting point alloy having a melting point of 1040°-1120° C. and Rockwell C hardness of 55-65 to the casting mold to centrifugal-cast at least a predetermined area including a tip of each tooth with the hard metal, and pouring a molten tough metal to the casting mold to centrifugal-cast the cone body.
Claim 2
Independent Claim 159 words
A method of manufacturing a rock bit cone of the type which comprises a substantially conical body and a number of teeth formed on a surface of the conical body and each covered by a hard metal layer and which is rotatably supported by each of a plurality of bearing pins extending centripetally obliquely from a drill bit body, an axis of the conical body being registered with an axis of the bearing pin, comprising the steps of preparing a casting mold having a molding surface including a cone body defining surface portion and tooth defining surface portions, pouring a molten metal of very hard and low melting point alloy having a melting point of 1040°-1120° C. and Rockwell C hardness of 55-65 to the casting mold to centrifugal-cast at least a predetermined area including a tip of each tooth with the hard metal, and pouring a molten tough metal to the casting mold to centrifugal-cast the cone body.
Claim 3
Independent Claim 159 words
A method of manufactuing a rock bit cone of the type which has a substantially conical body on a surface of which a number of teeth each covered by a hard metal layer are formed, comprising the steps of preparing a casting mold having a molding surface including a cone body defining surface portion and tooth defining surface portions, preparing tooth pieces of the same material as that forming the cone body, disposing the tooth pieces on the tooth defining surface portions, respectively, with a predetermined gap being provided between an outer surface of each tooth piece and corresponding tooth defining surface portion and with a root portion of each tooth piece being inside the cone defining surface portion, pouring a molten metal of very hard and low melting point alloy having a melting point of 1040°-1120° C. and Rockwell C hardness of 55-65 to centrifugal-cast the gaps and pouring a molten tough metal to centrifugal-cast the cone body.
Claim 4
Independent Claim 159 words
A method of manufactuing a rock bit cone of the type which has a substantially conical body on a surface of which a number of teeth each covered by a hard metal layer are formed, comprising the steps of preparing a casting mold having a molding surface including a cone body defining surface portion and tooth defining surface portions, preparing tooth pieces of the same material as that forming the cone body, disposing the tooth pieces on the tooth defining surface portions, respectively, with a predetermined gap being provided between an outer surface of each tooth piece and corresponding tooth defining surface portion and with a root portion of each tooth piece being inside the cone defining surface portion, pouring a molten metal of very hard and low melting point alloy having a melting point of 1040°-1120° C. and Rockwell C hardness of 55-65 to centrifugal-cast the gaps and pouring a molten tough metal to centrifugal-cast the cone body.

References Cited (Backward Citations)

US1043831A Cited
US2125332A Cited
US2184776A Cited
US2260593A Cited
US2442718A Cited
US2743495A Cited
US2740176A Cited
US4276788A Cited
US4423646A Cited
US4396077A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-05-25 1990-11-24 1991-05-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-05-25 1994-11-24 1995-05-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-05-25 1998-11-24 1999-05-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag