← Back to Patent Explorer
US4654388A Expired / Lapsed US ⏱️ 0.0 years remaining

Latex adhesives for floor laying

Assignee: Bostik Inc
•
Filing: 1985-08-19
•
Granted: 1987-03-31
•
Expires: 2005-08-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An adhesive composition comprising an aqueous dispersion of film forming resin, filler and tackifying substances. The dispersion uses wood rosin and esterified rosin as tackifying substances and also includes diethylene glycol monobutyl ether. The compositions are specially formulated to avoid use of the more volatile organic solvents which are undesirable for flammability or health reasons. The compositions are particularly suitable for use as nonflammable floor laying adhesives by methods in which porous flooring material is laid onto the wet adhesive layer or non-porous flooring material is laid onto the "semi-dry" adhesive layer.

Inventors

  • 👤 Per-Erik Lofgren

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 01:16
CPC Classifications
C; C09; C09J; C09J131/00; C09J131/02; C09J131/04; C09J133/00; C09J133/04; C09J133/06; C09J133/08; C08; C08L; C08L2205/00; C08L2205/02; C08L2666/00; C08L2666/02; C08L2666/26; C08L2666/28; C08L93/00; C08L93/04

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 43 words
An adhesive composition, free of volatile organic solvent of boiling point less than about 200° C., comprising an aqueous dispersion of film-forming resin, finely divided filler, diethylene glycol monobutyl ether, and, as a tackifying substance, a mixture of wood rosin and esterified rosin.
Claim 2
Dependent Claim 43 words
An adhesive composition, free of volatile organic solvent of boiling point less than about 200° C., comprising an aqueous dispersion of film-forming resin, finely divided filler, diethylene glycol monobutyl ether, and, as a tackifying substance, a mixture of wood rosin and esterified rosin.
Claim 3
Dependent Claim 77 words
An adhesive composition, free of volatile organic solvent of boiling point less than about 200° C., comprising an aqueous dispersion of film-forming resin, finely divided filler, diethylene glycol monobutyl ether, and, as a tackifying substance, a mixture of wood rosin and esterified rosin in a weight ratio of about 1:3 to about 1:8 by weight, said mixture present in quantities to provide a weight ratio of film-forming resin to tackifying substance of about 3:1 to about 6:1.
Claim 4
Dependent Claim 77 words
An adhesive composition, free of volatile organic solvent of boiling point less than about 200° C., comprising an aqueous dispersion of film-forming resin, finely divided filler, diethylene glycol monobutyl ether, and, as a tackifying substance, a mixture of wood rosin and esterified rosin in a weight ratio of about 1:3 to about 1:8 by weight, said mixture present in quantities to provide a weight ratio of film-forming resin to tackifying substance of about 3:1 to about 6:1.
Claim 5
Dependent Claim 14 words
A composition according to claim 1 further comprising a thickener and a wetting agent.
Claim 6
Dependent Claim 14 words
A composition according to claim 2 further comprising a thickener and a wetting agent.
Claim 7
Dependent Claim 14 words
A composition according to claim 1 wherein the film-forming resin comprises an acrylate copolymer.
Claim 8
Dependent Claim 14 words
A composition according to claim 2 wherein the film-forming resin comprises an acrylate copolymer.
Claim 9
Dependent Claim 16 words
A composition according to claim 1 wherein the film-forming resin comprises an ethylene vinyl acetate copolymer.
Claim 10
Dependent Claim 16 words
A composition according to claim 2 wherein the film-forming resin comprises an ethylene vinyl acetate copolymer.
Claim 11
Dependent Claim 32 words
A composition according to claim 1 wherein the film-forming resin comprises a mixture of an acrylate copolymer and an ethylene vinyl acetate copolymer in a ratio of about 2:1 to about 8:1.
Claim 12
Dependent Claim 32 words
A composition according to claim 2 wherein the film-forming resin comprises a mixture of an acrylate copolymer and an ethylene vinyl acetate copolymer in a ratio of about 2:1 to about 8:1.
Claim 13
Dependent Claim 12 words
A composition according to claim 1 containing about 50-75 weight percent solids.
Claim 14
Dependent Claim 12 words
A composition according to claim 2 containing about 50-75 weight percent solids.

References Cited (Backward Citations)

US3838079A Cited
US4143019A Cited
US4018732A Cited
US4590230A Cited
US4503184A Cited
US4532273A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-03-30 1990-09-29 1991-03-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-03-30 1994-09-29 1995-03-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-03-30 1998-09-29 1999-03-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag