← Back to Patent Explorer
US4663240A Expired / Lapsed US ⏱️ 0.0 years remaining

RFI shielded plastic articles and process for making same

Assignee: MacDermid Enthone Inc
•
Filing: 1984-11-06
•
Granted: 1987-05-05
•
Expires: 2004-11-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An RFI shielded enclosure and a process for making same are disclosed. The process comprises coating at least one surface of the enclosure with a fluid organic binder having a substantial percentage of catalytic particles suspended therein. The particles used cause the electroless deposition of copper or nickel to produce an RFI shielded enclosure having in excess of 40 dB's shielding at frequencies above 10 kiloHertz.

Inventors

  • 👤 Juan B. Hajdu
  • 👤 Edwin W. Bastenbeck

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 02:28
CPC Classifications
H; H05; H05K; H05K9/00; H05K9/0073; H05K9/0081; H05K9/0083; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12007; Y10T428/12014; Y10T428/13; Y10T428/131; Y10T428/1314; Y10T428/1317; Y10T428/1321; Y10T428/1352; Y10T428/1355; Y10T428/1359; Y10T428/25; Y10T428/252; Y10T428/254; Y10T428/256; Y10T428/26; Y10T428/263; Y10T428/266

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 146 words
A process for producing an article or enclosure having electromagnetic/radio frequency shielding, said process comprising: (a) selecting a suitable electrically nonconductive enclosure; (b) applying to at least one side of said enclosure a primary layer comprising a fluid organic binder, having active metal particles dispersed therein, said binder being a paint selected from the class of acrylic paints, epoxy paints, urethane paints and oil based paints with said particles being chosen from the group consisting of nickel, copper, iron, cobalt, gold, silver, platinum, palladium and combinations thereof; (c) depositing onto said primary layer a second layer of electroless copper; and (d) depositing onto said second layer a third layer of metal selected from the group consisting of nickel, copper, zinc, tin and alloys thereof, to provide an enclosure having a shielding of at least 40 dB's against electromagnetic radiation having a frequency greater than 10 kiloHertz.
Claim 2
Dependent Claim 146 words
A process for producing an article or enclosure having electromagnetic/radio frequency shielding, said process comprising: (a) selecting a suitable electrically nonconductive enclosure; (b) applying to at least one side of said enclosure a primary layer comprising a fluid organic binder, having active metal particles dispersed therein, said binder being a paint selected from the class of acrylic paints, epoxy paints, urethane paints and oil based paints with said particles being chosen from the group consisting of nickel, copper, iron, cobalt, gold, silver, platinum, palladium and combinations thereof; (c) depositing onto said primary layer a second layer of electroless copper; and (d) depositing onto said second layer a third layer of metal selected from the group consisting of nickel, copper, zinc, tin and alloys thereof, to provide an enclosure having a shielding of at least 40 dB's against electromagnetic radiation having a frequency greater than 10 kiloHertz.
Claim 3
Dependent Claim 42 words
The process of claim 1 wherein said non-conductive enclosure is fabricated from the group consisting of moldable thermosetting resins, moldable thermoplastic resins, reinforced thermosetting resins, reinforced thermoplastic resins, glass, ceramic, glass fiber, reinforced ceramic, pressed fiber board and composite materials made therefrom.
Claim 4
Dependent Claim 22 words
The process of claim 1 wherein said primary layer, when dry has a metal to binder ratio of at least about 50%.
Claim 5
Dependent Claim 22 words
The process of claim 1 wherein said particles have a size in the range of between about 0.5 and about 10 microns.
Claim 6
Dependent Claim 19 words
The process of claim 1 wherein in step b, the thickness of said coating is at least 0.5 mils.
Claim 7
Dependent Claim 37 words
The process of claim 1 wherein said primary layer is etched to achieve at least a partial removal of the organic binder in said coating so as to expose at least a portion of said metal particles.
Claim 8
Dependent Claim 28 words
The process of claim 6 wherein said exposed metal particles are deoxidized by rinsing the surfaces thereof with an acid solution prior to the performance of step c.
Claim 9
Dependent Claim 27 words
The process of claim 1 wherein the combined thickness of the second and third layer is in the range of between about 40 and about 200 microinches.
Claim 10
Dependent Claim 13 words
The process of claim 1 wherein the third layer is applied by electroplating.
Claim 11
Dependent Claim 16 words
The process of claim 1 wherein the third layer is a layer of electrolessly plated nickel.
Claim 12
Dependent Claim 18 words
The process of claim 1 wherein the second layer of electroless copper is at least 11 microinches thick.
Claim 13
Dependent Claim 23 words
The process of claim 1 wherein the primary layer is applied by spray-painting the enclosure with the organic binder containing the metal particles.
Claim 14
Dependent Claim 147 words
An article or enclosure having electromagnetic/radio frequency shielding, said enclosure being fabricated by a process comprising: (a) selecting a suitable electrically nonconductive enclosure; (b) applying to at least one side of said enclosure a primary layer comprising a fluid organic binder having active metal particles dispersed therein, said binder being a paint selected from the class of acrylic paints, epoxy paints, urethane paints and oil based paints with said particles being chosen from the group consisting of nickel, copper, iron, cobalt, gold, silver, platinum, palladium and combinations thereof; (c) depositing on said primary layer a second layer of electroless copper; and (d) depositing onto said second layer a third layer of metal chosen from the group consisting of electroless nickel, electroless copper and combinations thereof to provide an enclosure having a shielding of at least 40 dB's against electromagnetic radiation having a frequency greater than 10 kiloHertz.
Claim 15
Dependent Claim 147 words
An article or enclosure having electromagnetic/radio frequency shielding, said enclosure being fabricated by a process comprising: (a) selecting a suitable electrically nonconductive enclosure; (b) applying to at least one side of said enclosure a primary layer comprising a fluid organic binder having active metal particles dispersed therein, said binder being a paint selected from the class of acrylic paints, epoxy paints, urethane paints and oil based paints with said particles being chosen from the group consisting of nickel, copper, iron, cobalt, gold, silver, platinum, palladium and combinations thereof; (c) depositing on said primary layer a second layer of electroless copper; and (d) depositing onto said second layer a third layer of metal chosen from the group consisting of electroless nickel, electroless copper and combinations thereof to provide an enclosure having a shielding of at least 40 dB's against electromagnetic radiation having a frequency greater than 10 kiloHertz.

References Cited (Backward Citations)

US3745045A Cited
US4258100A Cited
US4447492A Cited
US4507359A Cited
GB2169925A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-05-04 1990-11-03 1991-05-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-05-04 1994-11-03 1995-05-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-05-04 1998-11-03 1999-05-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag