US4639279A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Single frequency induction hardening process
Assignee: Rolls Royce Corp
•
Filing: 1985-11-13
•
Granted: 1987-01-27
•
Expires: 2005-11-13
Abstract
Abstract The teeth and roots of a gear are contour hardened by induction at a single work station with a single solid state power supply. The inductor or coil is full-faced and encircles the gear during the preheat and final heat steps of the process. The power supply energizes the inductor with alternating current of a single frequency in the general range of 50-100 kHz according to a predetermined schedule of on-time and power level. The supply of current to the inductor is such that the time required for the supplied power level to achieve the scheduled power level in the final heat step is no more than approximately one-third of the scheduled final heat time.
Inventors
- 👤 Madhu S. Chatterjee
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-09 07:03
CPC Classifications
C; C21; C21D; C21D1/00; C21D1/06; C21D1/09; C21D1/10; C21D9/00; C21D9/32; Y; Y02; Y02P; Y02P10/00; Y02P10/25; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49462
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
147 words
In a single shot process for contour hardening a gear by induction, the process including a preheat step during which the gear is positioned within an encircling coil and heated by supplying the coil with alternating current for a desired preheat interval at a preheat power level, and a final heat step during which the gear is maintained within the coil and further heated by supplying the coil with alternating current for a desired final heat interval at a final heat power level, the improvement wherein: the alternating current supplied to the coil in both the preheat and final heat steps is of a single frequency in the general range of 50 kHz-100 kHz, and the time required for the supplied power level to achieve the final heat power level in the final heat step is no more than approximately one-third of the desired final heat time.
Claim 2
Dependent Claim
147 words
In a single shot process for contour hardening a gear by induction, the process including a preheat step during which the gear is positioned within an encircling coil and heated by supplying the coil with alternating current for a desired preheat interval at a preheat power level, and a final heat step during which the gear is maintained within the coil and further heated by supplying the coil with alternating current for a desired final heat interval at a final heat power level, the improvement wherein: the alternating current supplied to the coil in both the preheat and final heat steps is of a single frequency in the general range of 50 kHz-100 kHz, and the time required for the supplied power level to achieve the final heat power level in the final heat step is no more than approximately one-third of the desired final heat time.
Claim 3
Dependent Claim
221 words
A process for single shot contour hardening a gear by induction comprising the steps of: positioning the gear to be contour hardened within a full faced coil on the central axis thereof such that the coil extends beyond the gear faces along the direction of such axis; supplying the coil with alternating current of predetermined frequency in the general range of 50 kHz to 100 kHz and at a desired preheat power level for a desired preheat time to define a preheat step during which the gear teeth and roots are heated to an initial desired temperature; defining a dwell interval during which the coil is not supplied with current and tips of the gear teeth are permitted to cool to a somewhat lower temperature than the rest of the gear; supplying the coil with alternating current of said predetermined frequency at a desired final heat power level for a desired final heat time to define a final heat step during which the gear teeth and root surfaces are heated to a final desired temperature, the supply of alternating current during said final heat step being such that the time required to achieve the final heat power level is no more than approximately one-third of the desired final heat time; and quenching the gear to produce the desired depth of hardness.
Claim 4
Dependent Claim
221 words
A process for single shot contour hardening a gear by induction comprising the steps of: positioning the gear to be contour hardened within a full faced coil on the central axis thereof such that the coil extends beyond the gear faces along the direction of such axis; supplying the coil with alternating current of predetermined frequency in the general range of 50 kHz to 100 kHz and at a desired preheat power level for a desired preheat time to define a preheat step during which the gear teeth and roots are heated to an initial desired temperature; defining a dwell interval during which the coil is not supplied with current and tips of the gear teeth are permitted to cool to a somewhat lower temperature than the rest of the gear; supplying the coil with alternating current of said predetermined frequency at a desired final heat power level for a desired final heat time to define a final heat step during which the gear teeth and root surfaces are heated to a final desired temperature, the supply of alternating current during said final heat step being such that the time required to achieve the final heat power level is no more than approximately one-third of the desired final heat time; and quenching the gear to produce the desired depth of hardness.
References Cited (Backward Citations)
US2446202A
Cited
US3196244A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1990-01-26 | 1990-07-28 | 1991-01-27 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1994-01-26 | 1994-07-28 | 1995-01-27 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1998-01-26 | 1998-07-28 | 1999-01-27 | $7700.00 | Window Closed / Lapsed |